Carbon fiber damage evolution under flame attack and the role of impurities

Pablo Chávez-Gómez, Tanja Pelzmann, Darren R. Hall, Cornelia Chilian, Louis Laberge Lebel, Étienne Robert · 2025

Read Carbon fiber damage evolution under flame attack and the role of impurities by Pablo Chávez-Gómez, Tanja Pelzmann, Darren R. Hall, Cornelia Chilian, Louis Laberge Lebel, Étienne Robert (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2505-01408.txt.

Introduction

Pablo Chavez-Gomez, Tanja Pelzmann, and colleagues watch carbon fibers burn in a 2025 materials study. Carbon fiber composites are light and strong, but their fibers oxidize heavily in a fire, a real concern for aircraft accidents. Fibers made from the same precursor differ in microstructure, and impurities may steer how damage spreads.

A fixed-point technique inserts individual fibers into a premixed flame for timed exposures. Electron microscopy and X-ray spectroscopy then map the damage and chemistry fiber by fiber. Following single fibers over time separates the roles of structure and contamination in fire resistance.

Catalog record

CREATORPablo Chávez-Gómez, Tanja Pelzmann, Darren R. Hall, Cornelia Chilian, Louis Laberge Lebel, Étienne Robert
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE53 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2505-01408

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Carbon fiber damage evolution under flame attack and the role of impurities Pablo Chávez-Gómez, Tanja Pelzmann, Darren R. Hall, Cornelia Chilian, Louis Laberge Lebel, Étienne Robert Abstract \Acp CF are prone to extensive oxidation under fire attack, for instance, in an aircraft fire scenario. This work addresses the damage mechanisms observed on PAN ( PAN )-based CF with different microstructure exposed to open flames. A fixed-point technique was developed to follow up individual CF by means of time-controlled insertion into premixed methane/air flames, followed by SEM ( SEM ) and EDS ( EDS ) analyses. Besides diameter reduction, three localized damage mechanisms were discerned in presence of impurities, which were quantified by NAA ( NAA ). Severe pitting was ascribed to catalytic oxidation mainly caused by alkali and alkaline earth metals. After an initial period where catalytic reactions between impurities and the carbon surface dominate, the flame stoichiometry governed the CF gasification process, with lean flames being much more aggressive than rich ones. A second mechanism, channelling, was caused by mobile metallic impurities. Some impurities showed an opposite effect, lowering reactivity and thus preventing further catalysis. Amorphous damage with a skin-peeling effect is believed to be the result of localized impurities at high concentrations and microstructural variations. Hindrance or synergistic effects between impurities are discussed. Finally, apparent axial pit growth rates were determined and compared with other carbonaceous materials, revealing a strong influence of impurities and the flame reactive atmosphere on CF oxidation. Keywords— carbon fiber, flame attack, impurities, pitting, damage evolution, catalytic oxidation AFM atomic force microscopy ASA active surface area CASA contact active surface area CF carbon fiber CI confidence interval CFRP carbon fiber reinforced polymer CMC ceramic matrix composite CNT carbon nanotube DSC differential scanning calorimetry EDS energy-dispersive X-ray spectroscopy E_{a} activation energy ESEM environmental scanning electron microscopy ETEM environmental transmission electron microscopy FAA Federal Aviation Administration FFB flat flame burner HOPG highly oriented pyrolytic graphite HT-SEM high temperature environmental scanning electron microscopy HTT heat treatment temperature HUR heat-up rate ISO International Organization for Standardization NAA neutron activation analysis PAN polyacrylonitrile PMC polymer matrix composite \dot{Q} heat flux SEM scanning electron microscopy STM scanning tunneling microscopy STEM scanning transmission electron microscopy TEM transmission electron microscopy SLOWPOKE-2 Safe LOW-POwer Kritical Experiment SS stainless steel STA simultaneous thermal analyses T temperature T_{Ta} Tammann temperature T_{m} melting point T_{max} temperature corresponding to the maximum oxidation rate TEM transmission electron microscopy TGA thermogravimetric analysis TPS thermal protection systems TTF time-to-failure fnum@section1 Introduction In-flight or post-crash aircraft fires pose a threat to passenger safety, either from a smoke and toxicity standpoint, or repercussions on the vehicle structural integrity [ 1 ] . This translates into challenging design constraints for modern aircraft, since they extensively rely on inherently-flammable CFRP ( CFRP ) composites [ 2 ] . The intricate thermal, physical and chemical processes involved in CFRP combustion [ 3 , 4 ] make the fate of CF exposed to fire difficult to predict. Moreover, desirable outcomes are sometimes conflicting. On one hand, full gasification might be sought [ 5 , 6 ] to avoid the release of CF fragments from burning composites, resulting in health and electrical hazards [ 7 , 8 , 9 ] . On the other hand, oxidative resistance is required to prevent burn-through if the component is structural or serves as a firewall [ 1 ] . However, the conditions under which this resistance is assessed varies, with samples typically exposed to the atmospheres created by non-premixed or partially premixed turbulent flames. \Acp CF readily gasify at high temperatures when exposed to reactive or oxidizing environments. Like any other carbonaceous material [ 10 ] , the fiber reactivity is mainly driven by its ASA ( ASA ) [ 11 , 12 ] , which is defined by structural order and available functional groups [ 13 ] . CF oxidation takes place through preferential etching starting at defects (e.g. vacancies, Stone-Wales type, interstitials, adatoms [ 14 ] ) and crystal edges (armchair & zig-zag) [ 15 , 12 , 16 , 17 , 18 ] . Such features mainly arise during the fiber manufacturing process [ 19 , 20 ] . The heterogeneous CF microstructure involving turbostratic and amorphous regions [ 21 , 22 , 23 , 24 , 19 ] results in intricate oxidation processes [ 25 ] . Moreover, fibers from the same precursor, e.g. PAN , have different structures depending on the HTT ( HTT ). High strength/low modulus CF show a core-sheath structure with small crystallites in the skin zone and regions of amorphous carbon in the core [ 23 ] , while high modulus CF have a less disordered structure [ 24 ] as aresult of higher HTT . Fiber gasification is influenced by several factors, namely the composition of the atmosphere, temperature and pressure [ 11 , 26 , 27 , 28 , 13 , 29 ] . For instance, with molecular oxygen ( \text{O}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} ), oxidation takes place by \text{O}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} chemisorption and subsequent carbon monoxide and dioxide ( CO / \text{CO}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} ) desorption. Other mechanisms can come into play in the absence of \text{O}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} , such as the Boudouard reaction in the presence of \text{CO}{\vphantom{\text{X}}}_{\smash[t]{\text{2}}} [ 10 ] . These mechanisms enlarge pores, create more active sites and new defects thus increasing the ASA , enhancing the oxidation process and degrading the CF mechanical properties [ 30 , 31 , 32 , 33 , 34 ] , with analogous processes observed with other carbonaceous materials [ 35 ] . These phenomena can be accelerated by the presence of impurities in the carbon structure, which act locally or with a certain mobility [ 36 , 37 , 38 , 39 ] . As with other carbonaceous materials, alkali and alkaline earth metals, along with their carbonate and acetate compounds, are known to catalyze the CF oxidation process [ 40 , 41 , 6 , 5 , 42 , 43 , 11 ] . Other elements can mitigate catalytic effects, for instance boron doping results in active site blockage and crystallite size increase [ 44 , 45 ] , while some halogens, sulphur ( S ) and phosphorus ( P ) can poison impurities with catalytic effects [ 46 , 47 ] . CF gasification invariably leads to diameter reduction [ 48 , 31 ] and internal porosity may develop in a process analogous to carbon activation, i.e., controlled pore and ASA enlargement [ 49 , 50 ] . However, locally accelerated oxidation may take place in the presence of impurities and large structural defects. This process, known as pitting, has been reported on CF under liquid or gaseous oxidative conditions, such as electrolyte [ 51 ] and acid treatments [ 52 , 53 ] , TGA ( TGA ) [ 11 , 54 , 55 , 26 , 56 , 32 ] , plasma etching [ 22 , 52 ] , as well as using tube furnaces [ 57 , 32 ] , flow tube reactors [ 58 , 59 ] , air-filled ovens [ 30 , 11 ] , environmental electron microscopes [ 60 ] and other heated processing systems [ 33 ] . Under open flame attack, exacerbated pitting was observed

Read the complete text