A Review of Solid Electrolyte Interphases on Lithium Metal Anode.
Cheng XB, Zhang R, Zhao CZ, Wei F, Zhang JG, Zhang Q. · 2016
Read A Review of Solid Electrolyte Interphases on Lithium Metal Anode. by Cheng XB, Zhang R, Zhao CZ, Wei F, Zhang JG, Zhang Q. (2016) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/europmc-pmc5063117.txt.
Introduction
Xin-Bing Cheng and five co-authors review the protective skin that forms on lithium metal anodes, in Advanced Science in 2016. Lithium metal batteries promise very high energy density for phones and electric cars, but needle-like lithium growths, called dendrites, short them out and have blocked use for decades. A stable surface layer, the solid electrolyte interphase, is the main hope for taming that growth.
The review explains how the layer forms, the rival models of its structure, and the tools that probe its chemistry, shape, and behavior while a battery runs. Heat, current density, and the liquid's makeup all steer what kind of layer grows. Fixes surveyed include new electrolyte recipes and additives, ready-made artificial layers, and redesigned electrodes that spread current evenly. The authors close by asking for more precise links between the layer's structure and battery performance.
Catalog record
| CREATOR | Cheng XB, Zhang R, Zhao CZ, Wei F, Zhang JG, Zhang Q. |
|---|---|
| YEAR | 2016 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 85 KB |
| LICENSE | CC BY 4.0 |
| RIGHTS | CC BY |
| SOURCE | Europe PMC |
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
A Review of Solid Electrolyte Interphases on Lithium Metal Anode By Xin‐Bing Cheng, Rui Zhang, Chen‐Zi Zhao, Fei Wei, Ji‐Guang Zhang, Qiang Zhang Published in: Advanced Science DOI: 10.1002/advs.201500213 ABSTRACT Lithium metal batteries (LMBs) are among the most promising candidates of high‐energy‐density devices for advanced energy storage. However, the growth of dendrites greatly hinders the practical applications of LMBs in portable electronics and electric vehicles. Constructing stable and efficient solid electrolyte interphase (SEI) is among the most effective strategies to inhibit the dendrite growth and thus to achieve a superior cycling performance. In this review, the mechanisms of SEI formation and models of SEI structure are briefly summarized. The analysis methods to probe the surface chemistry, surface morphology, electrochemical property, dynamic characteristics of SEI layer are emphasized. The critical factors affecting the SEI formation, such as electrolyte component, temperature, current density, are comprehensively debated. The efficient methods to modify SEI layer with the introduction of new electrolyte system and additives, ex‐situ‐formed protective layer, as well as electrode design, are summarized. Although these works afford new insights into SEI research, robust and precise routes for SEI modification with well‐designed structure, as well as understanding of the connection between structure and electrochemical performance, is still inadequate. A multidisciplinary approach is highly required to enable the formation of robust SEI for highly efficient energy storage systems. INTRODUCTION Rechargeable lithium (Li)‐based batteries have been world‐widely investigated as the light‐weight and high‐energy‐density energy storage devices.1, 2 The earliest commercial products of rechargeable Li batteries appeared in the 1970s, employing Li metal as the anode.3, 4 However, metallic Li electrodes were quickly discarded due to the Li dendrite growth during electrodeposition. Li dendrites can short‐circuit the cell causing a safety risk. In the 1990s, Li‐ion batteries (LIBs) were introduced by Sony Corporation to address the dendrite issues by hosting Li in a graphitic material. Li ion insertion strategies led to the tremendous success of LIBs in consumer portable electronics.5 It should be noted that the enhanced battery safety of LiBs is at a significant cost of energy density, because the specific capacity of Li metal (3860 mA h g−1) is ten times larger than that of graphite (370 mA h g−1). Though LIBs are now gradually approaching their theoretical limit, they still cannot meet the booming requirements for personal electronics and electric vehicles. With the development of advanced electrolytes, separators, and other battery components, Li‐metal‐based rechargeable batteries have been strongly considered in recent years.6, 7, 8 The safe use of Li metal as an anode is still a great challenge, as the dendritic and mossy metal deposits are very easily obtained on the working Li metal anode. Li dendrites induce a low Coulombic efficiency and severe safety risk, hindering the practical demonstration of Li metal batteries (LMBs) with very high energy density. The dendrite nucleation and growth are closely related to the surface layer between the electrolyte and anode. The surface component and structure of the layer play an extremely important effect on the morphology of Li deposits and decide the cycling performance of LMBs.7, 9, 10, 11, 12, 13, 14 As Li metal can react with most organic solvents, a surface film is formed during the initial charging/discharging processes. In 1979, Peled firstly realized the electrically insulating and ionically conductive interface and named it as the solid electrolyte interphase (SEI).15 The SEI layer is with a thickness of ≈20 nm and includes various organic and inorganic components. On one hand, the formation of the SEI intrinsically consumes the anode and electrolyte, leading to a low efficiency. On the other hand, the SEI effectively prevents the further physical contact between Li and the solvent, therefore making Li dynamically stable in certain organic solvents. Beyond that, the SEI can adjust the distribution of Li ions from the bulk electrolyte to the anode15 (Figure 1 ): (1) the solvated Li ion sheds its solvent molecules and thus has the access to the internal Schottky vacancy of the SEI; (2) the Li ion continuously migrates through the bulk of the SEI by relaying itself in Schottky vacancies; (3) finally, it reaches the anode surface and accepts an electron from the current collector, then is deposited as Li metal. The even deposition of Li ions leads to dendrite‐free morphology of LMBs with high efficiency. [Figure: A schematic description of Li‐ion diffusion from the bulk electrolyte to the anode.15 a) The solvated Li ion sheds its solvent molecules and thus has the access to the internal Schottky vacancy of the SEI. b) The Li ion continuously migrates through the bulk of the SEI by relaying itself in Schottky vacancies. c) The free Li ion reaches the anode surface and accepts an electron from the current collector, then deposits as Li metal.] The SEI film is widely observed in LIBs. In routine LIBs, robust SEI layers can be formed when graphite, silicon and other oxides are employed as the anode. Since the SEI on the graphite anode can be extremely stable during several thousands of cycles in the carbonate electrolyte, the as‐obtained LIBs with the graphite anode have been successfully commercialized. However, the SEI layer of Li metal is usually unstable and is not yet well understood. Compared with volume changes of ≈10 and 400% for graphite and silicon anodes, respectively, the relative volumetric change of Li metal anode is virtually infinite, because Li metal is ‘hostless’. The huge volume change requires the SEI layer with high elastic modulus. Dendrite growth is widely observed in LMBs, which is a fundamental challenge in LMB researche but has been detected less in current commercial LIBs. Consequently, the issue is much tougher for the SEI layer of Li metal in LMBs than that of LIBs. The fundamental exploration of SEIs on LMB is the first step to understand the complex but important issue of Li metal anode. For an ideal SEI, it should have several features, such as high Li ionic conductivity, proper thickness with compact structure, and high elastic strength to mechanically suppress the breakthrough by Li dendrites, which is an important part to inhibit the dendrite growth on Li metal anode. However, the SEI layer of LMBs is unstable in some extreme operation conditions, such as extreme high/low temperature and high cycling rates. The formed SEI either grows much thicker or becomes non‐protective, which induces rapid performance degradation. Consequently, many strategies have been proposed to construct a stable SEI, such as the electrolyte additives, electrode design, charging models, etc. In this contribution, the recent advances in fundamental science of the SEI formation on the Li metal anode are reviewed. Firstly, the formation mechanisms of SEI and models of SEI structure on Li metal anode are briefly summarized. The recent progress in the characterization of the components, structure, and electrochemical property of SEI layer are fully investigated. The principles of SEI formation under different operation parameters and SEI modification for robust use in a working cell are summarized. Finally, recent developments and new directions in research on SEIs of Li metal anode are also involved. MECHANISM OF SEI FORMATION The present electrolyte systems in LMBs mostly contain solvents and Li salts.16, 17, 18 The common solvents are esters (e.g. ethylene carbonate (EC), propylene carbonate