Stress Corrosion Cracking of Ti-6Al-4V ELI Titanium Alloy in 3.5 wt.% NaCl Solution

Qing Zhao, Aifeng Zhang, Zhengquan Wan, Yafei Wang, Chengqi Sun · 2026

Read Stress Corrosion Cracking of Ti-6Al-4V ELI Titanium Alloy in 3.5 wt.% NaCl Solution by Qing Zhao, Aifeng Zhang, Zhengquan Wan, Yafei Wang, Chengqi Sun (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/pmc-13566888.txt.

Description

Qing Zhao and co-authors test a deep-sea titanium alloy for cracking under stress in salt water, in a 2026 paper. The alloy, an extra-low-interstitial grade of Ti-6Al-4V, is prized for toughness and assumed to resist stress corrosion even better than the standard grade. The team pulled notched samples at speeds spanning a thousandfold range, in air and in a seawater-like salt solution.

In air, toughness fell by more than a fifth at slow pull rates, with fracture faces hinting at hydrogen damage. In salt water the lowest toughness matched values reported for the standard alloy. Toughness alone, the authors conclude, does not guarantee cracking resistance, and loading rate belongs in any marine safety case.

Catalog record

CREATORQing Zhao, Aifeng Zhang, Zhengquan Wan, Yafei Wang, Chengqi Sun
YEAR2026
COLLECTIONPAPERS
FORMATTXT
FILE SIZE31 KB
VERSION1.0
LICENSECC BY 4.0
RIGHTSCC BY
SOURCEEurope PMC

Source: https://europepmc.org/articles/PMC13566888

Browse the full library · About the Tower of Babel