Investigating the Degradation of LATP Solid Electrolyte in High Alkaline Li − O 2 \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} Batteries

Tara P. Mishra, Zhuohan Li, Meghan Shen, Maximilian Jaugstetter, Livia P. Matte, Jung O. Park, Hyunjin Kim, Benjamin Lam, Karen Bustillo, Gerbrand Ceder, Mary Scott · 2025

Read Investigating the Degradation of LATP Solid Electrolyte in High Alkaline Li − O 2 \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} Batteries by Tara P. Mishra, Zhuohan Li, Meghan Shen, Maximilian Jaugstetter, Livia P. Matte, Jung O. Park, Hyunjin Kim, Benjamin Lam, Karen Bustillo, Gerbrand Ceder, Mary Scott (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2508-08654.txt.

Introduction

Tara Mishra and co-authors trace how a solid electrolyte falls apart inside humid lithium-oxygen batteries, in a 2025 study. Such batteries could store far more energy than today's lithium-ion cells at lower cost. The solid in question, called LATP, is a lithium aluminum titanium phosphate. In the damp, strongly alkaline cell, its surface starts to leach.

Fine microscopes and surface probes, backed by atom-level math, show phosphate and aluminum ions washing out on discharge. On charging, the lost ions rain back as new lithium and aluminum phosphate crusts on the surface. Cycle by cycle the crust piles up and the cell fades. What stays behind is a titanium-rich skin, which may shield the surface from worse side effects. The authors frame the loop, dissolve then re-deposit, as the core decay path, and a guide for tougher designs.

Catalog record

CREATORTara P. Mishra, Zhuohan Li, Meghan Shen, Maximilian Jaugstetter, Livia P. Matte, Jung O. Park, Hyunjin Kim, Benjamin Lam, Karen Bustillo, Gerbrand Ceder, Mary Scott
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE71 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2508-08654

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Investigating the Degradation of LATP Solid Electrolyte in High Alkaline Li − O 2 \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} Batteries Tara P. Mishra, Zhuohan Li, Meghan Shen, Maximilian Jaugstetter, Livia P. Matte, Jung O. Park, Hyunjin Kim, Benjamin Lam, Karen Bustillo, Gerbrand Ceder, Mary Scott Abstract In this study, we address the challenge of electrolyte degradation in all-solid-state humidified Li − O 2 \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} batteries, which offer high theoretical energy density and potential cost advantages over conventional lithium-ion batteries. Combining STEM-EELS, and XPS characterizations with DFT calculations, we reveal the leaching of PO 4 3 – \text{PO}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{4}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{4}}\text{3\hskip 0.90417pt--\hskip 0.90417pt}} and Al 3+ \text{Al}{\vphantom{\text{X}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{}}\text{3+}} ions from the Li 1.3 ​ Al 0.3 ​ Ti 1.7 ​ ( PO 4 ​ ) 3 \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{1.3}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{1.3}}\text{}}\text{Al}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{0.3}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{0.3}}\text{}}\text{Ti}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{1.7}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{1.7}}\text{}}\text{(}\text{PO}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{4}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{4}}\text{}}\text{)}\text{}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{3}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{3}}\text{}} (LATP) solid electrolyte upon battery discharge, caused by the highly alkaline environment. Upon charging, the leached ions precipitate as Li 3 ​ PO 4 \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{3}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{3}}\text{}}\text{PO}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{4}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{4}}\text{}} and AlPO 4 \text{AlPO}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{4}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{4}}\text{}} , which accumulate on the LATP surface and contribute to battery degradation. A Ti-rich layer is observed at the surface after a few cycles due to depletion of other cations. Our findings suggest that the degradation products are formed through repeated dissolution and precipitation in the discharge-charge cycles. Furthermore, our results indicate that the Ti-rich layer on the LATP surface can potentially reduce parasitic reactions. Our study provides mechanistic understanding of LATP solid electrolyte degradation in humidified Li − O 2 \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} cell, paving the way for designing more durable and efficient Li − O 2 \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} batteries. keywords American Chemical Society, L a T e X † † affiliation: Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: Contributed equally † † affiliation: Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: Contributed equally † † affiliation: National Center for Electron Microscopy, Molecular Foundry, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: Department of Materials Science and Engineering, University of California, Berkeley, California 94720, United States † † affiliation: Chemical Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: National Center for Electron Microscopy, Molecular Foundry, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: Department of Materials Science and Engineering, University of California, Berkeley, California 94720, United States † † affiliation: Battery Material TU, Samsung Advanced Institute of Technology, Samsung Electronics, Co., Ltd.,Suwon, Gyeonggi-do, Republic of Korea † † affiliation: Battery Material TU, Samsung Advanced Institute of Technology, Samsung Electronics, Co., Ltd.,Suwon, Gyeonggi-do, Republic of Korea † † affiliation: Department of Materials Science and Engineering, University of California, Berkeley, California 94720, United States † † affiliation: National Center for Electron Microscopy, Molecular Foundry, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † affiliation: Department of Materials Science and Engineering, University of California, Berkeley, California 94720, United States † † email: [email protected] † † affiliation: Department of Materials Science and Engineering, University of California, Berkeley, California 94720, United States † † affiliation: National Center for Electron Microscopy, Molecular Foundry, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States † † email: [email protected] † † abbreviations: IR,NMR,UV 1 Introduction The development of advanced energy storage systems has become paramount in addressing the growing demand for sustainable and efficient power sources. Among the various emerging technologies, lithium-air ( \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} ) batteries have garnered significant attention Lee et al. 2011 ; Capasso and Veneri 2014 ; Au et al. 2022 . The usage of \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} from the air as the active material allows a Li- \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} battery to achieve much higher gravimetric ( \approx 3500 Wh/kg) and volumetric ( \approx 3400 Wh/L) energy density (the values are based on the fully discharged state) than conventional Li-ion batteries ( \approx 100-300 Wh/kg and \approx 400-800 Wh/L), as well as potentially much lower cost as Li- \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} cathodes do not use expensive transition metals (e.g., Ni and Co). Zheng et al. 2008 ; Tan et al. 2013 ; Ma et al. 2015 ; Luntz and McCloskey 2014 ; Tian et al. 2021 . In a non-aqueous environment, the discharge and charge of the \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} are based on the formation of \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} Lu et al. 2010 : {}{}\mathrm{2}\,\mathrm{Li}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{+}}+2{}\mathrm{e}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{-}}+{}\mathrm{O}{\vphantom{\mathrm{X}}}_{\vphantom{\mathrm{2}}\smash[t]{\mathrm{2}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{2}}\mathrm{}}{}\mathrel{\hbox to0.0pt{\raisebox{0.94722pt}{$\mathrel{\mathop{\makebox[0.0pt]{\to}}\limits}$}\hss}\raisebox{-0.94722pt}{$\mathrel{\mathop{\makebox[0.0pt]{\to}}\limits}$}}{}{}{}\mathrm{Li}{\vphantom{\mathrm{X}}}_{\vphantom{\mathrm{2}}\smash[t]{\mathrm{2}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{2}}\mathrm{}}\mathrm{O}{\vphantom{\mathrm{X}}}_{\vphantom{\mathrm{2}}\smash[t]{\mathrm{2}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{2}}\mathrm{}}\quad({}\mathrm{E}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{0}}=2.96\text{ V}\text{ vs. }{}\mathrm{Li}/{}\mathrm{Li}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{+}}) (1) Despite its high theoretical energy density, the conventional Li - \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} battery faces some significant limitations. First, undesirable side reactions can occur between the highly oxidative radicals formed at the cathode during the charge and discharge cycles and organic liquid electrolytes McCloskey et al. 2011 ; Freunberger et al. 2011 or carbon cathodes McCloskey et al. 2012 ; Ottakam Thotiyl et al. 2013 . Secondly, the side reaction results in the formation of carbonates, which significantly increases the charge overpotential. McCloskey et al. 2012 . To overcome these issues, the use of all-solid-state Li - \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} batteries has been proposed Hong 1978 ; Adachi et al. 1996 ; MacFarlane et al. 1999 ; Knauth 2009 ; Chi et al. 2021 ; Le et al. 2019 ; Kim et al. 2022 , where stable solid electrolytes and carbon-free cathodes are utilized. However in solid-state \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} batteries, the insulating nature of the solid discharge product \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} can lead to limited practical discharge capacity Radin and Siegel 2013 ; Luntz et al. 2013 ; Radin et al. 2012 ; Viswanathan et al. 2011 ; Gerbig et al. 2013 ; Radin et al. 2015 . The limited electron transport restricts the continuous growth of \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} once the initial discharge products passivate the original cathode surfaces, leading to the “sudden death” of the Li- \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} cell during discharge Zhang et al. 2022 . To address this challenge, humidified \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} has been proposed, which chemically converts the growth-limited \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} into soluble and higher conductivity LiOH Liu et al. 2015 ; Ma et al. 2020 ; Kim et al. 2022 . In a humidified environment, the cell reaction also changes into a 4 \text{e}{\vphantom{\text{X}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{}}\text{\hskip 0.90417pt--\hskip 0.90417pt}} process and follows the equation Liu et al. 2015 ; Lu et al. 2014 : {}{}\mathrm{4}\,\mathrm{Li}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{+}}+4{}\mathrm{e}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{-}}+{}\mathrm{O}{\vphantom{\mathrm{X}}}_{\vphantom{\mathrm{2}}\smash[t]{\mathrm{2}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{2}}\mathrm{}}+2{}{}\mathrm{H}{\vphantom{\mathrm{X}}}_{\vphantom{\mathrm{2}}\smash[t]{\mathrm{2}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{2}}\mathrm{}}\mathrm{O}{}\mathrel{\hbox to0.0pt{\raisebox{0.94722pt}{$\mathrel{\mathop{\makebox[0.0pt]{\to}}\limits}$}\hss}\raisebox{-0.94722pt}{$\mathrel{\mathop{\makebox[0.0pt]{\to}}\limits}$}}{}4{}\mathrm{LiOH}\quad({}\mathrm{E}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{0}}=3.4\text{ V}\text{ vs. }{}\mathrm{Li}/{}\mathrm{Li}{\vphantom{\mathrm{X}}}^{\vphantom{\smash[t]{\mathrm{2}}}\hphantom{\mathrm{}}\mathrm{+}}) (2) Besides a slight reduction in the specific capacity, humidified \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} batteries have two significant advantages over traditional Li- \text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} systems. Firstly, the humidity facilitates ion transport by converting the insoluble solid \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} to soluble LiOH , thereby increasing the discharge capacity Gao et al. 2023 ; Dai et al. 2019 . Secondly, the theoretical discharge voltage is increased from 2.96 to 3.4 V (vs \text{Li}\text{/}\text{Li}{\vphantom{\text{X}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{}}\text{+}} ) thereby increasing the power output of the battery Kim et al. 2022 . In light of this, several chemical platforms for \text{Li}{-}\text{O}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2}}\text{}} batteries have been investigated, including LISICON, NASICON-type Li-ion conductors such as \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{1+x}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{1+x}}\text{}}\text{Al}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{x}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{x}}\text{}}\text{Ti}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2-x}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2-x}}\text{}}\text{(}\text{PO}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{4}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{4}}\text{}}\text{)}\text{}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{3}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{3}}\text{}} (LATP) and \text{Li}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{1+x}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{1+x}}\text{}}\text{Al}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{x}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{x}}\text{}}\text{Ge}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{2-x}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{2-x}}\text{}}\text{(}\text{PO}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{4}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{4}}\text{}}\text{)}\text{}{\vphantom{\text{X}}}_{\vphantom{\text{2}}\smash[t]{\text{3}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{3}}\text{}} (LAGP), thio-LISICON, glass-ceramics, and solid organic electrolytes Hong 1978 ; Kumar and Kumar 2010 ; Kichambare et al. 2012 ; Kanno and Murayama 2001 ; Kobayashi et al. 2008 ; Mizuno et al. 2005 ; Kondo et al. 1992 ; Takada et al. 1993 ; Fergus 2010 . Oxide Li-ion conductors such as garnets and layered oxides are sensitive to humidity and undergo \text{Li}{\vphantom{\text{X}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{}}\text{+}} / \text{H}{\vphantom{\text{X}}}^{\vphantom{\smash[t]{\text{2}}}\hphantom{\text{}}\text{+}} exchange and surface degradation under ambient conditions Cheng et al. 2018 ; Wang et al.

Read the complete text