Influence of Ni substitution on the phase transitions and magnetocaloric effect of NdCo 2 \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} at cryogenic temperatures Preprint: APS/123-QED
Vilde G. S. Lunde, Øystein S. Fjellvåg, Allan M. Döring, Marc Straßheim, Vladimir Pomjakushin, Konstantin P. Skokov, Oliver Gutfleisch, Tino Gottschall, Joachim Wosnitza, Anja O. Sjåstad, Bjørn C. Hauback, Christoph Frommen · 2026
Read Influence of Ni substitution on the phase transitions and magnetocaloric effect of NdCo 2 \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} at cryogenic temperatures Preprint: APS/123-QED by Vilde G. S. Lunde, Øystein S. Fjellvåg, Allan M. Döring, Marc Straßheim, Vladimir Pomjakushin, Konstantin P. Skokov, Oliver Gutfleisch, Tino Gottschall, Joachim Wosnitza, Anja O. Sjåstad, Bjørn C. Hauback, Christoph Frommen (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2604-17336.txt.
Introduction
Lunde and eleven colleagues study how replacing cobalt with nickel changes the cold-temperature behavior of NdCo2, a cubic Laves compound prized for magnetic cooling. Cooling drives the pure material through structural transitions at 100 K and 42 K. Both transitions slide to lower temperatures as nickel rises, and the lower-temperature phase vanishes at higher nickel levels. Magnetic cooling power also falls, from over six degrees to under five degrees at the same field, as the magnetic moment shrinks.
Catalog record
| CREATOR | Vilde G. S. Lunde, Øystein S. Fjellvåg, Allan M. Döring, Marc Straßheim, Vladimir Pomjakushin, Konstantin P. Skokov, Oliver Gutfleisch, Tino Gottschall, Joachim Wosnitza, Anja O. Sjåstad, Bjørn C. Hauback, Christoph Frommen |
|---|---|
| YEAR | 2026 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 47185 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2604.17336
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Influence of Ni substitution on the phase transitions and magnetocaloric effect of NdCo 2 \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} at cryogenic temperatures Preprint: APS/123-QED Vilde G. S. Lunde, Øystein S. Fjellvåg, Allan M. Döring, Marc Straßheim, Vladimir Pomjakushin, Konstantin P. Skokov, Oliver Gutfleisch, Tino Gottschall, Joachim Wosnitza, Anja O. Sjåstad, Bjørn C. Hauback, Christoph Frommen Abstract We have investigated NdCo 2 – x Ni x \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2\hskip 0.90417pt--\hskip 0.90417ptx\/}}}\text{Ni}{\vphantom{\text{X}}}_{\smash[t]{\text{x\/}}} cubic Laves compounds with 0 ≤ \leq x ≤ \leq 1 using neutron diffraction and bulk magnetization measurements to study the influence of partial Ni substitutions of Co on the phase transitions and the magnetocaloric effect. Upon cooling, NdCo 2 \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} undergoes a cubic to tetragonal transition at 100 K, and a tetragonal to orthorhombic transition at 42 K. The transitions are associated with long-range ferromagnetic ordering of the magnetic moments along the c c axis and spin reorientation into the a b ab plane, respectively. Both transitions shift to lower temperatures as the Ni content x x increases. For x ≥ 0.5 x\geq 0.5 , the orthorhombic phase is suppressed. Additionally, there was a reduction in the magnetic moment upon increasing the Ni substitution of Co. The magnetocaloric effect was determined both indirectly and directly, with good agreement between the methods. NdCo 2 \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} exhibits an adiabatic temperature change of 6.3 K for a field of 20 T, which is decreased to 4.9 K for NdCoNi for the same field strength due to the reduced magnetic moment upon Ni substitution. I Introduction Magnetic refrigeration utilizing the magnetocaloric effect (MCE) offers superior cooling efficiency at cryogenic temperatures (20-77 K) compared to conventional gas compression-expansion methods franco_magnetocaloric_2018 . Consequently, significant efforts have been made to discover materials with a large MCE in this temperature region. Laves compounds are a class of materials that have shown significant MCEs at low temperatures, but most high-performing candidates contain expensive and scarce heavy rare-earth elements with high magnetic moments, such as Ho, Gd, and Dy castro_machine-learning-guided_2020 ; tereshina_effects_2023 ; franco_magnetocaloric_2018 . Therefore, there is a need to identify more cost-effective and abundant materials to scale up the technology. Replacing the heavy rare-earth elements in Laves compounds with more abundant light rare-earth elements at the expense of a lower MCE is one promising strategy to reduce cost liu_matter_2024 . \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} is a well-studied light rare-earth cubic \text{AB}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} Laves phase (space group Fd\bar{3}m ) which is paramagnetic at room temperature. The compound exhibits a magnetostructural phase transition at 100 K associated with a tetragonal distortion (space group I4_{1}/amd ) and ferromagnetic ordering ( T_{\text{C}} ). The nature of this phase transition has been a subject of some debate in the literature. Most studies agree that the phase transition is of a second-order nature xiao_crystal_2006 ; murtaza_magnetocaloric_2020 ; dublon_crystal_1976 ; atzmony_crystal-field-induced_1976 ; ouyang_magnetic_2005 ; herrero2006nature . However, studies based on perturbed angular correlation PhysRevB.68.014409 ; forker2007comment and resonant ultrasound spectroscopy driver2014multiferroic argue that the transition is first-order or close to tricritical in character. This discrepancy highlights the challenge of definitively characterizing magnetostructural transitions involving coupled magnetic and structural order parameters. Additionally, \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} undergoes a first-order phase transition at 42 K associated with an orthorhombic distortion (space group Imma ) and a spin reorientation ( T_{\text{SR}} ) xiao_crystal_2006 ; murtaza_magnetocaloric_2020 ; dublon_crystal_1976 ; atzmony_crystal-field-induced_1976 ; ouyang_magnetic_2005 . Since Co is a resource-critical metal, raising ethical and environmental concerns european_commision , partial substitution with other elements, such as Ni, can reduce the criticality of the compound. Our previous investigations of NdCoNi have revealed that the compound exhibits a T_{\text{C}} at 36 K, but no T_{\text{SR}} lunde_machine_2025 ; lunde_electronic_2025 . First-order magnetic transitions can exhibit high MCEs but are often accompanied by thermal hysteresis law_quantitative_2018 . In contrast, second-order magnetic transitions typically result in both lower thermal hysteresis and MCE. The MCE is quantified by the magnetic entropy change \Delta S_{\text{m}} and the adiabatic temperature change \Delta T_{\text{ad}} . To distinguish between the indirectly and directly determined \Delta T_{\text{ad}} in this work, we will denote these \Delta T_{\text{ad,ind}} and \Delta T_{\text{ad,dir}} , respectively. \Delta T_{\text{ad,ind}} can either be determined from S - T -diagrams constructed from heat capacity C_{\text{P}} data, or as \Delta T_{\text{ad,ind}}=-\Delta S_{\text{m}}(T/C_{\text{P}}) where \Delta S_{\text{m}} is determined from field-dependent magnetization isotherms M(H) . The latter method can be unreliable for first-order phase transitions and at low temperatures, where C_{\text{P}} approaches zero, and should be applied with caution to avoid an area of phase coexistence. \Delta T_{\text{ad,dir}} can be determined by measuring the temperature change under application of a magnetic field. This direct \Delta T_{\text{ad,dir}} is generally more reliable than the indirect \Delta T_{\text{ad,ind}} , in particular for first-order magnetic transitions politova_magnetism_2024 . Pulsed-field measurements can be used to accurately determine \Delta T_{\text{ad,dir}} by ensuring adiabatic conditions in the experiment salazar_mejia_high-field_2023 . In this work, \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2\hskip 0.90417pt--\hskip 0.90417ptx\/}}}\text{Ni}{\vphantom{\text{X}}}_{\smash[t]{\text{x\/}}} with (0 \leq x \leq 1) were studied to investigate the influence of Ni substitution on the MCE. The crystal structures, as well as local and bulk magnetic moments, were investigated in detail to understand how these properties are influenced by the partial substitution of Co with Ni. Studying the magnetic properties of a material is essential to understand the origin of its MCE. Therefore, neutron scattering was used to probe both magnetic and crystal structures of the compounds. These experiments are important for understanding the relationship between crystal structure, magnetic ordering, and MCE, to optimize the material performance. II Methods Five \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2\hskip 0.90417pt--\hskip 0.90417ptx\/}}}\text{Ni}{\vphantom{\text{X}}}_{\smash[t]{\text{x\/}}} ( x= 0, 0.25, 0.50, 0.75, 1) compositions ( \sim 1 g batches) were synthesized by arc melting (Edmund Bühler, Compact Arc Melter MAM-1) under argon atmosphere ( \geq 99.99 %, Nippon Gases) from high-purity elements ( \geq 99 %, Goodfellow), with 3 wt.% excess of Nd to compensate for evaporation losses macaluso_challenges_2012 . The chamber was evacuated and purged with argon gas three times, and left under a final pressure of 0.7 bar. The ingots were turned and remelted four times, followed by 72 hours of annealing at 1073 K and 72 hours at 833 K in evacuated and sealed quartz tubes to improve homogeneity. The final products were cooled to room temperature at a rate of 2 K/min and stored under argon atmosphere to prevent oxidation. Microstructure and chemical compositions were characterized using a JEOL JSM-7900F scanning electron microscope (SEM) equipped with an Oxford Instruments AZtec Ultim Max 65 energy-dispersive x-ray (EDS) analyzer. Bulk pieces of the samples were embedded in ”polyfast” resin, ground, and polished. Back-scattered electron (BSE) mode was utilized to obtain elemental contrast, and EDS mode was used for elemental analysis, both using an acceleration voltage of 15 kV. Synchrotron radiation powder x-ray diffraction (SR-PXD) data were obtained at BM01 at the Swiss-Norwegian Beamlines (SNBL) of the European Synchrotron Radiation Facility (ESRF) in Grenoble, France. Powder samples were prepared in 0.3 mm quartz capillaries and measured using the PILATUS2M detector SNBL while rotating the capillary 360 degrees. All samples were measured at room temperature with a wavelength of 0.49537 Å. Additionally, \text{NdCo}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} was cooled to 80 K using a nitrogen blower, and measured with a wavelength of 0.71859 Å while heating with a rate of 1 K/min to 120 K, followed by 5 K/min to 300 K. The data were integrated with the SNBL Bubble