Pure and stable metallic phase molybdenum disulfide nanosheets for hydrogen evolution reaction.

Geng X, Sun W, Wu W, Chen B, Al-Hilo A, Benamara M, Zhu H, Watanabe F, Cui J, Chen TP. · 2016

Read Pure and stable metallic phase molybdenum disulfide nanosheets for hydrogen evolution reaction. by Geng X, Sun W, Wu W, Chen B, Al-Hilo A, Benamara M, Zhu H, Watanabe F, Cui J, Chen TP. (2016) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/europmc-pmc4749985.txt.

Introduction

Geng and nine colleagues report a water-based route to a form of molybdenum disulfide that does not exist in nature: the metallic phase. It is prized for catalysis but so unstable that earlier preparations mixed phases or reverted within days. Their hydrothermal synthesis yields pure metallic nanosheets directly.

A predicted Raman signature at 146 wavenumbers confirms the structure. A single layer of water molecules clinging to both faces of each sheet keeps the sheets apart and prevents collapse, granting lasting stability in water. As a hydrogen evolution catalyst the material performs strongly, needing only minus 175 millivolts to reach a benchmark current density.

Catalog record

CREATORGeng X, Sun W, Wu W, Chen B, Al-Hilo A, Benamara M, Zhu H, Watanabe F, Cui J, Chen TP.
YEAR2016
COLLECTIONPAPERS
FORMATTXT
FILE SIZE31 KB
LICENSECC BY 4.0
RIGHTSCC BY
SOURCEEurope PMC

Source: https://europepmc.org/articles/PMC4749985

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Pure and stable metallic phase molybdenum disulfide nanosheets for hydrogen evolution reaction By Xiumei Geng, Weiwei Sun, Wei Wu, Benjamin Chen, Alaa Al-Hilo, Mourad Benamara, Hongli Zhu, Fumiya Watanabe, Jingbiao Cui, Tar-pin Chen Published in: Nature Communications DOI: 10.1038/ncomms10672 ABSTRACT Metallic-phase MoS2 (M-MoS2) is metastable and does not exist in nature. Pure and stable M-MoS2 has not been previously prepared by chemical synthesis, to the best of our knowledge. Here we report a hydrothermal process for synthesizing stable two-dimensional M-MoS2 nanosheets in water. The metal–metal Raman stretching mode at 146 cm−1 in the M-MoS2 structure, as predicted by theoretical calculations, is experimentally observed. The stability of the M-MoS2 is associated with the adsorption of a monolayer of water molecules on both sides of the nanosheets, which reduce restacking and prevent aggregation in water. The obtained M-MoS2 exhibits excellent stability in water and superior activity for the hydrogen evolution reaction, with a current density of 10 mA cm−2 at a low potential of −175 mV and a Tafel slope of 41 mV per decade. The metallic-phase MoS2 (M-MoS2) is a single-layer S-Mo-S structure in which each molybdenum atom is surrounded by six sulfur atoms in an octahedral lattice. With dense active sites and an electronic conductivity that is six orders of magnitude higher than that of the semiconductor phase of MoS2 (S-MoS2) (ref. 1), M-MoS2 has emerged as a promising candidate for a broad range of applications and is expected to exhibit better performance than its semiconducting counterpart, in particular in the hydrogen evolution reaction (HER) and as a photocatalyst and supercapacitor2345. These attractive properties of M-MoS2 are offset by the fact that a pure phase of M-MoS2 is very challenging to prepare, because it is highly unstable. Over the past few decades, many efforts to develop a process to prepare stable and highly pure M-MoS2 have largely proved futile. A complicated method for the preparation of metastable M-MoS2 using lithium intercalation of S-MoS2 has been reported5678. However, the reported M-MoS2 suffered from coexistence with S-MoS2 in a relative proportion of 50–80% (refs 3, 9). In addition, the intermediary LixMoS2 and intercalator of n-butyllithium are both dangerous materials that may self-heat8 and are highly pyrophoric in air5. The preparation procedures are also tedious and can take as long as 3 days1011. The previously mentioned M-MoS2 easily transformed to S-MoS2 due to S–S van der Waals interactions121314. Therefore, an efficient synthesis method for the production of a large quantity of stable and pure M-MoS2 is still highly desirable. M-MoS2 could be an intermediary state during the synthesis of S-MoS2, which is a stable form in many chemical reactions1516. This approach provides a possible method for capturing the metastable M-MoS2 even though it is thermodynamically unstable and may rapidly transform to S-MoS2 at elevated temperatures. In fact, S-MoS2 can transform into an octahedral structure of M-MoS2 under a high pressure of 35 GPa (refs 17, 18, 19), which implies that the metallic phase of MoS2 may be achievable at a relatively low temperature, a specific pressure and a proper chemical environment. Therefore, we employ octahedral MoO3 as the starting material in a pressurized hydrothermal process, to directly grow highly pure M-MoS2 in water. The as-prepared M-MoS2 is highly stable in water due to the reduced stacking of the layered materials, which are separated by water molecules. Urea, which is a weak reducing agent, plays a key role in the formation of M-MoS2. The structure of octahedral MoO3 can be maintained under acidic conditions. To satisfy the expected growth conditions, thioacetamide is chosen as the sulfur source and the reaction is maintained at a low pH value (pH∼4). The synthesis of M-MoS2 is performed at 200 °C by mixing MoO3, thioacetamide and urea in an autoclave. The as-prepared M-MoS2 is pure and stable with high activity for the HER. RESULTS Highly pure metallic phase MoS2 Figure 1a shows a typical scanning electron microscopic (SEM) image of the as-prepared M-MoS2 sample. The MoS2 nanosheets are 100 nm in size and a few nanometres in thickness. The morphology of S-MoS2 is similar to that of M-MoS2 on the nanoscale (Supplementary Fig. 1). The results from energy dispersive X-ray spectroscopy indicated that the S to Mo atomic ratio of the as-prepared M-MoS2 is ∼2.05 (Supplementary Fig. 2). The most notable difference between M-MoS2 and S-MoS2 is the symmetry of the sulfur in their structures. The structural variations result in significant differences in their characteristic Raman features. Figure 1b shows the Raman spectra of M-MoS2 and S-MoS2 synthesized at 200 °C and 240 °C, respectively. A strong Raman band is observed at 146 cm−1 and attributed to Mo–Mo stretching vibrations in M-MoS2. Calculations have predicted this band at the K points of the Brillouin zone for octahedrally coordinated distorted MoS2 (ref. 12). Our results confirm the existence of this band in M-MoS2. The Raman shifts (that is, ∼219, 283 and 326 cm−1) are also associated with the phonon modes in M-MoS2. S-MoS2 exhibits typical Raman shifts of ∼378 and 404 cm−1 for E12g and A1g, respectively, which are substantially different from those of M-MoS2. The phase identification of the synthesized M-MoS2 and S-MoS2 was further studied using X-ray photoelectron spectroscopy and the results are shown in Fig. 1c,d. The Mo 3d spectra consist of peaks located at approximately 228.7 and 231.8 eV, which correspond to the 3d5/2 and 3d3/2 components, respectively, of Mo4+ in M-MoS2. However, the Mo 3d peaks of the M-MoS2 samples also exhibit weak shoulders at the positions as those in S-MoS2 due to the transformation of M-MoS2 in vacuum and X-ray illumination. The details for the peak deconvolution are provided in Supplementary Fig. 3 and Supplementary Note 1. The Mo 3d peaks of M-MoS2 shifted to lower binding energies by ∼1 eV with respect to the corresponding peaks in S-MoS2. This result is consistent with the previously obtained relaxation energy of 1 eV for M-MoS2 derived from S-MoS2 (refs 20, 21). Similarly, the S 2p peaks of M-MoS2 were located at ∼161.6 and 162.7 eV, and associated with S 2p3/2 and 2p1/2, respectively, which are also ∼1 eV lower than the corresponding peaks in S-MoS2. It is important to note that the prominent S peak located at ∼168 eV was absent, indicating that the sulfur atoms remain unoxidized in M-MoS2. However, this peak was observed in S-MoS2 after annealing at 240 °C. Morphologies and optical properties of MoS2 Figure 2a shows optical images of the two types of MoS2 dispersed in water. M-MoS2 does not appear to exhibit bulk aggregation, whereas S-MoS2 aggregates at the bottom of the solution. This result may be because M-MoS2 possesses hydrophilic surfaces, whereas S-MoS2 possesses relatively hydrophobic surfaces522. After sonication, both M-MoS2 and S-MoS2 can uniformly disperse in water (Fig. 2b). However, M-MoS2 was grey colour, whereas S-MoS2 was green colour. These colours were associated with their optical properties, which were confirmed by optical absorption spectroscopy. Figure 2c shows the ultraviolet–visible absorption spectra of M-MoS2 and S-MoS2 in water. Two typical absorption peaks located at 613 and 660 nm were observed for S-MoS2 and these peaks are associated with the energy split from the valence band spin–orbital coupling in S-MoS2 with large lateral dimensions23. In addition, another optical