Long Spin Relaxation Times in CVD-Grown Nanodiamonds

2026

Read Long Spin Relaxation Times in CVD-Grown Nanodiamonds (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2605-16394.txt.

Introduction

Prooth and seven others report glowing nanodiamonds averaging around 60 nm with mean spin T1 times of 800 microseconds and a maximum over 1.8 ms, close to bulk values. Crystal defects limit how well nitrogen-vacancy diamonds sense external fields, by shaping their spin relaxation and coherence times. Their advanced growth method uses heterogeneous nucleation on pre-engineered sites, a nearly ten-fold improvement over commercial diamonds of 50 to 150 nm. Heavy-nitrogen doped shells for sensing near the diamond surface are also made, with scalability addressed for production volumes.

Catalog record

YEAR2026
COLLECTIONPAPERS
FORMATTXT
FILE SIZE44829
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2605.16394

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Long Spin Relaxation Times in CVD-Grown Nanodiamonds Abstract Currently, the primary applications of fluorescent nanodiamonds (FNDs) are in the area of biosensing, by using photoluminescence or spin properties of colour centres, mainly represented by the Nitrogen Vacancy (NV) point defect. The sensitivity of NV-FNDs to external fields is, however, limited by crystallographic defects, which influence their key quantum state characteristics - the spin longitudinal ( T 1 ) and spin transversal ( T 2 ) relaxation and coherence times, respectively. We report on utilising an advanced FND growth technique consisting of heterogeneous nucleation on pre-engineered sites to create FNDs averaging around 60 nm in size, with mean longitudinal coherence times of 800 μ \mu s and a maximum over 1.8 ms, close to bulk theoretical values. This is a major, nearly ten-fold improvement over commercially available nanodiamonds for the same size range of 50 to 150 nm. Heavy-N doped nanodiamond shells, important for sensing events in nm proximity to the diamond surface, are fabricated and discussed in terms of re-nucleation and twinning on {111} crystal facets. We also discuss scalability issues in order to enable the production of FND volumes matching the needs of sensing applications. keywords Fluorescent Nanodiamonds, Chemical Vapour Deposition, NV Spin Relaxometry, Quantum Sensing Jeroen Prooth Michael Petrov Alevtina Shmakova Michal Gulka Petr Cigler Jan D’Haen Hans-Gerd Boyen Milos Nesladek* \dedication J. Prooth 1∗ , M. Petrov 1∗ , A. Shmakova 1 , Dr. M. Gulka 2 , Prof. Dr. P. Cigler 2 , Prof. Dr. J. D’Haen 1 , Prof. Dr. H.-G. Boyen 1 , Prof. Dr. M. Nesladek 1 1 Institute for Materials Research (IMO), Hasselt University, Wetenschapspark 1, B-3590, Diepenbeek, Belgium 2 Institute of Organic Chemistry and Biochemistry of the CAS, Prague, 166 10, Czech Republic ∗ Authors contributed equally Email Address: [email protected] 1 Introduction Nanodiamond (ND) is a fascinating class of nano-material because of its unique properties, such as low cytotoxicity and biocompatibility. [ 45 , 46 , 25 ] NDs can be used for nanoscale sensing based on fluorescent properties of incorporated point (colour) defect centres. For these purposes, this type of nanodiamond is referred to as Fluorescent Nanodiamond (FND). Further on, the paramagnetic, e.g. spin properties of colour centres, enable using FNDs for sensing the magnetic field noise close to the ND surface, leading to novel measuring concepts such as nano-NMR. [ 18 , 30 , 9 , 33 , 15 ] Most of the FNDs sensors are based on the nitrogen-vacancy (NV) centre, that has attracted significant attention due to its bright photoluminescence and negligible photobleaching. [ 28 ] The NV centre consists of a nitrogen atom next to a vacancy and has been studied fundamentally and used in initial applications. The NV spin ground triplet state can easily be manipulated by microwaves at ambient conditions. The crucial challenge for developing nanoscale sensing probes, based on the NV colour centres, is to engineer FNDs with high spin relaxation ( T 1 ) and spin coherence ( T 2 ) times, which differ significantly for various types of FNDs, and which limit a wide spread use of FNDs sensors in biology and chemistry fields, for example in drug delivery, bio-imaging, and bio-nanosensors for applications operating at room temperatures. Currently, commercial FNDs have T 1 times in the range of 100 microseconds, while the bulk diamond T 1 limit is about three milliseconds, thus limiting FND use significantly. [ 12 ] Here, we present data on about 8-fold improvement of the T 1 time by Chemical Vapor Deposition (CVD) technique, supported by understanding the underlying physics. Figure 1 : A nano-roughening pre-treatment on silicon is performed by using an ultrasonic vibration table on which diamond micro-particles are spread and on which the substrate is vibrated. This produces nano-roughness, and leaves carbon traces on the substrate surface, pictured in the AFM image. The growth scheme shows the introduction of gasses during the growth stage. As a base diamond material we use low N-doped samples, whereas for the shell-doped particles we created in addition a highly nitrogen-doped shell. Images of particles grown at 750 °C, 850 °C and 900 °C taken with a GeminiSEM 450 at 5 kV. Left side shows low-doped samples, with nitrogen shell-doped samples on the right. Shell-doped particles show preferential re-nucleation on their {111} facets due to the too-high nitrogen concentration, whereas low-doped particles show no such structures. Twinning can be found for all conditions. Currently, commercial FNDs are mainly prepared from high pressure, high temperature (HPHT) diamond by milling [ 5 ] and subsequent irradiation and annealing. HPHT FNDs have a typical NV T 1 relaxation time between 50 and 100 µs. [ 3 ] As the sensitivity of NV centre to magnetic fields is limited by the T 1 relaxation time, the ability to engineer FNDs with higher T 1 times would improve the detection sensitivity. [ 8 ] Nevertheless, this requires precise control over particle properties such as size, morphology, defects, and dopants. The HPHT FND approach, based on milling and grinding N-containing bulk diamond, produces FNDs that range in size from around 10 nm to 1 µm. This mechanical process makes these FNDs highly irregular and jagged, generating a significant amount of spin-active surface defects, dangling bonds and subsurface damage. [ 31 ] Further processing using high energy particle irradiation, employed to create nitrogen-vacancies, can cause internal lattice damage and introduce spin active defects, strain fields, or vacancy clusters. For HPHT nanodiamonds, one usually irradiates them with electrons (e - ), protons (p + ), or He 2+ and Li + ions. An annealing step allows the vacancies to diffuse towards the substitutional nitrogen and create NV centres, while at the same time some of the damage can be repaired. Nevertheless, a study done on several HPHT nanodiamonds irradiated by these methods showed that particles with sizes around 50 to 150 nm had T 1 times between 50 and 100 µs for those irradiated with e - , and He 2+ and up to 150 µs for particles irradiated with p + . [ 29 ] Other studies have shown similar results, with T 1 times ranging around 100 µs. [ 3 ] FNDs with a size of around 15 nm showed lower T 1 times around 25 µs. [ 12 ] Another method for large-scale production of fluorescent nanodiamonds (FND) using neutron irradiation is capable of producing significant amounts of nanodiamonds, typically on the order of around 100 grams. [ 16 ] However, the FNDs’ obtained T 1 times are short compared to their expected bulk values. In another work, the milling technique has been improved, leading to 1.2 ms T 1 times, however, only a few percent of FNDs contained NV centres. [ 20 ] Chemical vapour deposition (CVD) using isotopically pure 12 C as a source gas was used to grow diamond films, which were then again milled to produce FNDs. [ 44 ] Using this technique T 2 coherence close to 400 microseconds was reported. However, all methods employing milling face challenges related to defect formation, chipping, and the production of irregular sizes caused by the milling process. One of the techniques to eliminate milling is based on the etching of diamond

Read the complete text