Mechanical Scaling Laws and Deformation Behavior of Nanoporous Tantalum Microparticles Journal: Undisclosed journal
J.I. Ramallo, N. Vázquez von Bibow, M.A. Monclús, I. McCue, M.C. Fuertes, C.J. Ruestes · 2026
Read Mechanical Scaling Laws and Deformation Behavior of Nanoporous Tantalum Microparticles Journal: Undisclosed journal by J.I. Ramallo, N. Vázquez von Bibow, M.A. Monclús, I. McCue, M.C. Fuertes, C.J. Ruestes (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2604-22726.txt.
Introduction
Ramallo and five colleagues test whether scaling laws for nanoporous metals hold beyond gold, using single-crystal nanoporous tantalum made by liquid-metal dealloying. Indentation of single microparticles shows stiffness and hardness rising with solid fraction in line with Gibson-Ashby predictions for foams. Simulations point to dislocation-driven plasticity, and the authors credit bath chemistry with the stronger ligament connections.
Catalog record
| CREATOR | J.I. Ramallo, N. Vázquez von Bibow, M.A. Monclús, I. McCue, M.C. Fuertes, C.J. Ruestes |
|---|---|
| YEAR | 2026 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 35005 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2604.22726
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Mechanical Scaling Laws and Deformation Behavior of Nanoporous Tantalum Microparticles Journal: Undisclosed journal J.I. Ramallo, N. Vázquez von Bibow, M.A. Monclús, I. McCue, M.C. Fuertes, C.J. Ruestes Abstract The mechanical scaling laws of dealloyed nanoporous metals depart from classical Gibson-Ashby predictions for open-cell foams due to a decreased connectivity in their solid network. However, these scaling relations have been established almost exclusively on nanoporous gold produced by electrochemical dealloying, and it is an outstanding question whether the relations apply to nanoporous networks fabricated by other dealloying methods. Here, we investigate the mechanical response of single-crystalline nanoporous tantalum (np-Ta) produced by liquid metal dealloying (LMD) a TiTa alloy in molten CuBi. Nanoindentation of individual microparticles yields an elastic modulus of 10–30 GPa and a hardness of 0.3–1.1 GPa, both scaling with the solid volume fraction in agreement with Gibson-Ashby predictions. This stiffness-density response of np-Ta departs from previous reports on nanoporous gold and is attributed to enhanced ligament connectivity enabled by the thermodynamics of the CuBi metal bath. Molecular dynamics simulations reveal dislocation-dominated plasticity during indentation of np-Ta, consistent with scanning electron microscopy observations of limited densification beneath the indents, ruling out unusual deformation mechanisms as an origin of the observed scaling. These findings identify solvent chemistry in LMD as a tunable lever for ligament connectivity, and thus for the mechanical response of nanoporous metals. \elsprelimpagehlfalse 1 Introduction Open-cell nanoporous metals, characterized by pores and ligaments at the nanometer scale, are an emerging class of materials with tunable structure and properties montemayor2015materials , greer2019three . While relative density has traditionally served as the primary design parameter for cellular solids, advances in synthesis now enable control over the strut morphology, feature size, and hierarchy surjadi2025double , surjadi2025enabling , shi2021scaling , vyatskikh2018additive , zhang2021recent . As a result, these new materials exhibit unique combinations of mechanical and physical properties, which are anticipated to be rapidly adopted across a diversity of applications such as actuation biener2009surface , detsi2016metallic , structural portela2020extreme , shaw2019computationally , wu2023consequences , huber2023densification , optics and sensing zhang2013nanoporous , catalysis wittstock2023nanoporous , and nuclear bringa2012nanoporous , ruestes2025nanoporous . Dealloying is a potentially scalable technique to fabricate open-cell nanomaterials, during which the selective dissolution of element(s) from an alloy drives the spontaneous formation of a random porous network. The resulting material can be cubic centimeters in volume, with features as small as 2 nm and solid volume fractions between 0.2 and 0.6 mccue2016dealloying , mccue2018pattern . Although the mechanical properties of nanoporous metals have been extensively studied, these reports focused on noble metals, particularly nanoporous gold, whose cost and limited availability constrain use in practical applications. In contrast, more-common base metals (e.g., Fe, Ni, Ti) offer broader technological relevance but are challenging to process via electrochemical dealloying due to their higher reactivity and oxidation tendency mccue2018pattern . Liquid metal dealloying (LMD) overcomes these processing limitations, replacing aqueous electrolytes and applied potentials with molten metal solvents and enthalpic driving forces. The kinetics and morphological evolution during LMD have been studied over the past decade, enabling the fabrication of a wide range of nanoporous metals, including Ti wada2011nano , wada2011dealloying , okulov2017dealloying , berger2020open , Fe wada2013three , FeCr xiang2020universal , zou2024ligament , Ta geslin2015topology , mccue2016kinetics , song2020liquid , lai2022topological , Nb kim2014sub , gaskey2019self , sohn2025compressive , stainless steel zhao2017three and even high entropy alloys okulov2020nanoporous , wada2024accelerated , lee2025development , lee2026nanoporous , choi2026formation . Despite this progress, mechanical characterization of LMD nanoporous metals remains scarce. Recent studies have shown that the ligament connectivity and morphology of LMD structures are markedly different from those fabricated electrochemically and are linked to both the initial parent alloy composition and the solubility of the remaining component in the liquid metal solvent lai2022topological . In turn, these differences call into question the applicability of mechanical scaling laws developed for nanoporous gold, and how the interplay between dislocation activity and densification during deformation may be altered farkas2018indentation . Here, we investigate the mechanical behavior of the prototypical LMD system, nanoporous tantalum (np-Ta), to determine whether scaling laws developed for electrochemically dealloyed nanoporous gold remain predictive. Beyond its potential use in high-power electronics and biomedicine chakraborti2016ultrathin , wauthle2015additively , np-Ta is of interest for extreme environments, where refractory metals are needed as heat-pipe wicks and plasma-facing components peters2024materials , cunningham2024alloying , garrison2023review . To isolate the intrinsic foam response from grain-boundary effects, single-crystalline (single-grain-derived) np-Ta microparticles were experimentally fabricated chuang2022powder and tested via nanoindentation. The resulting mechanical response was then analyzed within established scaling frameworks for cellular solids and compared against previous studies on nanoporous gold and other LMD-derived nanoporous metals. Complementary atomistic simulations were also employed to rule out unusual deformation mechanisms as the origin of the observed trends. The resulting picture points to ligament connectivity, tuned by solvent chemistry during LMD, as the dominant factor setting the stiffness of np-Ta. 2 Materials and Methods 2.1 Sample preparation Ti 65 Ta 35 alloys were prepared in-house by radio-frequency (RF) induction using an Ambrel Ekoheat 45 kW system by melting Ti (99.995 wt.%), and Ta (99.95 wt.%) pellets from Kurt Lesker in a water-cooled copper crucible from Arcast Inc. under flowing Ar (99.999 wt.%). After casting, the ingots were annealed under flowing Ar (99.999 wt.%) for approximately 10 h. Compositional homogeneity was confirmed using energy-dispersive X-ray spectroscopy (EDS). Master ingots of \sim 30 g were made, rolled to foils \sim 100 \mu m thick, and then annealed at 1200 °C for 8 h. Dealloying was carried out by immersing foils into a 40 g bath of molten Cu 40 Bi 60 at \sim 800 °C in an ultra-high purity alumina crucible cast in-house using materials from Cotronics Corp. Induction melting was used to heat the samples under flowing Ar (99.99%), and the LMD process was run for 5 min. After dealloying, the samples were immersed in concentrated nitric acid to remove the CuBi and then rinsed with de-ionized water. The resulting material consisted of nanoporous powders (Fig. 1 .A,B) and the ligament diameter and solid volume fraction ( \phi ) were quantified using AQUAMI stuckner2017aquami , mccue2018gaining . The solid fraction is estimated from surface scanning electron microscopy and thus is an approximate 2D proxy. X-ray diffraction (XRD) measurements were performed to determine the presence of crystalline phases of tantalum (Fig. 1 .C). A PANalytical Empyrean X-ray diffractometer (INN-CNEA-CONICET) equipped with Cu K radiation ( \lambda = 1.54 Å) and a PIXcel3D area detector was used. Morphology and composition of particles obtained were evaluated using scanning electron microscopy (SEM). Investigations were performed using a FEI Quanta 200 microscope equipped with EDS (EDAX ® )(Gerencia de Materiales, CAC-CNEA) and a FEI Helios NanoLab 600i FEGSEM microscope (IMDEA Materials Institute). Figure 1 : A. SEM image of typical np-Ta particles. B. SEM image of the surface showing the nanoporous bicontinuous structure of one particle. C. XRD pattern of the np-Ta powder sample. D. Particles deposited on top of a Si wafer using CrystalBond ® 509 (bright phase bounding particles) for nanoindentation testing. 2.2 Nanoindentation To carry out the nanoindentation experiments, np-Ta powder particles were immobilized on polished Si substrates for nanoindentation measurements (Fig, 1 .D) by heating the Si substrate to \sim 70 °C, applying CrystalBond ® 509 forming