Non-isothermal stress relaxation in conventional and high-entropy metallic glasses and its relationship to the mixing and excess entropy
G.V. Afonin, S.L. Scherbakov, R.A. Konchakov, N.P. Kobelev, J.B. Cui, J.C. Qiao, V.A. Khonik · 2025
Read Non-isothermal stress relaxation in conventional and high-entropy metallic glasses and its relationship to the mixing and excess entropy by G.V. Afonin, S.L. Scherbakov, R.A. Konchakov, N.P. Kobelev, J.B. Cui, J.C. Qiao, V.A. Khonik (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2505-17889.txt.
Introduction
G V Afonin and co-authors compare metal glasses in a 2025 study on stress release under heat. Metal glasses are metals with a disordered structure, like glass. Some mix many elements in near equal shares, which gives them a high mixing entropy, a measure of disorder from the mix itself.
Six glasses, standard and high entropy kinds, were heated at a steady rate while heat flow and twist stress were tracked. The high entropy glasses held their stress far better. The team also built a score for how much disorder grows as the glass warms past a key range. That score tracks how deep the stress release runs.
Catalog record
| CREATOR | G.V. Afonin, S.L. Scherbakov, R.A. Konchakov, N.P. Kobelev, J.B. Cui, J.C. Qiao, V.A. Khonik |
|---|---|
| YEAR | 2025 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 24 KB |
| VERSION | 1.0 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2505-17889
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Non-isothermal stress relaxation in conventional and high-entropy metallic glasses and its relationship to the mixing and excess entropy G.V. Afonin, S.L. Scherbakov, R.A. Konchakov, N.P. Kobelev, J.B. Cui, J.C. Qiao, V.A. Khonik Abstract We performed calorimetric and torsion stress relaxation measurements upon linear heating of six conventional and high-entropy metallic glasses with the mixing entropy Δ S m i x \Delta S_{mix} ranging from 0.86 R 0.86R to 1.79 R 1.79R ( R R is the universal gas constant). It is shown that high-entropy metallic glasses ( Δ S m i x > 1.5 R \Delta S_{mix}>1.5\;R ) exhibit significantly greater resistance to stress relaxation. Based on calorimetric data, we calculated the excess entropy of glass relative to the counterpart crystalline state and introduced an entropy-based dimensionless parameter Δ S \Delta_{S} , which characterizes the rise of the entropy and structural disordering of glass in the supercooled liquid region. It is shown that the depth of stress relaxation at a given temperature decreases with Δ S m i x \Delta S_{mix} but increases with Δ S \Delta_{S} . Possible reasons for this relationship are discussed. 1 Introduction High-entropy alloys were first developed in the early 2000s and continue to attract researchers’ attention due to their unique properties compared to conventional structural alloys, i.e. high toughness and tensile ductility, ultra-high microhardness, exceptional wear resistance, corrosion and oxidation resistance, heat resistance, superelasticity, etc [ 1 , 2 , 3 , 4 , 5 ] . High-entropy alloys are usually characterized by the mixing entropy \Delta S_{mix}=-R\sum^{N}_{i=1}{c_{i}lnc_{i}} , where R is the universal gas constant, c_{i}\ is the atomic fraction of the i- th element, and N is the number of elements. The mixing entropy \Delta S_{mix} thus defined characterizes how much disorder is introduced upon alloy preparation. Alloys are usually considered to be high-entropy provided that \Delta S_{mix}\geq 1.5\ R , which is achieved in the compounds containing at least five main metallic components, each with a fraction of 5 to 35 at. \% [ 6 , 7 ] . The maximum of the mixing entropy is reached in the equiatomic compositions. In the early 2010s is was shown that rapid quenching of high-entropy melts can lead to the formation of a non-crystalline state [ 8 ] . These non-crystalline alloys have been referred to as high-entropy metallic glasses (HEMGs) [ 8 ] . Numerous studies over the past decade showed that HEMGs can combine a number of unique properties common to both conventional metallic glasses and crystalline high-entropy alloys: extremely high elastic limit, strength and hardness, wear/scratch and corrosion resistance, superplastic formability as well as the ability for polishing to an almost atomically smooth surface, etc. [ 9 , 10 ] . The non-crystalline structure of HEMGs provides a thermodynamic driving force for structural relaxation, which leads to changes in various physical properties during physical aging. However, despite intensive studies over the past decade [ 11 ] , the role of the high-entropy state in the relaxation behavior of HEMGs and their physical properties still remains uncertain [ 12 ] . In particular, it is largely unclear whether and how the mixing entropy \Delta S_{mix} affects HEMGs’ relaxation ability and are there any specific parameters suitable for a characterization of physical properties of HEMGs. The current research aims to address these issues. We studied stress relaxation behavior of metallic glasses upon systematically increasing \Delta S_{mix} and on the basis of calorimetric data introduced a new entropy-based parameter \Delta_{S} , which determines, together with \Delta S_{mix} , their relaxation ability. We found that the depth of stress relaxation at given normalized temperature systematically decreases with \Delta S_{mix} but increases with \Delta_{S} . Possible reasons for this behavior are discussed. 2 Experimental Table 1: Parameters of MGs under investigation: mixing entropy \Delta S_{mix}/R , excess entropy \Delta S_{scl} , excess entropy \Delta S_{T_{g}} and entropy rise in the SCL range \Delta_{S}=(\Delta S_{scl}-\Delta S_{Tg})/R . N Glass composition \Delta S_{mix}/R \Delta S_{scl} \Delta S_{T_{g}} \Delta_{S} at. \% [\frac{J}{K\times mol}] [\frac{J}{K\times mol}] 1 Cu_{50}Zr_{45}Al_{5} 0.86 5.6 4.7 0.11 2 Zr{}_{46}Cu_{36.8}Ag_{9.2}Al_{8} 1.15 7.0 5.7 0.16 3 Pd_{43.2}Cu_{28}Ni_{8.8}P_{20} 1.25 6.3 4.5 0.22 4 Zr_{35}Hf_{13}Al_{11}Ag_{8}Ni_{8}Cu_{25} 1.63 3.5 2.9 0.072 5 Zr_{40}Hf_{10}Ti_{4}Y_{1}Al_{10}Cu_{25}Ni_{7}Co_{2}Fe_{1} 1.66 3.4 2.9 0.060 6 Zr_{16.67}Hf_{16.67}Al_{16.67}Co_{16.67}Ni_{16.67}Cu_{16.67} 1.79 4.8 4.7 0.012 Six metallic glasses (MGs), Cu 50 Zr 45 Al 5 , Zr 46 Cu 36.8 Ag 9.2 Al 8 , Pd 43.2 Cu 28 Ni 8.8 P 20 , Zr 35 Hf 13 Al 11 Ag 8 Ni 8 Cu 25 , Zr 40 Hf 10 Ti 4 Y 1 Al 10 Cu 25 Ni 7 Co 2 Fe 1 and Zr 16.67 Hf 16.67 Al 16.67 Co 16.67 Ni 16.67 Cu 16.67 (at.%) listed in Table 1 were chosen for the investigation. The first three MGs constitute conventional glass compositions with the mixing entropy \Delta S_{mix}/R increasing from 0.86 to 1.25 while three latter MGs are high-entropy with 1.63\leq\Delta S_{mix}/R\leq 1.79 . It is to be noted that this composition range covers almost complete \Delta S_{mix}/R -range available experimentally. All MGs were produced by single-roller spinning as 25–35 \mu m ribbons and X-ray checked to be fully amorphous. Differential scanning calorimetry (DSC) was performed using a Hitachi DSC 7020 in flowing N_{2} (99.999 \% pure) atmosphere. The instrument was calibrated using the melting points and enthalpies of 99.99 \% pure In, Sn, Pb and Al. Every glass composition was tested as follows: i ) an initial sample was heated with empty reference DSC cell up to the temperature of the complete crystallization T_{cr} and cooled down to room temperature; this sample was next moved into the reference cell; ii ) a new initial sample of nearly the same mass (50-70 mg) was tested up to T_{cr} . This procedure allowed calculating the differential heat flow \Delta W=W_{gl}-W_{cr} , where W_{gl} and W_{cr} are the heat flows coming from glass and maternal (counterpart) crystal, respectively. Then, one can calculate the excess entropy of glass using the relationship suggested recently [ 13 , 14 ] , \Delta S(T)=\frac{1}{\dot{T}}\int_{T}^{T_{cr}}\frac{\Delta W(T)}{T}dT, (1) where \dot{T} is heating rate. It is to be mentioned that if temperature T\rightarrow T_{cr} then \Delta S\rightarrow 0 and, therefore, \Delta S thus determined constitutes the excess entropy of glass with respect to the counterpart crystal. In this work, we chose stress relaxation as a method to test the relaxation ability of MGs characterized by different mixing entropy. The stress relaxation method is often used in experimental studies, but it is only done under isothermal conditions and in the tensile mode. For non-isothermal experiments (i.e. at a constant heating rate) in the tensile mode, this method is practically unsuitable because of thermal expansion of the testing machine, which corrupts measurement results making them completely unreliable. However, if measurements are taken in the torsional mode, thermal expansion has no effect on the stress relaxation data. In this case, it is possible to measure the relaxation kinetics in the whole temperature range, starting from room temperature up to T_{cr} or even higher temperatures. However, this experimental technique is rather complicated and we know just a few examples of non-isothermal measurements of torsional stress relaxation [ 15 ,