Influence of thickness on magnetic properties of RF-sputtered amorphous CoNbZr thin films

Indujan Sivanesarajah, Leon Abelmann, Uwe Hartmann · 2025

Read Influence of thickness on magnetic properties of RF-sputtered amorphous CoNbZr thin films by Indujan Sivanesarajah, Leon Abelmann, Uwe Hartmann (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2505-22077.txt.

Introduction

Indujan Sivanesarajah, Leon Abelmann, and Uwe Hartmann show how film thickness steers the magnetism of amorphous CoNbZr films. Such cobalt-based films serve as soft magnetic materials in sensors, inductors, and flux concentrators. The team made RF-sputtered films of Co91Nb7Zr2 from 52 nm to 1040 nm thick. Average saturation magnetisation came out at 1.01 MA/m across the set.

As thickness grew, coercivity, the remanent-to-saturation ratio, and peak permeability all fell sharply. Domain patterns shifted too, from irregular domains at 52 nm to flux-closure structures above 208 nm. The changes fit a switch from Néel to Bloch type domain walls, expected near 84 nm.

Catalog record

CREATORIndujan Sivanesarajah, Leon Abelmann, Uwe Hartmann
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE30 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2505-22077

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Influence of thickness on magnetic properties of RF-sputtered amorphous CoNbZr thin films Indujan Sivanesarajah, Leon Abelmann, Uwe Hartmann Abstract Amorphous sputtered Co-based thin films are widely used as soft magnetic materials in applications such as sensors, inductors and magnetic flux concentrators. The magnetic properties of these films can be controlled by deposition parameters like film thickness, argon pressure, deposition rate and others. In this study, we present a detailed investigation of the magnetic properties of RF-sputtered Co 91 Nb 7 Zr 2 films with thicknesses ranging from 52 nm 52\text{\,}\mathrm{n}\mathrm{m} to 1040 nm 1040\text{\,}\mathrm{n}\mathrm{m} . These amorphous films exhibit an average saturation magnetisation of 1.01 ​ ( 4 ) MA / m 1.01(4)\text{\,}\mathrm{M}\mathrm{A}\mathrm{/}\mathrm{m} . As the film thickness increases, there is a significant decrease in coercivity, remanent-to-saturation magnetisation ratio M r / M s M_{\mathrm{r}}/M_{\mathrm{s}} , and maximum permeability. The change in macroscopic magnetic properties is also reflected by the domain structure. At a thickness of 52 nm 52\text{\,}\mathrm{n}\mathrm{m} , the remanent domain state shows irregular domains, while films thicknesses above 208 nm 208\text{\,}\mathrm{n}\mathrm{m} exhibit flux-closure domain structures instead. The thickness-dependent modifications are attributed to the transition between Néel and Bloch type domain walls, which is expected to occur at approximately 84 nm 84\text{\,}\mathrm{n}\mathrm{m} . Journal: Journal of Magnetism and Magnetic Materials 1 Introduction Amorphous alloys have gained substantial prominence as soft magnetic materials Shimada and Kojima [1982] , Sakakima [1983] , Herzer [2013] . These materials find versatile applications, ranging from magnetic sensors Meydan [1994] , Treutler [2001] , Morón et al. [2015] and inductors Korenivski [2000] , Ryłko et al. [2009] , Hsiang et al. [2022] to motors Hasegawa [2004] , Chai et al. [2020] , Enomoto et al. [2023] . Of particular interest is CoNbZr, a specific variant of amorphous Co-based alloys, known for its high susceptibility, large saturation magnetisation, and low coercive field de Wit et al. [1987] , Żuberek et al. [1992] . These properties make CoNbZr an ideal choice for integrated magnetic flux concentrators, establishing it as a material of paramount importance in this area Marinho et al. [2011] , He et al. [2018] , Maspero et al. [2021] . CoNbZr films are typically prepared by sputter deposition. However, the magnetic properties can be considerably influenced by details of the deposition process. For instance, different argon pressures can induce changes in the magnetic properties due to residual stress and morphology alterations, leading to the emergence of perpendicular magnetic anisotropy Peng et al. [2013] . Furthermore, Takahashi et al. revealed intriguing insights into how a compressed magnetic field magnetron sputtering technique affects key magnetic parameters Takahashi et al. [1989] . Of particular interest is the pivotal role that the film thickness plays in determining the magnetic performance of CoNbZr films. Observations involve an inverse relationship between film thickness and coercive field Li et al. [2007] , Cao and Zhou [2012] , Takahashi et al. [1989] and an increasing anisotropy field with increasing film thickness Katada et al. [2000] . An increasing film thickness also leads to an intriguing in-plane uniaxial magnetic anisotropy Cao and Zhou [2012] . However, despite extensive research in the field, a comprehensive understanding of how fine film thickness influences the magnetic properties in samples prepared through RF-magnetron sputtering is not yet existing. In particular, the intricate relationship between the film thickness and soft magnetic properties, such as permeability has not been thoroughly explored. This present study conducts an examination of the magnetic properties of RF-sputtered CoNbZr films at varying film thickness. 2 Materials and methods This section describes the fabrication of CoNbZr thin films and the methods used for their structural and magnetic characterisation. 2.1 Sample preparation CoNbZr films were deposited on Si - SiO 2 substrates of 8\text{\times}8\text{\,}\mathrm{m}\mathrm{m} , mounted on a rotating holder using RF-magnetron sputtering. The target composition Co 85 Nb 12 Zr 3 (at. %) was chosen due to the nearly zero magnetostriction ( \lambda_{\mathrm{s}}<10^{-6} ) Yamaguchi et al. [2015] . The target-to-substrate distance was set to 12\text{\,}\mathrm{c}\mathrm{m} . After reaching a base pressure below 1\text{⋅}{10}^{-8}\text{\,}\mathrm{m}\mathrm{b}\mathrm{a}\mathrm{r} , the films were deposited at an argon pressure of 1.7\text{⋅}{10}^{-3}\text{\,}\mathrm{m}\mathrm{b}\mathrm{a}\mathrm{r} at 100\text{\,}\mathrm{W} , while maintaining a deposition rate of 4.9(2)\text{\,}\mathrm{n}\mathrm{m}\mathrm{/}\mathrm{m}\mathrm{i}\mathrm{n} . By adjusting the sputtering time, films with thicknesses between 52\text{\,}\mathrm{n}\mathrm{m} and 1040\text{\,}\mathrm{n}\mathrm{m} were fabricated. For magnetic domain structure analysis via magnetic force microscopy (MFM), CoNbZr films were patterned into 20\text{\times}20\text{\,}\mathrm{\SIUnitSymbolMicro m} squares using a focused ion beam ( FEI Helios NanoLab 600 ) at an acceleration voltage of 30\text{\,}\mathrm{k}\mathrm{V} . Initially, an outer frame was patterned to coarsely remove material at a beam current of 21\text{\,}\mathrm{n}\mathrm{A} , followed by patterning of the final structures at a current of 6.5\text{\,}\mathrm{n}\mathrm{A} . No ion beam imaging was performed in the patterned area to prevent detrimental effects of Ga ions on the magnetic properties of the structures Fassbender and McCord [2008] . 2.2 Microstructural characterisation X-ray diffraction (XRD) patterns of the investigated samples were recorded at room temperature using a D8-A25-Advance diffractometer (Bruker, Karlsruhe, Germany) in Bragg-Brentano \theta-\theta geometry, with a goniometer radius of 280\text{\,}\mathrm{n}\mathrm{m} and Cu \mathrm{K}_{\alpha} radiation ( \lambda = 154.0596\text{\,}\mathrm{p}\mathrm{m} ). A 12\text{\,}\mathrm{\SIUnitSymbolMicro m} Ni foil served as a \mathrm{K}_{\beta} filter and a variable divergence slit was positioned at the primary beam side. A lynxeye detector with 192 channels was employed on the secondary beam side. Experiments were conducted in a 2\theta range of 30\text{\,}\mathrm{\SIUnitSymbolDegree}60\text{\,}\mathrm{\SIUnitSymbolDegree} with a step size of 0.013\text{\,}\mathrm{\SIUnitSymbolDegree} and a total scan period of 4\text{\,}\mathrm{h}\mathrm{o}\mathrm{u}\mathrm{r}\mathrm{s} . Electron diffraction patterns were acquired using a JEOL 2011 transmission electron microscope (TEM), equipped with a LaB 6 cathode and operated at 200\text{\,}\mathrm{k}\mathrm{V} . TEM slices were prepared by milling a 15\text{\times}5\text{\,}\mathrm{\SIUnitSymbolMicro m} area from the continuous film using a focused ion beam (FIB) followed by in situ lift-out with a micromanipulator Tomus and Ng [2013] . The elemental composition of the TEM slices was determined using an energy-dispersive X-ray spectroscopy (EDX) system. 2.3 Magnetic characterisation Magnetic measurements were performed on the as deposited films using a DMS Model 10 Vector Vibrating Sample Magnetometer (VSM) to measure both in-plane and out-of-plane magnetic hysteresis loops. The lateral sample size was 8\text{\times}8\text{\,}\mathrm{m}\mathrm{m} . The system was calibrated using a 0.3\text{\,}\mathrm{m}\mathrm{m} thick Ni foil with the same area and a mass of 156\text{\,}\mathrm{m}\mathrm{g} , assuming a magnetic moment of 8.61\text{\,}\mathrm{m}\mathrm{A}\mathrm{m}^{2} based on the specific magnetisation of Ni ( 55.1\text{\,}\mathrm{A}\mathrm{m}^{2}\mathrm{/}\mathrm{k}\mathrm{g} ) Crangle and Goodman [1971] . The diamagnetic contributions from the sample holder and Si substrate were subtracted as a linear background signal of 0.5\text{\,}\mathrm{\SIUnitSymbolMicro} , obtained by fitting the high-field branches of the in-plane hysteresis loops. For MFM analysis, a Bruker Multimode 8 atomic force microscope (AFM) was used. The AFM head was positioned between two electromagnetic coils capable of applying a field B of up to 80\text{\,}\mathrm{m}\mathrm{T} . Cantilevers (Olympus OMCL-AC240TS) coated with 40\text{\,}\mathrm{n}\mathrm{m} Co 85 Cr 15 were used to detect the stray magnetic fields of the samples Babcock et al. [1994] . 3 Results and discussion This section presents the structural and magnetic properties of the CoNbZr thin films, followed by a discussion of key hypotheses based on the observed trends. 3.1 Microstructural properties Figure 1: XRD patterns of sputtered CoNbZr films with varying thicknesses t . The y -axis represents intensity I and the x -axis represents the diffraction

Read the complete text