Leakage current of high-fluence neutron-irradiated 8” silicon sensors for the CMS Endcap Calorimeter Upgrade

E. Zubaroglu · 2025

Read Leakage current of high-fluence neutron-irradiated 8” silicon sensors for the CMS Endcap Calorimeter Upgrade by E. Zubaroglu (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2510-17280.txt.

Introduction

The CMS HGCAL collaboration reports leak currents in neutron-hit silicon sensors in this 2025 paper. The sensors will serve a new fine-grained calorimeter at the Large Hadron Collider. An upgrade will raise clash rates near tenfold in the next runs. Sensors must shrug off huge neutron doses and still read well.

Hexagonal pads on eight-inch wafers fill over six hundred square meters in total. The team blasted sensors with neutrons at a range of dose levels. Leak current acts were mapped by sensor type and dose. Heat shifts of the current were tracked as well. Split blasts were tested as a way to curb cure time in tests.

Catalog record

CREATORE. Zubaroglu
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE61 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2510-17280

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Leakage current of high-fluence neutron-irradiated 8” silicon sensors for the CMS Endcap Calorimeter Upgrade E. Zubaroglu Abstract The HL-LHC will challenge the detectors with a nearly 10-fold increase in integrated luminosity compared to the previous LHC runs combined, thus the CMS detector will be upgraded to face the higher levels of radiation and the larger amounts of collision data to be collected. The High-Granularity Calorimeter will replace the current endcap calorimeters of the CMS detector. It will facilitate the use of particle-flow calorimetry with its unprecedented transverse and longitudinal readout/trigger segmentation, with more than 6M readout channels. The electromagnetic section as well as the high-radiation regions of the hadronic section of the HGCAL (fluences above 10 14 ​ n eq / cm 2 10^{14}~\mathrm{n_{eq}}/\mathrm{cm}^{2} ) will be equipped with silicon pad sensors, covering a total area of 620 m 2 620\text{\,}{\mathrm{m}}^{2} . Fluences up to 10 16 ​ n eq / cm 2 10^{16}~\mathrm{n_{eq}}/\mathrm{cm}^{2} and doses up to 1.5 MGy are expected. The sensors are processed on novel 8" p-type wafers with an active thickness of 300 µ ​ m 300\text{\,}\mathrm{\SIUnitSymbolMicro m} , 200 µ ​ m 200\text{\,}\mathrm{\SIUnitSymbolMicro m} and 120 µ ​ m 120\text{\,}\mathrm{\SIUnitSymbolMicro m} and cut into hexagonal shapes for optimal use of the wafer area and tiling. Each sensor contains several hundred individually read out cells of two sizes (around 0.6 cm 2 0.6\text{\,}{\mathrm{cm}}^{2} or 1.2 cm 2 1.2\text{\,}{\mathrm{cm}}^{2} ). To investigate the radiation-induced bulk damage, the sensors have been irradiated with neutrons at RINSC to fluences between 6.5 × 10 14 ​ n eq / cm 2 6.5\times 10^{14}~\mathrm{n_{eq}}/\mathrm{cm}^{2} and 1.4 × 10 16 ​ n eq / cm 2 1.4\times 10^{16}~\mathrm{n_{eq}}/\mathrm{cm}^{2} . Electrical characterization results are presented for full sensors, as well as for partial sensors cut from multi-geometry wafers with internal dicing lines on the HV potential within the active sensor area. Leakage current behaviour is investigated for various sensor types and fluence levels, including its temperature dependence. Finally, methods to limit the annealing time of the sensors during irradiation are investigated by analysing the impact of splitting high-fluence irradiations. 1 1 footnotetext: Corresponding author. Email: [email protected] 1 Introduction The Large Hadron Collider (LHC) [ 1 ] will enter its High-Luminosity phase (HL-LHC) in 2030. It will challenge the detectors with a nearly 10-fold increase in integrated luminosity compared to the previous LHC runs combined [ 2 ] . Therefore, the CMS [ 3 ] detector will be upgraded to handle the higher levels of radiation and the larger amounts of collision data to be collected. The CMS endcap calorimeter (CE), also known as High-Granularity Calorimeter (HGCAL), will replace the current endcap calorimeters of the CMS detector [ 4 ] . It will facilitate the use of particle-flow calorimetry with its unprecedented transverse and longitudinal readout/trigger segmentation, with more than 6M readout channels. The electromagnetic section as well as the high-radiation regions of the hadronic section of the CE (fluences above 1\times 10^{14} 1-MeV neutron-equivalents per square centimetre - \mathrm{n_{eq}}/\mathrm{cm}^{2} ), will be equipped with silicon pad sensors, covering a total area of 620 m 2 . Integrated fluences up to 1\times 10^{16}~\mathrm{n_{eq}}/\mathrm{cm}^{2} are expected at the end of its 10-year operation at the HL-LHC. The silicon sensors are processed on novel 8” p-type wafers with an active thickness of 300\text{\,}\mathrm{\SIUnitSymbolMicro m} , 200\text{\,}\mathrm{\SIUnitSymbolMicro m} and 120\text{\,}\mathrm{\SIUnitSymbolMicro m} and cut into hexagonal shapes for optimal use of the wafer area and tiling. Each sensor contains several hundred individually read-out cells of two main sizes: around 0.6\text{\,}{\mathrm{cm}}^{2} for HD (High Density) sensors and 1.2\text{\,}{\mathrm{cm}}^{2} for LD (Low Density) sensors. In order to investigate the radiation-induced bulk damage, the sensors have been irradiated with neutrons at RINSC (Rhode Island Nuclear Science Centre, US) to target fluences between 6.5\times 10^{14}~\mathrm{n_{eq}}/\mathrm{cm}^{2} and 1.4\times 10^{16}~\mathrm{n_{eq}}/\mathrm{cm}^{2} . This work presents electrical characterization (IV) studies conducted between 2020 and 2024. It includes the dataset analysed in [ 5 ] , referred to as the version 1 campaign, as well as the newly analysed version 2 campaign. In the latter, the target fluence maximum was 40 ~\% above the fluence of 1\times 10^{16}~\mathrm{n_{eq}}/\mathrm{cm}^{2} of the version 1 campaign. This increase was done to account for uncertainty in the integrated fluence prediction for the final years of the HL-LHC operation. To ensure reliable operation under higher fluence, the version 2 sensors have an upgraded layout aimed at improving high voltage (HV) performance. Moreover, this study also includes additional sensor geometry variants introduced in the version 2 campaign. The results of this work have been used to optimize the layout of the CE silicon section and to deploy thicker sensors in higher radiation regions. Additionally, the irradiation facility RINSC is investigated for a better understanding and control of the irradiation processes and procedures with emphasis on high-fluence irradiations. This paper is organized as follows: section 2 describes the version 2 prototypes of the CE silicon pad sensors, irradiated and measured in the campaign conducted after the publication of the previous study. Section 3 focuses on the RINSC irradiation facility, describing the process improvements to reduce in-reactor annealing times. Section 4 examines the leakage current distribution across the sensor area, with a particular focus on investigating potential effects related to the presence of internal guard rings and high-voltage lines in partial sensors. Section 5 deals with the relationship between leakage current and voltage, presenting key observations, including exponential leakage current behaviour under specific conditions. The leakage current-related damage rate coefficient ( \alpha ) for various sensor types and fluence levels is presented in section 6 , along with an evaluation of the fluence estimation methods applied during irradiation. Section 7 presents the temperature dependence of the leakage current to extract the silicon activation energy and identify the primary source of the leakage current. The conclusions of this study are summarized in section 8 . 2 Silicon sensors for the CMS endcap calorimeter upgrade The previous study [ 5 ] described the fabrication and design parameters of the silicon sensors for the CE project, focusing on full sensors from the version 1 prototype campaign. In contrast, the present study analysed version 2 prototypes introduced in 2021. An overview of the sensors examined in both campaigns is provided in table 1 . The table summarizes key sensor characteristics, including layout, thickness, and the delivered fluence (see section 3.2 ). The term "epi" refers to the epitaxial growth process, while "FZ" stands for float-zone process. The table also lists the material used for the irradiation holder (puck), and provides in-reactor annealing estimates derived from resistance temperature detector (RTD) measurements (see section 3.3 ). Table 1 : Overview of the irradiation rounds performed at RINSC. Version Round (Part) Thickness [ \upmu{} m] Process Layout Target fluence [ ~\mathrm{n_{eq}}/\mathrm{cm}^{2} ] Delivered fluence [ \mathrm{n_{eq}}/\mathrm{cm}^{2} ] A Puck material In-reactor annealing [min at 60\text{\,}\mathrm{\SIUnitSymbolCelsius} ] B Front C Back Average D 1 1 300 FZ full 6.5E+14 5.03\text{\times}{10}^{14} wood 9.9 - E - 1 2 200 FZ full 2.5E+15 1.78\text{\times}{10}^{15} wood 8.6 - E - 1 3 120 epi full 1.0E+16 8.07\text{\times}{10}^{15} wood 2199.3 - E 1 4 200 FZ full 2.5E+15 1.75\text{\times}{10}^{15} Acrylic - F - E - 1 5 200 FZ full 2.5E+15 1.76\text{\times}{10}^{15} Acrylic - F - E

Read the complete text