Waterborne Polyurethane Treated with Flame Retardant Based on Polydimethylsiloxanes and Boron Phenolic Resin for Improving the Char Residue and Anti-Dripping Performance

Yadian Xie, Chao Liu, Yujie Wang, Dongmei Bao, Wei Yan, Guoyong Zhou, Gaëlle Fontaine, Giulio Malucelli · 2024

Read Waterborne Polyurethane Treated with Flame Retardant Based on Polydimethylsiloxanes and Boron Phenolic Resin for Improving the Char Residue and Anti-Dripping Performance by Yadian Xie, Chao Liu, Yujie Wang, Dongmei Bao, Wei Yan, Guoyong Zhou, Gaëlle Fontaine, Giulio Malucelli (2024) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/pmc-11643660.txt.

Description

Yadian Xie and co-authors published a materials study in twenty twenty-four on making waterborne polyurethane far less flammable. The coating is popular but burns and drips. The team cured it with a flame retardant blending silicone polymer and boron phenolic resin, then measured how the film behaved in fire tests.

Heat resistance rose by about forty degrees, and the oxygen index needed to sustain burning jumped from about twenty-two to thirty-three percent. Char left after heating to six hundred degrees grew sixty-fold, and the char was highly graphitic. Smoke, heat release, and flue gas all fell sharply. The coating earned the top UL-94 rating with no melt dripping, at only two percent additive loading.

Catalog record

CREATORYadian Xie, Chao Liu, Yujie Wang, Dongmei Bao, Wei Yan, Guoyong Zhou, Gaëlle Fontaine, Giulio Malucelli
YEAR2024
COLLECTIONPAPERS
FORMATTXT
FILE SIZE57 KB
VERSION1.0
LICENSECC BY 4.0
RIGHTSCC BY
SOURCEEurope PMC

Source: https://europepmc.org/articles/PMC11643660

Browse the full library · About the Tower of Babel