Magneto-Optical Analysis of Magnetic Anisotropy in Ultrathin Tm 3 Fe 5 O 12 /Pt Bilayers

T. Nathan Nunley, Daniel Russell, Liang-Juan Chang, David Lujan, Jeongheon Choe, Side Guo, Shang-Fan Lee, Fengyuan Yang, Xiaoqin Li · 2025

Read Magneto-Optical Analysis of Magnetic Anisotropy in Ultrathin Tm 3 Fe 5 O 12 /Pt Bilayers by T. Nathan Nunley, Daniel Russell, Liang-Juan Chang, David Lujan, Jeongheon Choe, Side Guo, Shang-Fan Lee, Fengyuan Yang, Xiaoqin Li (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2504-17071.txt.

Introduction

Nunley and co-authors probe ultra-thin magnetic films in a 2025 paper, using light to read which way the magnetism points. The films pair a garnet layer just a few atoms thick with a platinum cap. Such pairs are prized for devices that steer spin with electric signals.

A sharp light method let the team compare loops under fields pointing out of and along the film. The favored direction shifted as the garnet thinned by less than one tiny unit, they found. The platinum cap more than doubled the key field that sets that direction. That means the join between the layers rules the film at this scale. Builders of spin devices must count that join as a main design part, not a side note.

Catalog record

CREATORT. Nathan Nunley, Daniel Russell, Liang-Juan Chang, David Lujan, Jeongheon Choe, Side Guo, Shang-Fan Lee, Fengyuan Yang, Xiaoqin Li
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE28 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2504-17071

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Magneto-Optical Analysis of Magnetic Anisotropy in Ultrathin Tm 3 Fe 5 O 12 /Pt Bilayers T. Nathan Nunley, Daniel Russell, Liang-Juan Chang, David Lujan, Jeongheon Choe, Side Guo, Shang-Fan Lee, Fengyuan Yang, Xiaoqin Li Abstract Magnetic bilayers consisting of an epitaxially grown ferrimagnetic insulator and a heavy metal layer are attractive for spintronic application because of the opportunity for electric control and read-out of spin textures via spin orbit torque. Here, we investigate ultrathin thulium iron garnet (TmIG)/Pt bilayers when the TmIG layer thickness is 3 nm and below using a sensitive Sagnac magneto-optical Kerr effect technique. We compare the hysteresis loops from out-of-plane and in-plane applied magnetic fields. The preferred magnetization orientation evolves with the TmIG thickness and the presence of the Pt overlayer. We quantify the evolution of the magnetic anisotropy in these ultrathin films and find a significant change even when the TmIG thickness is varied by less than 1 nm. In these ultrathin films, the presence of a Pt overlayer changes the effective anisotropy field by more than a factor of 2, suggesting that the interfacial anisotropy at the Pt/TmIG interface plays a critical role in this regime. Preprint: AIP/123-QED I Introduction Many ferrimagnetic insulators exhibit Curie temperatures significantly above room temperature. In their multilayer form, these materials provide promising platforms for both fundamental studies of magnetism [ 1 , 2 , 3 , 4 , 5 , 6 , 7 , 8 , 9 , 10 ] and future spintronic applications [ 11 , 12 , 13 , 14 , 15 , 16 , 17 ] . For example, skyrmions are more readily stabilized in two-dimensional system than the 3D skyrmion crystal phase [ 18 ] . Epitaxially grown magnetic garnet thin films, e.g. TmIG (Tm 3 Fe 5 O 12 ) are particularly interesting as they may host nanoscale skyrmions stable at room temperature [ 19 , 20 , 21 , 22 ] . These films exhibit low damping, high crystalline quality with low pinning density [ 23 , 10 , 6 , 24 ] , tunable interfacial Dzyaloshinskii-Moriya interaction (DMI) [ 25 , 10 , 21 ] , and strain-tunable anisotropy [ 20 , 26 , 27 , 19 , 28 , 29 , 30 ] . Many of these features are highly desirable for the formation and current-driven motion of chiral domain walls [ 8 , 9 , 10 ] and skyrmions. Figure 1: Sample quality and illustrations of experimental apparatus and sample structure. (a) is XRD of an epitaxially grown 5 nm TmIG film grown by the same method indicating the high crystalline quality of the TmIG film. (b) Rendering of the Pt/TmIG films geometry. (c) is the SaMOKE apparatus. The SLD is the superluminescent diode, Pol is the polarizer, \lambda/2 is the \lambda/2 -waveplate, EOM is the electro-optic modulator, and \lambda/4 is the \lambda/4 -waveplate. The lock-in measures the first and second harmonic of the reference frequency that is sent to the EOM. (d) and (e) Show the sample with the probe beam and electromagnet poles. The directional axes in (d) show the OP, IP ∥ , and Transverse (IP ⟂ ) directions with respect to the sample surface. The IP ⟂ direction is perpendicular to the TmIG to Pt/TmIG transition. (d) shows the magnet and sample configuration for OP field, (e) for IP. Multiple parameters are important for generating robust skyrmions including saturation magnetization, exchange constant, DMI, and anisotropy. These parameters control the skyrmion type, size, and stability. The saturation magnetization and exchange constants are difficult to engineer because these properties are largely intrinsic. We note that some thickness dependence has been found, especially at the ultrathin limit [ 19 , 20 ] . However, for ferrimagnetic films such as TmIG, anisotropy and DMI are highly tunable [ 31 , 32 , 33 , 9 , 25 , 34 , 35 , 21 , 36 , 37 , 34 , 38 ] . A commonly used strategy is to choose different heavy metal layers. There have been extensive studies on engineering magnetic anisotropy of TmIG thin films through substrate-induced epitaxial strain [ 31 , 32 , 33 , 27 ] , which leads to perpendicular magnetic anisotropy (PMA), However, debates continue about the role of a heavy metal overlayer and whether the interfacial DMI originate from the epitaxial interface or the insulator/metal interface [ 25 , 37 , 26 , 39 ] . The latter produces the spin Hall-topological Hall resistivity when topological spin textures in the bilayer form. Previously, the dependence of interfacial anisotropy at the insulator/metal interface on the crystal orientation has been investigated when the TmIG and YIG films are 5 nm thick [ 27 ] . Below this thickness, traditional techniques, such as vibrating sample magnetometry or superconducting quantum interference device magnetometry, do not offer sufficient sensitivity, partly because the very strong paramagnetic background from garnet substrates containing rare earth elements. Studying films less than 3 nm thick, the ultrathin limit, is critical for understanding topological magnetic phases near room temperature [ 20 , 22 ] . Here, we investigate how magnetic anisotropy in epitaxial TmIG bare films and Pt/TmIG bilayers evolves as a function of the film thickness in the ultrathin film limit. We apply a highly sensitive magneto-optical Kerr effect (MOKE) technique to measure the hysteresis loops of TmIG films 2.3 to 3 nm thick. We compare the measurements when an out-of-plane (OP) vs. in-plane (IP) magnetic field is scanned. By extracting and comparing the saturation fields in these two geometries, we quantify the effective anisotropy field. In this ultrathin film limit, the interfacial anisotropy energy density becomes large compared to the volumetric anisotropy terms. We confirm that the Pt/TmIG interface produces a compass anisotropy that dominates the magnetic anisotropy when the TmIG film thickness is varied by less than 1 nm. Our study provides previously inaccessible insight into anisotropy engineering in these ultrathin ferrimagnetic insulating films and bilayers. II Methods Epitaxial-Pt/TmIG bilayers were deposited by off-axis sputtering on Gd 2.6 Ca 0.4 Ga 4.1 Mg 0.25 Zr 0.65 O 12 (sGGG) (111) substrates from MTI Corporation. The different TmIG and sGGG lattice constants, 12.324 [ 30 , 20 ] and 12.480 Å, respectively, result in a tensile strain which produces perpendicular magnetic anisotropy [ 31 , 32 ] . An x-ray diffraction (XRD) scan of a representative 5 nm TmIG film grown on sGGG is shown in Fig. 1 a with broad Laue oscillations around the TmIG(444) peak, demonstrating the high quality of the epitaxial film. It has been shown previously by some of us that this growth method produces high quality, single crystal films [ 20 , 21 , 37 , 27 ] without a magnetic dead layer at the TmIG/sGGG interface [ 27 ] . In order to explore the anisotropy transition, we prepared TmIG films of three different thicknesses, 3.0, 2.7, and 2.3 nm. After the TmIG growth, 2 nm Pt was deposited on each sample at room temperature. The TmIG films were partially blocked during the Pt deposition, leading to Pt coverage on only part of the sample surface. This method allows us to isolate the effect the Pt layer has on each TmIG film while keeping constant

Read the complete text