Etching-free dual lift-off for direct patterning of epitaxial oxide thin films
Jiayi Qin, Josephine Si Yu See, Yanran Liu, Xueyan Wang, Wenhai Zhao, Yang He, Jianbo Ding, Yilin Wu, Shanhu Wang, Huiping Han, Afzal Khan, Shuya Liu, Sheng’an Yang, Hui Zhang, Jiangnan Li, Qingming Chen, Jiyang Xie, Ji Ma, Wanbiao Hu, Jianhong Yi, Liang Wu, X. Renshaw, Wang · 2025
Read Etching-free dual lift-off for direct patterning of epitaxial oxide thin films by Jiayi Qin, Josephine Si Yu See, Yanran Liu, Xueyan Wang, Wenhai Zhao, Yang He, Jianbo Ding, Yilin Wu, Shanhu Wang, Huiping Han, Afzal Khan, Shuya Liu, Sheng’an Yang, Hui Zhang, Jiangnan Li, Qingming Chen, Jiyang Xie, Ji Ma, Wanbiao Hu, Jianhong Yi, Liang Wu, X. Renshaw, Wang (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2509-02618.txt.
Introduction
Jiayi Qin and twenty-one co-authors present a 2025 materials science paper on patterning epitaxial oxide films, single-crystal layers prized for electronic and magnetic functions. Standard patterning etches the film, risking damage, undercutting, and extra cost.
Their dual-lift-off method avoids etching entirely. A sacrificial layer of amorphous strontium aluminate acts like a photoresist that survives high growth temperatures. After the first lift-off clears the resist pattern, the oxide film is deposited, then the sacrificial layer is dissolved to lift away unwanted oxide. Patterns matched the resist shape closely. Demonstrations cover a ferromagnetic manganite film and a ferroelectric bismuth ferrite film. The authors describe the route as simple, precise, flexible, and cheaper than etching.
Catalog record
| CREATOR | Jiayi Qin, Josephine Si Yu See, Yanran Liu, Xueyan Wang, Wenhai Zhao, Yang He, Jianbo Ding, Yilin Wu, Shanhu Wang, Huiping Han, Afzal Khan, Shuya Liu, Sheng’an Yang, Hui Zhang, Jiangnan Li, Qingming Chen, Jiyang Xie, Ji Ma, Wanbiao Hu, Jianhong Yi, Liang Wu, X. Renshaw, Wang |
|---|---|
| YEAR | 2025 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 25 KB |
| VERSION | 1.0 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2509-02618
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Etching-free dual lift-off for direct patterning of epitaxial oxide thin films Jiayi Qin, Josephine Si Yu See, Yanran Liu, Xueyan Wang, Wenhai Zhao, Yang He, Jianbo Ding, Yilin Wu, Shanhu Wang, Huiping Han, Afzal Khan, Shuya Liu, Sheng’an Yang, Hui Zhang, Jiangnan Li, Qingming Chen, Jiyang Xie, Ji Ma, Wanbiao Hu, Jianhong Yi, Liang Wu, X. Renshaw, Wang Abstract Although monocrystalline oxide films offer broad functional capabilities, their practical use is hampered by challenges in patterning. Traditional patterning relies on etching, which can be costly and prone to issues like film or substrate damage, under-etching, over-etching, and lateral etching. In this study, we introduce a dual lift-off method for direct patterning of oxide films, circumventing the etching process and associated issues. Our method involves an initial lift-off of amorphous Sr 3 Al 2 O 6 or Sr 4 Al 2 O 7 ( a a SAO) through stripping the photoresist, followed by a subsequent lift-off of the functional oxide thin films by dissolving the a a SAO layer. a a SAO functions as a “high-temperature photoresist”, making it compatible with the high-temperature growth of monocrystalline oxides. Using this method, patterned ferromagnetic La 0.67 Sr 0.33 MnO 3 and ferroelectric BiFeO 3 were fabricated, accurately mirroring the shape of the photoresist. Our study presents a straightforward, flexible, precise, environmentally friendly, and cost-effective method for patterning high-quality oxide thin films. The application of functional thin films is heavily based on patterning, as exemplified by two of the most widely used technologies: thin-film transistors (TFTs) Geng et al. 2023 and complementary metal-oxide-semiconductor (CMOS) Lojek 2007 devices. In TFTs, patterning defines critical structures such as electrodes and semiconductor channels, enabling high-performance displays (e.g., LCDs, OLEDs). For CMOS, advanced patterning techniques (e.g., lithography) are indispensable for the fabrication of nanoscale transistors and interconnects in integrated circuits. Without precise patterning, neither technology could achieve the miniaturization, functionality, or performance demanded by modern electronics. Over the last few decades, research interest has grown mainly in functional oxide thin films due to their novel functionalities that either surpass or complement traditional TFT and CMOS technologies Schlom et al. 2008 ; Rondinelli and Spaldin 2011 ; Ogale et al. 2013 ; Tarancón and Pryds 2019 . However, the complexity involved in patterning epitaxial oxide thin films greatly limits their practical applications. Specifically, oxide thin films are often patterned via either wet or dry etching processes following traditional ultraviolet (UV) lithography (patterning of photoresist by development). Figure 1: (a) Schematic depiction of the two conventional patterning methods: etching (subtractive method) (left) and lift-off (additive method) (right). (b) Limitations of the etching process, which are inherently circumvented by employing the lift-off method. However, exposing the photoresist to high temperatures wuold lead to its deterioration. Consequently, to ensure compatibility with the high-temperature fabrication process, it is essential to develop an alternative to the conventional polymer-based, heat-sensitive photoresist (“high-temperature photoresist”). Etching is a top-down fabrication technique that begins from the surface of the material, removing material to create desired patterns (left panel of schematic Figure 1 (a)). However, etching processes present several limitations that warrant consideration (left panel of schematic Figure 1 (b)). Firstly, material compatibility can be a significant challenge, as certain materials are difficult to etch effectively. For example, Au or Pt are difficult and expensive to remove by etching due to their inertness. Secondly, achieving precise control over etch depth and material selectivity is challenging, leading to issues such as under-etching, over-etching, and unintended etching of adjacent layers, which can compromise pattern fidelity and layer integrity. Thirdly, the prevention of lateral etching poses considerable difficulties, which adversely affect the precision and dimensions of the etched features. Fourthly, it is arduous to prevent etching damage, including ion bombardment damage, resulting in physical damage to the material surface. Fifthly, many etching techniques utilize hazardous chemicals, necessitating careful handling and disposal practices to ensure safety. The cost and complexity of etching equipment, along with the maintenance required, can also pose significant barriers. Finally, some etching methods are time-consuming, particularly when high precision is needed Moreau 2012 ; Madou 2011 . In contrast to subtractive techniques like etching, lift-off is an additive method that employs a sacrificial layer to remove unwanted material from the substrate by detaching the sacrificial layer from the substrate. Therefore, lift-off avoids these problems, particularly as it minimizes the risk of over-etching, lateral etching, or harming the underlying substrate Biercuk et al. 2003 ; Banerjee et al. 2012 ; Trung et al. 2017 ; Yu et al. 2017 , as shown in the right panel of Figure 1 (a). For example, the standard commercial method for metal lift-off in patterning metal films involves the following steps: Initially, metallization is typically conducted via physical vapor deposition (PVD), which deposits metal across both the substrate and the photoresist. Organic solvents are subsequently employed as lift-off agents, stripping the remaining denatured photoresist and any attached metal, thus imprinting the resist pattern onto the metal layer Madou 2011 . However, unlike the room-temperature (RT) deposition of metal layers, monocrystalline epitaxial oxide thin films typically require high-temperature deposition, which can damage the photoresist and render it unsuitable for lift-off processes (right panel of Figure 1 (b)). Therefore, identifying a photoresist suitable for high-temperature applications or its alternatives is of significant importance. In this study, we introduce an etching-free dual lift-off technique specifically designed for the direct patterning of oxide films. Initially, analogous to the metal lift-off technique, we achieve the patterning of the amorphous oxides Sr 3 Al 2 O 6 Lu et al. 2016 or Sr 4 Al 2 O 7 Zhang et al. 2024 ; Nian et al. 2024 (SAO) by dissolving the underlying photoresist layer using isopropanol (IPA). In fact, SAO is the primary sacrificial layer for producing freestanding oxide thin films via its non-selective lift-off procedure Ji et al. 2019 ; Dong et al. 2019 ; Hong et al. 2020 ; Yang et al. 2022 ; Gu et al. 2022 ; Huang et al. 2022 ; Choo et al. 2024 , with its amorphous form maintaining high water solubility Han et al. 2019 . Here, amorphous Sr 3 Al 2 O 6 and Sr 4 Al 2 O 7 are collectively referred to as a SAO, with specific designations as a SAO326 and a SAO427, respectively. Therefore, the second lift-off step involves patterning the functional oxide thin films by dissolving and eliminating the a SAO layer in water. In other words, the a SAO layer acts as the “high-temperature photoresist”. We illustrate the advanced capabilities and versatility of this patterning technique in preserving film quality by patterning two representative ferroic materials, ferromagnetic La 0.67 Sr 0.33 MnO 3 (LSMO) Dagotto et al. 2001 and ferroelectric BiFeO 3 (BFO) Liu et al. 2022 . The precision of the oxide pattern in our research is directly correlated with the lithographic resolution of the photoresist. Enhanced exposure accuracy in lithography would correspondingly improve the accuracy of our technique, as the resulting pattern accurately mirrors the shape of the photoresist. Furthermore, considering that the substrate surface is almost unaltered after detaching the SAO layer, similar to a conventional photoresist Wang et al. 2023 ; An et al. 2024 ; Shen et al. 2025 , this