Native Cellulose: Structure, Characterization and Thermal Properties.
Poletto M, Ornaghi HL, Zattera AJ. · 2014
Read Native Cellulose: Structure, Characterization and Thermal Properties. by Poletto M, Ornaghi HL, Zattera AJ. (2014) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/europmc-pmc5456159.txt.
Introduction
Poletto and co-authors study how the structure of native cellulose shapes the heat resistance of natural fibers. Their research article appeared in Materials. Cellulose is the main building material of plants. Makers increasingly use plant fibers in composite products. A fiber's behavior under heat depends on its inner structure. Crystallinity, crystal size, and chemical makeup all matter. Knowing them in advance can guide better material choices.
The team examined ten natural fibers. Six came from plants such as sisal, jute, and ramie. Four came from Brazilian woods. They measured the fibers with infrared spectroscopy, X-ray diffraction, and heat-based weight tests. Fibers with more extractives and lower crystallinity broke down sooner. Smaller cellulose crystals also meant weaker heat stability. In contrast, larger crystals and higher crystallinity pushed breakdown to higher temperatures. The results let makers predict fiber performance before mixing composites.
Catalog record
| CREATOR | Poletto M, Ornaghi HL, Zattera AJ. |
|---|---|
| YEAR | 2014 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 39 KB |
| LICENSE | CC BY 4.0 |
| RIGHTS | CC BY |
| SOURCE | Europe PMC |
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Native Cellulose: Structure, Characterization and Thermal Properties By Matheus Poletto, Heitor L Ornaghi Júnior, Ademir J Zattera Published in: Materials DOI: 10.3390/ma7096105 ABSTRACT Abstract In this work, the relationship between cellulose crystallinity, the influence of extractive content on lignocellulosic fiber degradation, the correlation between chemical composition and the physical properties of ten types of natural fibers were investigated by FTIR spectroscopy, X-ray diffraction and thermogravimetry techniques. The results showed that higher extractive contents associated with lower crystallinity and lower cellulose crystallite size can accelerate the degradation process and reduce the thermal stability of the lignocellulosic fibers studied. On the other hand, the thermal decomposition of natural fibers is shifted to higher temperatures with increasing the cellulose crystallinity and crystallite size. These results indicated that the cellulose crystallite size affects the thermal degradation temperature of natural fibers. This study showed that through the methods used, previous information about the structure and properties of lignocellulosic fibers can be obtained before use in composite formulations. Keywords: natural fibers, cellulose, crystallinity, XRD, FTIR, thermal stability 1. INTRODUCTION The last few decades have revealed the growing interest of industry and scientists on the research and development of polymeric and composite materials from renewable sources [1,2,3,4]. As the most abundant component in most plants, cellulose is an almost inexhaustible polymeric raw material from renewable sources. Natural cellulose-based materials, such as wood and natural fibers, have been used as engineering materials for thousands of years, and their use currently continues, as demonstrated by the huge number of forest product-based worldwide industries. However, what makes cellulose such an important material for the development polymeric and composite materials? The cellulose macromolecule is made up of repeating glucose units that generate surprising specificity and impressively diverse architectures, reactivities and functions [5]. The reactions and properties of native cellulose are determined by the isolation process used, the number of inter- and intra-molecular hydrogen bonds, the chain lengths, the chain length distribution, the crystallinity and the distribution of functional groups within the repeating units and along the polymer chains [5,6,7]. These important parameters make cellulose a unique material. Therefore, knowledge of and understanding the properties of native cellulose before their use in composites can result in composites with better mechanical and thermal properties. In order to better understand the relationships between native cellulose structure and properties, the aim of this work was to establish the main structural differences between six vegetal fibers (curaua, ramie, kenaf, jute, sisal and buriti) and four wood fibers (Pinus elliottii, Eucalyptus grandis, Mezilaurus itauba and Dipteryx odorata) commonly used as reinforced fillers in composite materials through X-ray diffraction (XRD) analysis, Fourier transform infrared (FTIR) spectroscopy and thermogravimetric analysis (TGA). 2. EXPERIMENTAL SECTION 2.1. Materials The wood flour samples used in this study were obtained from wastes of the lumber industry in Brazil. The species investigated were Pinus elliottii (PIE), Eucalyptus grandis (EUG), Mezilaurus itauba (ITA) and Dipteryx odorata (DIP). The others six vegetal fibers also used in this study were: Hibiscus cannabinus (kenaf), Corchorus capsularis (jute), Agave sisalana (sisal), Ananas erectifolius (curaua), Boehmaria nivea (ramie) and Mauritia flexuosa (buriti). Kenaf, jute and sisal fibers were supplied by Tapetes São Carlos Technology (from São Carlos, SP, Brazil) as sheets. Curaua fiber was obtained from Centro de Apoio a Projetos de Ação Comunitária (CEAPAC), a support center for community action projects in Santarem/PA, Brazil. Ramie roving was purchased from Sisalsul Fibras Naturais (São Paulo, SP, Brazil), and buriti fiber was obtained from Sisalsul Fibras Naturais (Caxias do Sul, RS, Brazil). All of the fiber samples were dried at 105 °C for 24 h in a vacuum oven before the tests. The samples were grounded in a knife mill, and the average fiber particle length used in all analyses was around 200 μm. 2.2. Fourier Transform Infrared (FTIR) Spectroscopy FTIR spectra were obtained by means of a Nicolet IS10spectrometer (Thermo Scientific, Waltham, MA, USA). Natural fiber powder samples of each species (5 mg) were dispersed in a matrix of KBr (100 mg), followed by compression to form pellets. The sample collection was obtained using 32 scans, in the range of 4000 to 400 cm−1, at a resolution of 4 cm−1. Three different measurements for each fiber were evaluated, and the average value was considered. 2.3. X-ray Diffraction X-ray diffractograms were collected using a sample holder mounted on a XRD-6000 diffractometer (Shimadzu, Kyoto, Japan) with monochromatic CuKα radiation (λ = 0.15418 nm). The generator was utilized at 40 kV and 30 mA, and the intensities were measured in the range of 5° < 2θ < 30°, typically with scan steps of 0.05° at 2 s/step (1.5°/min). Peak separations were carried out using Gaussian deconvolution. After deconvolution, it is possible to calculate and compare several parameters. The d-spacings were calculated using the Bragg equation. In this study, the Z-discriminant function developed by Wada and Okano [8] for the determination of the crystalline structure (monoclinic and triclinic) of cellulose in natural fibers was used. By employing discriminant analysis, it is possible to categorize cellulose as Type Iα or Iβ [8]. The Z-value indicates whether cellulose is Iα or Iβ. The function that discriminates between Iα or Iβ is given by Equation (1): [formula: (1)Z = 1693d1 – 902d2 − 594] where d1 is the d-spacing of the peak (1–10); d2 is the d-spacing of the peak (110); and Z > 0 indicates Iα; while Z < 0 indicates the Iβ dominant type [8]. The crystalline index proposed by Hermans et al. [8,9] is presented in Equation (2): [formula: (2)] where Cr.I. is the crystalline index; Acryst is the sum of crystalline band areas; and Atotal is the total area under the diffractograms. The second approach used to determine the crystalline index, Equation (3), was the empirical method proposed by Segal et al. in 1959 [8,10], which is: [formula: (3)] where I200 is the maximum intensity of the (200) lattice diffraction; and Iam is the intensity diffraction of the amorphous band. The apparent crystallite size (L), shown in Equation (4), was calculated using the Scherrer equation [9]: [formula: (4)] where K is a constant of value 0.94; λ is the X-ray wavelength (0.1542 nm); β is the half-height width of the diffraction band; and θ is the Bragg angle corresponding to the (200) plane. 2.4. Thermogravimetric Analysis The thermogravimetric analysis was carried out on a TGA50 analyzer (Shimadzu, Kyoto, Japan) under constant nitrogen flow (50 mL/min), from 25 to 800 °C, at a heating rate of 10 °C/min. Approximately 10 mg of each sample were used. 3. RESULTS AND DISCUSSION 3.1. Fibers Chemical Composition Table 1 shows the composition of the fibers used in this study based on the literature [11,12,13,14]. Wood fibers present higher fractions of lignin and holocellulose (cellulose and hemicellulose) than the others natural fibers. Extractive content in wood is also higher than natural fibers. Tropical woods, such as Dipteryx odorata and Mezilaurus itauba, showed extractive contents three-times higher than temperate woods, such as Eucalyptus grandis and Pinus elliottii. On the other hand, vegetal fibers showed higher cellulose content associated with lower fractions of lignin and extractives. [Table: Chemical composition of the fibers used in this study obtained from the literature [11,12,13,14].] The mechanical and physical properties of the fibers are