Load-bearing capacities of occlusal veneers made of all-ceramic and resin composite: do the substrate and material type affect mechanical durability?
Arta Lamallari, Vera Colombo, Luiza Freitas Brum Souza, Enkelejd Angelo Cankja, Abdülhakim Alpaslan Sener, Mutlu Özcan · 2026
Read Load-bearing capacities of occlusal veneers made of all-ceramic and resin composite: do the substrate and material type affect mechanical durability? by Arta Lamallari, Vera Colombo, Luiza Freitas Brum Souza, Enkelejd Angelo Cankja, Abdülhakim Alpaslan Sener, Mutlu Özcan (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/PMC13613771.txt.
Description
Arta Lamallari and colleagues test in 2026 how much load thin chewing-surface veneers can bear before they crack, and whether the material and the base beneath them change the answer. Veneers one millimetre thick were made from zirconia, two glass-ceramic materials, and a resin composite. Each type was bonded to one of three bases that mimic worn teeth: dentine ringed by enamel, plain dentine, or resin composite, with ten samples per group.
Before breaking them, the team aged the samples through 1.2 million chewing cycles with heat and cold swings between 5 and 50 degrees. Both the veneer material and the base type shaped the breaking load, and reliability analysis showed how the risk of failure spread. Dentists restoring worn back teeth can use the results to pair material and tooth base more wisely.
Catalog record
| CREATOR | Arta Lamallari, Vera Colombo, Luiza Freitas Brum Souza, Enkelejd Angelo Cankja, Abdülhakim Alpaslan Sener, Mutlu Özcan |
|---|---|
| YEAR | 2026 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 52 KB |
| LICENSE | https://creativecommons.org/licenses/by/4.0 |
| RIGHTS | CC BY |
| SOURCE | Europe PMC |