Investigating ultra-thin 4H-SiC AC-LGADs for superior radiation-hard timing applications
Jaideep Kalani, Saptarshi Datta, Ganesh J Tambve, Prabhakar Palni · 2026
Read Investigating ultra-thin 4H-SiC AC-LGADs for superior radiation-hard timing applications by Jaideep Kalani, Saptarshi Datta, Ganesh J Tambve, Prabhakar Palni (2026) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2601-16925.txt.
Introduction
Jaideep Kalani, Saptarshi Datta, Ganesh Tambve, and Prabhakar Palni test thin sensors for fast particle hits. Such sensors, called LGADs, time hits to tens of trillionths of a second. Hard radiation zones need that speed to sort hits. Their 2026 preprint studies ultra-thin 4H-SiC forms of the sensor. The films run less than fifty microns thick.
A sim tool named WeightField2 models the films' acts. Thin films react fast but give small signals. The team weighs that trade for harsh zones. Good thin sensors could serve collider and space work. They may also serve fast scan tools in care.
Catalog record
| CREATOR | Jaideep Kalani, Saptarshi Datta, Ganesh J Tambve, Prabhakar Palni |
|---|---|
| YEAR | 2026 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 42 KB |
| VERSION | 1.0 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2601-16925
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Investigating ultra-thin 4H-SiC AC-LGADs for superior radiation-hard timing applications Jaideep Kalani, Saptarshi Datta, Ganesh J Tambve, Prabhakar Palni Abstract The Low Gain Avalanche Diodes (LGADs) are promising particle detectors for timing resolution better than 50 50 ps under a high radiation environment. This study investigates n-in-p LGAD architecture, focusing on ultra-thin sensors of thickness less than 50 μ 50\ \upmu m using the WeightField2 program. The capabilities of WeightField2 are demonstrated by comparing its results with irradiation measurements from an FBK LGAD wafer, showing good agreement across unirradiated and neutron-irradiated conditions. This paper presents device simulations in High Luminosity LHC conditions (lifetime integrated fluence 𝒪 ( 10 14 ) n eq cm − 2 \mathcal{O}(10^{14})\ \mathrm{n_{eq}~cm^{-2}} , temperature ≈ 243 K \approx 243\ \mathrm{K} ), and taking into account radiation damage, gain reduction due to fluence, and lattice defects. It is shown that a 20 μ \upmu m thick sensor achieves the best timing performance. Among Silicon (Si), Diamond (C), and 4H-Silicon Carbide (4H-SiC), we found 4H-SiC to be the most promising: it provides the highest gain value for a fixed thickness and gain implant layer configuration, and best retains high charge collection value and timing capability under increasing fluence up to 50 × 10 14 n eq cm − 2 50\times 10^{14}\ \mathrm{n_{eq}~cm^{-2}} . A time resolution less than 25 ps is reported with different gain implant concentrations for a 20 μ 20\ \upmu m 4H-SiC sensor. This work presents the potential of SiC-based LGADs in high-radiation collider environments. 1 Introduction The High-Luminosity Large Hadron Collider (HL-LHC) project aims to increase the instantaneous luminosity to \approx 7.5\times 10^{34}\ \text{cm}^{-2}\text{s}^{-1} [ 1 ] . These upgrades, including other future high-energy physics experiments ( [ 2 ] , [ 3 ] , [ 4 ] ) seeking larger event statistics, will lead to severe pile-up conditions. The Low Gain Avalanche Diodes (LGADs) offer a timing resolution of approximately 50 ps or lower ( [ 5 ] , [ 6 ] ), along with spatial resolution below 100\ \upmu m (depending on pixel dimensions [ 7 ] ). The LGADs provide an effective solution to mitigate high pile-up scenarios. Therefore, this technology has been qualified for use in the MIP Timing Detector (MTD) detector ( [ 8 ] , [ 9 ] ) of CMS and the High Granularity Timing Detector (HGTD) [ 10 ] of ATLAS for HL-LHC operations. The LGADs outperform standard PIN diodes by introducing an extra gain layer for controlled avalanche multiplication of charge carriers in addition to the drift and diffusion mechanisms. The gain layer is usually a thin, highly doped region with a moderate gain factor (gain \sim 10-30 ). This increases the signal amplitude while preserving a high signal-to-noise ratio without the dangers of noise-induced breakdown. A key advancement is the AC-LGAD (AC-coupled) design (Figure 1 ), which mitigates DC-LGAD [ 11 ] (DC-coupled) limitations such as charge-sharing inefficiencies and pixelation constraints due to direct coupling of the readout to the gain layer. In AC-LGADs, the readout is capacitively coupled to the gain layer through an insulating layer; this enables continuous gain layer (increasing fill factor), and improved spatial resolution (much lower than pixel size). These, along with compatibility with modern semiconductor processing techniques, make AC-LGADs suitable for high-granularity, high-resolution timing and tracking (4D) detectors. [ 12 ] Figure 1 : A typical AC-LGAD architecture This study examines the time resolution ( \sigma_{t} ) of an LGAD as a function of operational conditions like bias voltage and radiation damage, including device characteristics like gain implant (G.I.) layer concentration, thickness, and bulk material. This work evaluates three different bulk materials, including 4H Silicon Carbide (4H-SiC), where H denotes hexagonal symmetry and a 4-layer per unit cell poly-type of SiC ( [ 13 ] [ 14 ] ). It is well-suited for detector applications due to high saturation drift velocity of carriers, high bandgap (so low intrinsic charge concentration), high breakdown field, and good thermal conductivity. The operational qualities for a 4H-SiC-based LGAD are presented and compared to a Si-based LGAD with similar configurations to demonstrate the former’s superiority as a radiation-hard 4D detector. Throughout this study, SiC is used as an alias for the 4H-SiC polytype for brevity. 1.1 Theoretical framework of the LGAD mechanism The impinging minimum ionising particle (MIP) produces primary e^{-}h^{+} pairs while passing through the sensor bulk; these primary carriers further produces cascade of secondary carriers while passing through the gain layer. A calculation using the Shockley-Ramo theorem ( [ 15 ] , [ 16 ] , [ 17 ] ) gives the net current (in full signal time) as: I\propto N_{gen}~q_{0}~v_{sat}~(G/d) [ 18 ] . Here N_{gen} is the number of primary charge carriers generated by the MIP, q is the carrier’s charge, v_{sat} is the saturation velocity of the charge carrier in the sensor bulk, G is the gain value of the sensor, and d is the thickness of the sensor. This is the key advantage of the LGAD design over a typical semiconductor sensor with a diode-like design. Clearly the signal is amplified from N_{gen}~q_{0} for a typical diode to a larger factor for LGADs. In LGADs, impact ionisation is the crucial mechanism providing the gain factor. The Massey model [ 19 ] is an empirical framework used to simulate such a mechanism. The ionisation rate, characterised by the ionisation coefficients \alpha_{n} and \alpha_{p} for electrons and holes, respectively, follows an empirical relationship: \alpha_{n,p}(T)=A_{n,p}(T)\exp\left(-\frac{B_{n,p}(T)}{E}\right), where A_{n,p}(T) and B_{n,p}(T) are material-dependent parameters that account for temperature variations, and E is the local electric field. Furthermore, material-dependent parameter B_{n,p}(T) is represented as B_{n,p}(T)=C_{n,p}+D_{n,p}\cdot T . These A_{n,p} , C_{n,p} , and D_{n,p} are six model parameters which are fine-tuned by comparing simulations and empirical data. Corrections dependent on temperature and doping concentration are introduced to make the model more accurate. Comparative TCAD studies ( [ 20 ] , [ 21 ] ) demonstrate that the Massey model of LGAD mechanism agrees with experimental data across multiple regimes, including gain versus bias voltage, gain versus temperature, and breakdown voltage predictions. We used the Massey model in all simulations and the model parameters are fixed within the WF2 simulation framework as per published dafault values of the Massey model [ 19 ] . 1.2 Radiation damage in LGAD The radiation damage in an LGAD is broadly of two categories: surface damage and bulk damage [ 22 ] . The former is due to ionisation energy loss; the particle traversing through the sensor ionises the sensor bulk by energy deposition and forms \mathrm{e^{-}/h^{+}} pairs. Some of these form at the interface of the sensor bulk and the oxide layer, and cannot recombine properly, leaving trapped charges at the interface. A fraction of the non-ionising energy loss, causes bulk damage to the lattice. The impinging particle, like hadrons, forms Frankel pairs [ 23 ] . Some of these pairs get recombined, while others migrate through the lattice and can interact with the other impurities present in the bulk, producing point defects. Furthermore, these migrating Frankel pairs have enough energy to create further ionisation and atomic displacements. Here the radiation damage is measured in equivalent 1\,\text{MeV} neutron fluence