Structural and Electrical Transport Properties of NASICON type Na 3 Zr 2-x Ti x Si 2 PO 12 ( x = x= 0.1–0.4) Solid Electrolyte Materials

Ramcharan Meena, Rajendra S. Dhaka · 2025

Read Structural and Electrical Transport Properties of NASICON type Na 3 Zr 2-x Ti x Si 2 PO 12 ( x = x= 0.1–0.4) Solid Electrolyte Materials by Ramcharan Meena, Rajendra S. Dhaka (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2504-05858.txt.

Introduction

Ramcharan Meena and Rajendra Dhaka study a ceramic that can carry sodium ions, a trait wanted for solid-state batteries. Their 2025 paper varies the recipe by swapping some zirconium for titanium, in four small steps. The base is a NASICON-type material, a known family of fast ion movers.

X-ray fits show all four mixes share the same slanted crystal form. Heat-driven conduction follows the classic rising curve, and the energy needed to start it grows as the swap shrinks the cell. Charge storage gauges over heat and frequency show two relaxation paths with unlike start energies. Both the storage fits and the impedance fits point to a spread-out, non-ideal relaxation, with grain and grain-edge parts.

Catalog record

CREATORRamcharan Meena, Rajendra S. Dhaka
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE49 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2504-05858

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Structural and Electrical Transport Properties of NASICON type Na 3 Zr 2-x Ti x Si 2 PO 12 ( x = x= 0.1–0.4) Solid Electrolyte Materials Ramcharan Meena, Rajendra S. Dhaka Abstract We report the structural, resistivity, impedance, and dielectric studies of isovalent substituted Na 3 Zr 2-x Ti x Si 2 PO 12 ( x = x= 0.1–0.4) NASICON type solid electrolyte materials. The Rietveld refinement of XRD patterns shows the monoclinic phase with space group of C 2/c for all the samples. The resistivity analysis shows the Arrhenius-type thermal conduction with an increase in activation energy with doping is explained based on decreased unit cell volume. We use Maxwell-Wagner-Sillars (MWS) relaxation and space charge or interfacial polarization models to explain the frequency and temperature-dependent variations of electric permittivity. The double relaxation peaks in the dielectric loss data show the two types of relaxation mechanisms of different activation energy. The real ( ϵ ′ \epsilon^{{}^{\prime}} ) and imaginary ( ϵ ′′ \epsilon^{{}^{\prime\prime}} ) parts of permittivity are fitted using the modified Cole-Cole equation, including the conductivity term, which show the non-Debye type relaxation over the measured frequency and temperature range. The impedance analysis shows the contributions from grain and grain boundary relaxation. The fitting performed using the impedance and constant-phase element (CPE) confirm the non-Debye type relaxation. Moreover, the electric modulus analysis confirms the ionic nature having thermally activated relaxation and the modulus scaling analysis shows a similar type of relaxation in the measured temperature range. The modified power law is used to understand the frequency dependence of a.c. conductivity data. The temperature dependence of exponent ( s s ) in modified power law suggests the change in the conduction mechanism from near small polaron tunneling (NSPT) to correlated barrier hopping (CBH) above room temperature. The larger values of ϵ \epsilon r indicate these materials as a potential candidate for charge-storage devices. I Introduction In recent years, sodium (Na) based energy storage devices have attracted great attention due to the low cost as compared to Li-based devices for all solid-state batteries [ 1 , 2 ] . Among a wide available range, NASICON materials called as Sodium ( Na ) S uper I onic CON ductor are mostly used as solid electrolyte as well as cathode [ 3 , 4 ] due to their larger ionic conductivity 10 -4 S/cm at room temperature and 10 -1 S/cm at 300 ∘ C [ 5 ] as well as structural stability [ 6 ] . However, the ionic conductivity of these solid electrolytes is still two orders less than the liquid electrolytes, which challenge their commercial usage [ 7 , 8 ] . On the other hand, the liquid-based electrolytes have various disadvantages, such as flammability, leakage, and metallic reduction limits the liquid-based electrolytes for large-area applications. Interestingly, the solid electrolytes have various advantages like high chemical, mechanical, structural, and thermal stability, wide compatibility with materials, large ionic conductivity and high stability in air, making the NASICON-based materials a better choice to use as electrolytes in all solid-state batteries. These materials are also used for various other applications such as solid oxide fuel cells, gas sensors, ion-selective electrodes, supercapacitors, and microwave absorptions, where lower density of NASICON makes them a suitable choice for low-weight devices [ 9 , 10 ] . In this line, the NASICON having the chemical composition of Na 1+x Zr 2 Si x P 3-x O 12 , (0 \leq x \leq 3) was first characterized by Hong and Goodenough in 1976 [ 11 , 12 ] . The original NASICON composition is derived from the NaZr 2 P 3 O 12 by partially replacing P by Si and compensating the resulting charge difference by adding extra Na inside the matrix. During this process, the lattice parameters along the c- axis increase with Si amount for maximum at x= 2 and decrease thereafter. Interestingly, the Na 1+x Zr 2 Si x P 3-x O 12 , (0 \leq x \leq 3) stabilizes in rhombohedral phase (space group R \bar{3} C) except 1.8 \leq x \leq 2.2 range which stabilizes in the monoclinic phase (space group C 2/c) [ 12 , 13 , 11 ] . These NASICON structures (monoclinic and rhombohedral) have skeleton-type arrangement containing two ZrO 6 octahedra separated by three Si/PO 4 tetrahedra having two different sites available for hopping named as (Na 1 and Na 2 ). The Na 1 is located between two octahedral sites along the c- axis in six-fold coordination with corner-sharing oxygen ions. The Na 2 is located between two Na 1 sites along the a- axis in eight-fold coordination with O-ions containing four Na sites per unit cell. Here, the rhombohedral phase contains one Na 1 and three Na 2 sites having only conduction path (Na 1 -Na 2 -Na 1 ). However, the monoclinic phase has one Na 1 , one Na 2 and two Na 3 sites as in monoclinic phase Na 2 site further splits into Na 2 and Na 3 , which gives the additional conduction path (Na 1 -Na 2 -Na 1 and Na 1 -Na 3 -Na 1 ). Out of these total available sites, 2/3 are filled and 1/3 are available for conduction through the hopping of Na ions between the sites [ 14 , 15 ] . The Na ions migrate through an oxygen triangle (made from Na and O ions of two polyhedrons) called as bottleneck. The conductivity depends on the number of ions available for conduction and the bottleneck area. Here, the highest conductivity at room temperature is found for the Na 3 Zr 2 Si 2 PO 12 ( x= 2) sample which correlate with its larger c- axis value [ 9 , 14 , 15 ] . Notably, the monoclinic phase transforms to the rhombohedral phase at around 160 ∘ C has been confirmed using in-situ x-ray diffraction (XRD) and differential scanning calorimetry measurements (DSC) [ 15 , 16 ] . In this case, only Na ion ordering changes during the phase transition where one Na 2 and two Na 3 sites of the monoclinic phase merge into three Na 2 sites of the rhombohedral phase [ 15 ] . The analysis shows that the transformation from monoclinic to rhombohedral phase is due to the shear deformation of the unit cell [ 15 , 16 ] . Furthermore, the conductivity of NASICON based solid electrolyte materials can be tuned by changing the synthesis method, amount of initial precursors, sintering temperature, doping, valance state of dopant, Si to P ratio and the radius of dopant ions [ 19 , 20 , 21 , 18 , 17 , 22 , 23 , 24 ] . It is concluded from previous studies that lower sintering temperatures during sample preparation and a larger density of prepared NASICON samples are preferred for various applications like solid electrolyte. The doping of divalent or trivalent atoms at the Zr site will change the number of free charge carriers per unit cell. The dopant’s ionic radius (if larger than Zr ion) increases the bottleneck area, which decreases the activation energy resulting an overall increase in Na conduction. There are very few dielectric studies on doped

Read the complete text