The plastic flow of polycrystalline solids

Miguel Lagos · 2025

Read The plastic flow of polycrystalline solids by Miguel Lagos (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2510-27242.txt.

Introduction

Miguel Lagos offers a fresh model of how metals bend for good in this 2025 paper. Most metals are polycrystalline, built from many small crystal grains packed tight. When stressed past a point, the metal keeps its new shape instead of springing back. Old accounts blame cracks and holes inside the metal. Lagos instead pictures grains that slide past each other.

In his model, each grain is a rough block that fills space with no gaps. Neighbors slide when the shear force, a sideways push, passes a set level. The math can be solved in full, giving two regimes: normal bending and a softer superplastic one. For nickel alloys and stainless steels, the model's numbers match lab tests closely.

Catalog record

CREATORMiguel Lagos
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE15 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2510-27242

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

The plastic flow of polycrystalline solids Miguel Lagos Abstract A polycrystalline solid is modelled as an ensemble of random irregular polyhedra filling the entire space occupied by the solid body, leaving no voids or flaws between them. Adjacent grains can slide with a relative velocity proportional to the local shear stress resolved in the plane common to the two sliding grains, provided it exceeds a threshold. The local forces associated to the continuous grain shape accommodation for preserving matter continuity are assumed much weaker. The model can be solved analytically and for overcritical conditions gives two regimes of deformation, plastic and superplastic. The plastic regime, from yield to fracture, is dealt with. Applications to nickel superalloys and stainless steels give impressive agreement with experiment. Most work of the last century relies on postulating pre–existent cracks and voids to explain plastic deformation and fracture. The present model gives much better results. Fracture in solid materials has been dealt with for hundred years with Griffith’s theory Griffith , which posits that solid materials have pre–existent cracks that concentrate tension and are able to evolve when subjected to stress. Griffith’s original work, neatly explaining why glass tensile strength is about 1/100 of what is expected from the breaking of the atomic bonds, has influenced a century of investigations. In this scheme a crack in a brittle medium grows when the energy released by its extension is greater than, or equal to, the energy demanded to form a new free surface. Fracture mechanics goes beyond brittle fracture incorporating dissipative terms accounting for energy losses at the evolving crack tips. Griffith noted that the strength of thin enough rods of glass increases for decreasing width, and prepared rods or fibers of glass and quartz fine enough to have tensile strengths of about 10^{6} psi, which is a figure close to the strength one would expect from the inter–atomic bindings. These high strengths stayed stable for a few hours, and then fall to much smaller constant values which depend on the diameter of the fiber. The final strengths, about hundred times smaller, were observed to be comparable in glass and metal wires. Griffith interpreted that the finest glass fiber diameters were smaller than the equilibrium mean pre–existent crack sizes, and then the fiber have less or no flaws at all, which explains the higher strength Griffith ; Kendall . Much later Irwin Irwin and Orowan Orowan extended the idea of the pre–existent flaws to ductile solids. Brittle character is ascribed to the ability of cracks under stress to propagate conserving their atomically sharp edges. Ductile solids are assumed to have a more complex evolution, the tip of the stressed crack blunts by dissipative processes, broadens, splits and flows, demanding increasing effort to evolve Fineberg1 ; Kolvin ; Svetlizky ; Heizler ; Noell . Within this view, as all bodies can be broken, pre–existent flaws are present in all polycrystalline solids, and their properties are an interesting matter of study Kendall . Anyway, the complete regime of plastic flow under Griffith’s hypothesis, from yield to fracture, is not more nor less than a detailed account of an avalanche of catastrophic failure events. The model for the polycrystalline solid reported here is exactly opposed to Griffith’s hypothesis and most of the subsequent developments on it. The solid is assumed as a perfect polycrystal, with no flaws at all, and is modelled by an ensemble of random irregular polyhedra filling the entire space occupied by the solid body, leaving no voids between them. Under strong enough applied stress, adjacent grains can slide with a relative velocity proportional to the local shear stress resolved in the plane shared by the two grain boundaries, when it exceeds a finite threshold \tau_{c} . The local forces induced by the continuous grain reshaping in order to preserve matter continuity are assumed much weaker than those causing sliding. The plastic flow is then controlled mainly by the local shear forces making contiguous grain boundaries to slide Lagos1 ; Lagos2 ; Lagos3 ; Lagos4 . Grain boundary sliding is governed by the microscopic mechanism explained in Refs. Lagos1 and Lagos2 , and partially observed in Refs. Qi ; Bellon and Fukutomi . Matter between adjacent grains, represented by an elastic plate immersed into a different elastic medium, buckles and corrugates at a critical shear stress operating along it. The consequent periodic stress field exerted on the two grain surfaces causes the release and capture of vacancies in alternate sectors of them. The consequent streams in closed loops between the crystalline surfaces assist their relative motion in opposite senses. Hence, a relative disorder in the atomic scale at the grain interfaces does not reduce, but helps grain sliding. The equations of motion for the plastic flow are derived with no additional hypotheses, and have two families of solutions, corresponding to plastic and superplastic deformation Lagos5 ; Lagos6 . The superplastic solutions have been studied in an already published series of papers and successfully applied to the main superplastic materials. The study of solids with normal ductility in this context was initiated in a couple of recent papers Lagos3 ; Lagos4 , and the purpose of this letter is to review the matching of the novel approach to normal ductility with the phenomenology of real materials. Data on the nickel Inconel superalloys and stainless steel AISI 316, of use in the combustion chamber of jet engines and nuclear reactors, were chosen to compare with because have special reliability. Our hypothesis is that plastic deformation takes place by only the action of the shear forces operating in the grain boundary faces, making adjacent grains to slide. Forces involved in the consequent continuous grain reshaping are of less importance. Additionally, the relative speed of the two neighbouring grains is proportional to the shear stress resolved in the plane of the common grain boundary, provided that this shear stress is greater than a threshold \tau_{c} . Assuming axial symmetry with respect to the z- axis, the stress tensor reads (\sigma_{ij})=\left(\begin{array}[]{ccc}\sigma_{\perp}&0&0\\ 0&\sigma_{\perp}&0\\ 0&0&\sigma\end{array}\right), (1) where a non–vanishing transversal stress \sigma_{\perp} is assumed because it will be demonstrated that plastic strain always induces such kind of stress, no matter the initial conditions. The hydrostatic pressure p=-(\sigma+2\sigma_{\perp})/3 (the minus sign is placed just to be consistent with pressure in a fluid) will prove to be an essential variable in the plastic flow. The relative motion of two neighbouring grains is proportional to the shear stress \tau_{z^{\prime}}=[\sigma_{x^{\prime}x^{\prime}}^{2}+\sigma_{y^{\prime}y^{\prime}}^{2}]^{1/2} operating in the common boundary plane between them, provided that \tau_{z^{\prime}}>\tau_{c} . Here (\sigma_{i^{\prime}j^{\prime}}) is the stress tensor ( 1 ) expressed in a rotated frame of reference with the z^{\prime} –axis normal to the plane of the two grain boundaries and with coincident x – and x^{\prime} – axes. Therefore, the relative velocity of the two adjacent grains is \displaystyle\Delta v_{i^{\prime}}=\begin{cases}\mathcal{Q}\,\sigma_{i^{\prime}z^{\prime}}\left(1-\displaystyle\frac{\tau_{c}}{\tau_{z^{\prime}}}\right),\,&i^{\prime}=x^{\prime},y^{\prime},\,\text{if }\,\tau_{z^{\prime}}>\tau_{c}\\ 0,&\text{ otherwise},\end{cases} (2) \displaystyle\Delta v_{z^{\prime}}\equiv 0,, where \mathcal{Q} is a coefficient depending only on the local pressure p and temperature T . By the procedure explained in Ref. Lagos1 the force law ( 2 ) can be written in terms of the strain rates \dot{\varepsilon}_{ij} instead of the relative velocities \Delta\vec{v} between adjacent grains, and expressed in the common (x,y,z) frame of reference. The

Read the complete text