Burst-mode fs-laser direct writing for full-thickness oxidation of Ta thin films
Lina Grineviciute 1,∗ , Hsin-Hui Huang 2,3,4∗ , Haoran Mu 2,4 , Nguyen Hoai An Le 2 , Andrew Siao Ming Ang 2 , Dan Kapsaskis 2 , Tomas Katkus 2 , Saulius Juodkazis 2,4,5 · 2026
Read Burst-mode fs-laser direct writing for full-thickness oxidation of Ta thin films by Lina Grineviciute 1,∗ , Hsin-Hui Huang 2,3,4∗ , Haoran Mu 2,4 , Nguyen Hoai An Le 2 , Andrew Siao Ming Ang 2 , Dan Kapsaskis 2 , Tomas Katkus 2 , Saulius Juodkazis 2,4,5 (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2602-06444.txt.
Description
Writing oxide patterns directly on a metal film with a laser usually risks blasting the film away. Lina Grineviciute and 7 co-authors show a gentler route for tantalum. Using a burst mode that packs ultra-short pulses into pico- and nano-scale bursts at high repetition, they oxidized a thin tantalum film through its full thickness.
The oxidized lines came out flat, transparent, and only a few micrometers wide, with no ablation or debris. Rastering produced self-organized ripples of oxide with wavelength-scale spacing, aligned to the beam's polarization. Comparing burst recipes clarified how heat deposits during writing. The self-guided process promises sub-wavelength oxide patterning without annealing steps.
Catalog record
| CREATOR | Lina Grineviciute 1,∗ , Hsin-Hui Huang 2,3,4∗ , Haoran Mu 2,4 , Nguyen Hoai An Le 2 , Andrew Siao Ming Ang 2 , Dan Kapsaskis 2 , Tomas Katkus 2 , Saulius Juodkazis 2,4,5 |
|---|---|
| YEAR | 2026 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 45 KB |
| VERSION | 1.0 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2602-06444