Electron microscopy technique for determination of dispersoid distribution in powder blends
Unknown · 2013
Read Electron microscopy technique for determination of dispersoid distribution in powder blends by Unknown (2013) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/nasa-tm-19680000583-electron-microscopy-technique-for-determ.txt.
Introduction
Bruno C. Buzek, at the Lewis Research Center in Cleveland, developed a way to peek inside a metal powder before it is pressed into a part. Powder blends mix hard oxide particles, the dispersoid, into metal powder. Where those particles sit at the start shapes the finished product.
Buzek's technique wraps the blend in a thin carbon skin, then leaches the metal away. The leftover oxide particles show their size and clumping, unobstructed by metal. He tried it on nickel, tungsten, chromium, and nichrome blended with thoria or alumina. Well-spread particles stayed well spread after sintering; early clusters survived as large particles.
Catalog record
| CREATOR | Unknown |
|---|---|
| YEAR | 2013 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 15 KB |
| LICENSE | Public Domain |
| RIGHTS | PUBLIC DOMAIN |
| SOURCE | NASA NTRS |
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Electron microscopy technique for determination of dispersoid distribution in powder blends NASA Technical Memorandum \ ' J NASA TM X-1468 ELECTRON MICROSCOPY TECHNIQUE FOR DETERMINATION O F DISPERSOID DISTRIBUTION IN POWDER BLENDS By B r u n o C. Buzek Lewis Research Center Cleveland, Ohio NATIONAL AERONAUTICS AND SPACE ADMINISTRATION For sale by the Clearinghouse for Federal Scientific and Technical lnformotion Springfield, Virginia 22151 - CFSTl price $3.00 ELECTRON MICROSCOPY TECHNIQUE FOR DETERMINATION OF DISPERSOID DISTRIBUTION IN POWDER BLENDS by B r u n o C. Buzek Lewis Research Center SUMMARY The ability to clearly observe and distinguish between oxide and metal particles in a starting powder blend and to determine the initial distribution of the oxide prior to con- solidation enables predictions to be made about the final distribution of the oxide parti- , cles in a fully consolidated product. A new electron-microscope specimen-preparation technique was developed to aid in making these predictions. This procedure makes it possible to ascertain the size and the degree of agglomeration of the oxide particles, un- obstructed by the presence of the metal-matrix particles, before the compaction and sintering of the powder blend. In the application of this technique, the initial powder blend is enveloped with a thin layer of carbon, and the metal phase is leached out. The retained particles then reveal the state of the dispersoid phase after the blending opera- tion. Nickel, tungsten, chromium, and nicnrome, each blended with thoria or alumina, were investigated with the use of this technique. A good correlation exists between the dispersoid distribution in the initial blend and the state of agglomeration in the final sin- tered product; that is, if small oxide particles were well distributed in the initial pow- der blend, they remained in a similar state in the final product. On the other hand, if the small oxide particles were clustered in the original powder blend, they appeared as large particles similar in size to the initial clusters after consolidation. INTROD UCTlON The mechanical blending method of producing dispersion-st e gthened m terials has been used with varying success. In such materials, an interparticle spacing of the dis- persoid of less than 2 microns is required for effective strengthening. It has also been shown that interparticle spacing in the dispersion-strengthened product decreases with decreasing particle size of both the oxide and the metal powders (ref. 1). However, c ultrafine powders (as small as a few hundredths of a micron) present difficulties because of the possibility of agglomeration, which may occur during handling, consolidation, o r thermal processing. To determine the presence and extent of such agglomeration, i t has been necessary to prepare and examine consolidated and sintered specimens by replica electron micros- copy. Recently, ultrafine powder blends were successfully consolidated by high-energy- rate compaction. These compacts are dense enough (without sintering) for direct repli- cation and examination by electron microscopy (ref. 2). In this consolidated condition, it w a s not always possible to determine desired structural details, because of the cold work introduced during compaction. A low-temperature stress-relief annealing treat- ment preceding replication was used to improve details. Such an annealing treatment was not believed to cluster fine dispersoid particles (NO. 01 to 0.05 pm) appreciably, if at all; however, there remained some question as to whether any minute agglomeration would occur. Thus, a technique for examination of the completely unaltered (prior to compaction o r sintering) powder blends was required. A new technique using electron microscopy which permits discrimination between dispersoid and matrix particles in ultrafine metal-oxide powder blends is described herein. The technique clearly shows size, shape, and degree of agglomeration of oxide particles and similarly, but less clearly, characterizes the metal matrix particles. The ultrafine powder blends studied included the metals nickel, chromium, tungsten, and nichrome each blended with thoria o r alumina; however, only a study of the compacts of nickel and tungsten with thoria and alumina as dispersoids is presented herein. MATERIALS, APPARATUS, AND PROCEDURE The materials that were studied with the electron-microscopy technique a r e given in table I. Powder blends of nickel - 4 volume percent thorium oxide and nickel - 4 volume percent aluminum oxide were prepared by ball milling. A powder blend of tung- sten - 2 volume percent thorium oxide was prepared by vapor deposition. TABLE I. - MATERIALS INVESTIGATED Specimen Matrix Oxide additive Method of blending Tungsten 2 Percent thorium Vapor deposition oxide (Tho2) Nickel 4 Percent thorium Ball milling oxide (Tho2) Nickel 4 Percent aluminum Ball milling oxide (Alz03) 2 *-' The procedure for preparing the powders for electron microscopic examination is as follows: About 30 milligrams of each powder blend are placed on a glass slide, and a few drops of Cellosolve (ethylene glycol monoethyl ether) are added. The diluted slurry is lightly dispersed with a spatula and spread over the glass slide. After drying, the film of dried slurry on the slide is shadowed with platinum a t an angle of approximately 20°, after which a 0. 02-micron thickness of carbon is deposited vertically. This film is then scored into 1/8-inch (0.31-cm) grid-size squares. The slide with the film scored in the form of small squares is immersed in acid or water to float off the carbon film contain- ing the metal-oxide powders. When nickel is the matrix powder, the solutions used to separate the carbon films from the glass slides are also used to dissolve away the nickel from the film (see following table). Approxi- Remarks material mate time, hr Nickel 30 Percent nitric 24 Floated off directly acid in water in acid solution 24 Transferred to acid 2 Parts nitric acid solution after sepa- 1 Part hydrofluoric rating film from acid glass slide in water Water is used to float the film containing the tungsten and oxides, since hydrofluoric acid (HF), the acid to be used to dissolve tungsten, would attack the glass slide and con- taminate the specimen. The water-floated films (grid-size squares) are then trans- ferred to a solution of nitric acid and hydrofluoric acid to leach out the metal matrix. In both cases, the dissolution of the metal matrix is completed after 24 hours. Slow dis- solution is necessary to avoid a shifting of the dispersoid. The carbon films containing the undissolved dispersiod are then washed three to four times in distilled water, placed on an electron-microscope grid, dried on filter paper, and examined in the electron mi- croscope. Electron micrographs a r e made of the carbon film containing only the disper- soid at magnifications up to 75 000. DISCUSSION AND RESULTS The preparation procedure described may be termed a ** shell" technique. Electron micrographs obtained with this technique were compared with micrographs obtained by placing the same starting powder materials directly on the electron-microscope grid. For comparison of the results of the shell method and those obtained from consolidated 3 L and sintered blends, the same blends were also prepared by using a cartridge-actuated compaction press and then annealing (ref. 2) to reveal structures more clearly. Two of these specimens were annealed at a low temperature of 1700° F (927' C) f o r 1 hour, and after examination by replication were given an additional l-hour anneal at