Read Defect–Limited Efficiency of Pnictogen Chalcohalide Solar Cells by Cibrán López, Seán R. Kavanagh, Pol Benítez, Edgardo Saucedo, Aron Walsh, David O. Scanlon, Claudio Cazorla (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2512-01531.txt.
Introduction
Cibran Lopez and co-authors ask why a new class of solar cells lags its promise. Pnictogen chalcohalides soak up light well. They are non-toxic and can be made at low heat. Yet top cells stay well below ten percent efficiency. Their ideal cap is far higher.
The team blames defects in the material. Defects trap charge and waste light energy as heat. They map which defects hurt most. That map tells makers what to fix first in growth. Fixing the worst defects could lift these green cells toward real use in roofs and farms.
Catalog record
| CREATOR | Cibrán López, Seán R. Kavanagh, Pol Benítez, Edgardo Saucedo, Aron Walsh, David O. Scanlon, Claudio Cazorla |
|---|---|
| YEAR | 2025 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 46 KB |
| VERSION | 1.0 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2512-01531
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Defect–Limited Efficiency of Pnictogen Chalcohalide Solar Cells Cibrán López, Seán R. Kavanagh, Pol Benítez, Edgardo Saucedo, Aron Walsh, David O. Scanlon, Claudio Cazorla Abstract Pnictogen chalcohalides (MChX) have recently emerged as promising nontoxic and environmentally friendly photovoltaic absorbers, combining strong light absorption coefficients with favorable low-temperature synthesis conditions. Despite these advantages and reported optimized morphologies, device efficiencies remain below 10%, far from their ideal radiative limit. To uncover the origin of these performance losses, we present a systematic and fully consistent first-principles investigation of the defect chemistry across the Bi-based chalcohalide family. Our results reveal a complex defect landscape dominated by chalcogen vacancies of low formation energy, which act as deep nonradiative recombination centers. Despite their moderate charge-carrier capture coefficients, the high equilibrium concentrations of these defects reduce the theoretical maximum efficiencies by 6% in BiSeI and by 10% in BiSeBr. In contrast, sulfur vacancies in BiSI and BiSBr are comparatively benign, presenting smaller capture coefficients due to weaker electron-phonon coupling. Interestingly, despite its huge nonradiative charge-carrier recombination rate, BiSeI presents the best conversion efficiency among all four compounds owing to its most suitable bandgap for outdoor photovoltaic applications. Our findings identify defect chemistry as a critical bottleneck in MChX solar cells and proposes chalcogen-rich synthesis conditions and targeted anion substitutions as effective strategies for mitigation of detrimental vacancies. Keywords: first-principles calculations, emergent photovoltaics, pnictogen chalcohalides, defect chemistry, electron-phonon coupling I Introduction The global transition toward sustainable and low-carbon energy systems has placed photovoltaics (PV) at the forefront of research and technological innovation 1 . As a clean, renewable, and abundant energy source, PV provides a direct route to decarbonizing electricity generation. However, photovoltaic technologies must satisfy stringent performance criteria, including high power conversion efficiency (PCE), long-term stability, scalability, and low-cost manufacturing, while maintaining environmental sustainability 2 . Figure 1: MChX photovoltaic absorbers. a. MChX orthorhombic crystal structure (space group Pnma ) characterized by columnar motifs held together by weak dispersion forces. Pnictogen, chalcogen and halide atoms are represented by violet, yellow and dark pink spheres, respectively. b. A systematic study of MChX point defects disentangles general trends. Four different Bi-based chalcohalides and all possible intrinsic point defects have been systematically analyzed in this study. The van der Waals radius of each species is marked for reference. Pnictogen chalcohalides (MChX, Fig. 1 a) have recently emerged as a promising class of photovoltaic absorbers owing to their nontoxicity, bandgaps in the range of 1.2–2.1 eV, light absorption coefficients spanning from 25 to 66 \mu m -1 3 ; 4 ; 5 , exceptional thermodynamic stability 6 ; 7 , and low synthesis temperatures (below 300^{\circ} C) 8 ; 7 . MChX materials are often described as “perovskite-inspired” semiconductors 9 , since their electronic structures resemble those of lead-halide perovskites, despite crystallizing in different crystal lattices. In particular, such materials are believed to present defect tolerance, stemming from antibonding and bonding character of their valence and conduction bands, respectively. Actually, the closely related family of binary chalcogenides (e.g., Sb 2 S 3 , Sb 2 Se 3 , and Bi 2 S 3 ) has been shown to exhibit genuine defect-tolerance features 10 ; 11 ; 12 . Despite these encouraging prospects, experimental PCEs of MChX solar cells remain below 10%, far from their ideal Shockley-Queisser limit obtained from detailed balance (e.g., 30% in BiSeI) 13 ; 14 . Understanding the origin of this performance decline is therefore essential for realizing their full technological potential and enabling large-scale deployment. While efficiency losses can arise from synthesis routes, morphology, or even device architecture, recent studies indicate that such extrinsic factors are not the primary bottlenecks in MChX absorbers 9 ; 5 . Instead, intrinsic defects are increasingly recognized as the decisive factor. Extended, high-dimensional defects such as grain boundaries, dislocations, and precipitates, although typically detrimental in many semiconductors, are found to be noncritical in MChX 8 since their quasi-one-dimensional chain-like framework appears to hinder charge recombination 15 ; 16 ; 17 . On the other hand, point defects, often overlooked in early assessments, may dominate nonradiative recombination and ultimately constrain device performance 18 ; 19 . Recent theoretical studies on BiSeI 19 and their binary counterparts Sb 2 S 3 20 and Sb 2 Se 3 21 have identified chalcogen vacancies as dominant recombination centers, drastically reducing their maximum PCE. Experimental works have also reported similar defect behaviour in related materials 22 . Consequently, sulfur and selenium vacancies (V S and V Se ) might play a significant detrimental role in the broader MChX family. Yet, their relative impact on device performance may differ substantially depending on the interplay of the local chalcogen–halogen environment, which motivates a systematic, cross-material computational investigation of point defects on pnictogen chalcohalides. Systematically estimating point-defect behaviour (e.g., formation energies and carrier capture coefficients) in MChX is highly nontrivial 23 ; 24 . First-principles calculations of defect formation energies and carrier capture processes 25 are computationally demanding and highly sensitive to methodological choices 26 . Comparisons across different studies are often complicated 27 ; 28 ; 29 by variations in input parameters or approximations, often relying on error cancellation 30 , which hinders finding any general trends. By contrast, a consistent, family-wide study performed with identical computational protocols offers a robust framework to disentangle chemical effects from methodological artifacts (Fig. 1 b) 19 ; 31 . Here, we present a comprehensive investigation of the defect chemistry of four representative pnictogen chalcohalides (BiSI, BiSeI, BiSBr, and BiSeBr) using advanced first-principles density functional theory (DFT) calculations. A systematic comparison of all of them allows identifying selenium vacancies as the most detrimental defects within this family; in particular, they introduce deep electronic transition states near the Fermi level and enhance electron–phonon coupling, thus promoting nonradiative recombination in BiSeI and BiSeBr. In contrast, sulfur vacancies in BiSI and BiSBr are comparatively benign, owing to weaker electron-phonon coupling, despite presenting similar formation energies. This striking contrast originates from the larger ionic radius and higher polarizability of selenium atoms, which enhance lattice distortions around V Se , suggesting that the chemical environment (specifically, the interplay between chalcogen and halogen anions) dictates charge recombination activity in MChX. This work establishes design principles for defect engineering in pnictogen chalcohalides, while also offering a generalizable framework applicable to other emergent photovoltaic materials. II Results MChX crystallize into an orthorhombic phase (space group Pnma ) characterized by one-dimensional columns held together by weak van der Waals forces (Fig. 1 a) 9 , closely resembling the structure of binary pnictogen chalcogenides (Sb 2 S 3 , Sb 2 Se 3 and Bi 2 Se 3 15 ). Our DFT geometry optimizations for MChX yield lattice parameters that are in very good agreement with the available experimental data 3 ; 9 (Supplementary Table I). According to previous first-principles calculations and experimental observations 8 ; 7 , MChX are thermodynamically stable against phase separation into secondary phases (Supplementary Fig. 1) and present indirect bandgaps in the range of 1 to 2 eV (Supplementary Fig. 2). II.1 Defect Formation Energies Point defects play a pivotal role in the optoelectronic performance of semiconductors. They can compensate for doping-induced electrical imbalance, shift the Fermi energy level ( E_{\rm F} ), and act as deep nonradiative