Recommendations for Directly Processed 1-kg Sized CWF Products
Ebert, W. L., Gesualdi, J., Liao, Y. · 2026
Read Recommendations for Directly Processed 1-kg Sized CWF Products by Ebert, W. L., Gesualdi, J., Liao, Y. (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/doe-osti-3915852-recommendations-for-directly-processed-1.txt.
Introduction
W. L. Ebert, J. Gesualdi, and Y. Liao of Argonne National Laboratory set out how to make and test one-kilogram ceramic waste form products by a simpler direct route. Their report, ANL/CFCT-26/23, is dated September 25, 2026. The waste form is glass-bonded sodalite, a ceramic first designed in the 1990s to lock up salt waste from fuel work.
The authors give recipes that match smaller batches made before, so the team can spot what changes at larger scale. They call for checks on the main phases, on salt spread through the product, and on how well glass coats the sodalite grains. Standard wear tests should use samples cut near the top, middle, bottom, and sides. The results will guide full-scale production and help qualify the waste form.
Catalog record
| CREATOR | Ebert, W. L., Gesualdi, J., Liao, Y. |
|---|---|
| YEAR | 2026 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 43 KB |
| LICENSE | Public Domain |
| RIGHTS | PUBLIC DOMAIN |
| SOURCE | DOE OSTI |
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
RECOMMENDATIONS FOR DIRECTLY PROCESSED 1-kg SIZED CWF PRODUCTS Nuclear Fuel Cycle & Supply Chain Prepared for U.S. Department of Energy Materials Recovery and Waste Form Development Campaign W.L. Ebert, J. Gesualdi, and Y. Liao Argonne National Laboratory September 25, 2026 ANL/CFCT-26/23 September 25, 2026 iii ABSTRACT Recommendations for the processing and testing of 1-kg size ceramic waste form products are made to focus on the effectiveness of simplified direct processing to generate a waste form with acceptable quality from the perspective of microstructure and chemical durability. Recipes are provided to enable direct comparisons with smaller materials made previously to identify factors associated with scale up, including composition uniformity, important to developing methods for full-scale implementation. Recommended product analyses include identifying major phases, distributions of key salt constituents, microencapsulation of sodalite grains by glass, and the amounts and distributions of halite inclusion phases. The large amount of material available for testing supports replicate tests to measure the precision achieved using key test methods appropriate for demonstrating product consistency. Standard durability tests are recommended for samples taken from various locations near the top, middle, bottom, and sides of the product. The methods used to produce the 1-kg materials and measured characteristics will inform development of full-scale production methods, such as direct processing using molten salt feed, and provide data supporting qualification as a waste form. iv September 25, 2026 THIS PAGE INTENTIONALLY LEFT BLANK September 25, 2026 1 Recommendations for Directly Processed 1-kg Sized CWF Products 1. INTRODUCTION AND BACKGROUND The glass-bonded sodalite ceramic waste form (CWF) was designed in the 1990’s to accommodate most of the sodium and chloride ions in salt waste within synthetic sodalite (Na8[Al6Si6O24]Cl2) that is encapsulated in a durable borosilicate glass matrix that accommodates the other salt cations (see Ebert 2005 and references therein). Since it was first developed, the production method has changed as processes became better understood and aspects of large-scale implementation were addressed. The efficiency of processing and the quality of the product have been assessed continuously and comparatively as new methods were developed from laboratory to engineering scales. Recent developments have been focused on simplifying the production method for practical implementation in a product facility. This report provides recommendation on the production and testing of 1-kg CWF materials made by directly processing a mixture of Zeolite 4A, surrogate waste salt, and borosilicate glass using a method based on a fundamental understanding of the processes that occur and demonstrated to be effective at small scales. The generation of sodalite occurs by reaction Zeolite 4A with NaCl in the salt according to the reaction stoichiometry given in Equation 1. The process was originally designed to occlude molten salt within the Zeolite 4A cage structure by mixing the two components at approximately 500 °C to generate “salt-loaded zeolite” in an initial pre-conditioning step. The salt-loaded zeolite was mechanically mixed with crushed glass and then loaded into a canister that was sealed and processed at approximately 850 °C by using a hot isostatic press (HIP). The resulted in a densified glass-ceramic material contained within the collapsed canister. The canisters were sized so that two HIP CWF products could be placed in a standard short DOE container for storage, transport, and disposal. Na12(AlSiO4)12 + 4NaCl → 2 Na8(AlSiO4)6Cl2 (1) Zeolite 4A salt sodalite A “pressureless consolidation” (PC) method was later developed to directly process the mixture of salt- loaded zeolite and glass in a full-size canister without using HIP (Priebe and Bateman 2007). The PC CWF product had a similar microstructure and durability as HIPed material but was less dense. However, challenges to implement the PC process in a hot cell are significant in terms of handling fine particulate materials and multiple operation steps. A significant improvement in waste loading was made about 10 years ago by changing the binder glass used in the process. Specifically, the use of a high soda content glass was demonstrated to increase the waste loading by about 150% (Ebert et al. 2016). The high soda content increases the amount of sodalite that is generated by Reaction 1 due to in situ generation of NaCl through ion exchange of salt cations with sodium in the glass. This enables immobilization of chloride in salt waste streams devoid of NaCl. 2 September 25, 2026 2. DIRECT PROCESSING It has been hypothesized by several researchers that the production of CWF could be further simplified by omitting the pre-occlusion step and relaxing the reagent size and dryness control limits to facilitate material handling in a hot cell environment, as recently proposed by Ebert (2024). The efficacy of directly processing mixtures of various sizes and relative amounts of Zeolite 4A, salt, and glass to generate CWF material was demonstrated at the laboratory scale by successfully synthesizing monolithic waste forms at 880 and 925 °C and in both ceramic and steel crucibles (Gesualdi et al., 2025). Microstructure analysis by SEM and XRD analyses confirmed that Zeolite 4A was converted to sodalite by reaction with NaCl in the mixture and became microencapsulated within the glass phase along with small inclusions of halite that were generated as byproducts during processing. As observed in CWF materials made using HIP and PC methods, both glass and salt penetrated throughout the ~16 mesh-sized Zeolite 4A particles to microencapsulate the micrometer-sized grains of sodalite that formed. Materials made with uncrushed ~4-mm-sized Zeolite beads showed the generation of sodalite occurs by inward penetration of salt into the beads. It is hypothesized that this corresponds to the uptake of molten salt into the Zeolite 4A pore structure during processing when the mixture is heated to the salt melting temperature. That is, molten salt contacts both Zeolite 4A and glass particles as the mixture is heated. The thickness of the sodalite layer indicates the extent of salt uptake either due to kinetic limitations or the amount of salt available near enough to the zeolite surface due to physical constraints. Therefore, the Zeolite 4A reagent should be sized small enough to facilitate in situ occlusion of salt during processing by both the proximity of molten salt and the absorption rate. The molten salt and molten glass are expected to be immiscible at the processing temperature (e.g., 925 °C) but may intermix. Laboratory-scale products indicate the small amount of halite by-product inclusion phases distributed throughout the bulk are compositionally distinct from the added salt. It is expected that processing can be facilitated by directly adding molten salt (rather than crushed solid salt) to a mixture of crushed Zeolite 4A and crushed glass that has been heated to near or above the salt melting temperature but not as high as the temperature required to generate sodalite. The molten salt will be taken up by the Zeolite 4A as it percolates through the particles of Zeolite 4A and glass. It remains to be determined if physical mixing is necessary for adequate distribution. In a laboratory-scale test, the percolation of molten salt poured on top of a mixture of Zeolite 4A and glass was determined to have been effectively occluded in the Zeolite 4A throughout the bulk based on the generation of sodalite throughout the product. A mixing device (e.g., an Archimedes screw) could be used to enhance the mixing at a larger