Decoupled anisotropic Charge-Phonon Transport Enables Exceptional n-Type Thermoelectric Performance in CuBiSCl 2

Yu Wu, Ying Chen, Shuming Zeng, Liujiang Zhou, Chenhan Liu · 2025

Read Decoupled anisotropic Charge-Phonon Transport Enables Exceptional n-Type Thermoelectric Performance in CuBiSCl 2 by Yu Wu, Ying Chen, Shuming Zeng, Liujiang Zhou, Chenhan Liu (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2504-01319.txt.

Introduction

Yu Wu and co-authors compute heat and charge flow in a 2025 materials paper. A good thermoelectric material must let charge run freely while blocking heat, a pairing that rarely occurs. First principle calculations on a copper bismuth compound show both traits meeting along one crystal direction.

Charge moves fast along that axis through spread out electron states in the ribbons of the structure. Heat, meanwhile, stays very low because copper atoms shake in soft modes that scatter heat carrying waves. Both wins trace to the layered bond pattern of the crystal. The result points to a design rule for power from waste heat.

Catalog record

CREATORYu Wu, Ying Chen, Shuming Zeng, Liujiang Zhou, Chenhan Liu
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE24 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2504-01319

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Decoupled anisotropic Charge-Phonon Transport Enables Exceptional n-Type Thermoelectric Performance in CuBiSCl 2 Yu Wu, Ying Chen, Shuming Zeng, Liujiang Zhou, Chenhan Liu Abstract First-principles calculations demonstrate an exceptional decoupling of charge and thermal transport along the a -axis in CuBiSCl 2 . The material achieves superior electron mobility (138 cm 2 /V ⋅ \cdot s at 300 K) through delocalized Bi-6 p /S-3 p networks while maintaining ultralow lattice thermal conductivity (0.40 W/mK at 300 K) via Cu-dominated anharmonic phonon scattering - both optimized along the same crystallographic direction. This simultaneous optimization originates from the anisotropic bonding hierarchy where [BiSCl 2 ] n ribbons enable efficient charge transport along a -axis, while the soft vibrational modes associated with Cu atoms strongly scatter heat-carrying phonons. The resulting high power factor (1.71 mW/mK 2 at 700 K) and peak ZT of 1.57 establish CuBiSCl 2 as a model system that realizes the long-sought "phonon glass-electron crystal" paradigm through crystallographically engineered transport channels. † † email: [email protected] † † affiliation: Micro- and Nano-scale Thermal Measurement and Thermal Management Laboratory, School of Energy and Mechanical Engineering, Nanjing Normal University, Jiangsu, Nanjing 210023, China † † affiliation: Eastern Institute of Technology, Zhejiang, Ningbo 315200, China † † affiliation: College of Physics Science and Technology, Yangzhou University, Jiangsu 225009, China † † affiliation: School of Physics and State Key Laboratory of Electronic Thin Films and Integrated Devices, University of Electronic Science and Technology, Sichuan, Chengdu 610054, China † † email: [email protected] † † affiliation: Micro- and Nano-scale Thermal Measurement and Thermal Management Laboratory, School of Energy and Mechanical Engineering, Nanjing Normal University, Jiangsu, Nanjing 210023, China Introduction Thermoelectric materials enable direct energy conversion between heat and electricity through the Seebeck and Peltier effects, offering promising solutions for waste heat recovery and solid-state refrigeration Biswas et al. 2012 ; Tan et al. 2016 ; Zhao et al. 2014 ; Wu et al. 2024 . The conversion efficiency is governed by the dimensionless figure of merit ZT=S^{2}\sigma T/\kappa_{\text{tot}} , where S , \sigma , T , and \kappa_{\text{tot}} represent the Seebeck coefficient, electrical conductivity, absolute temperature, and total thermal conductivity (electronic \kappa_{e} + lattice \kappa_{L} ), respectively. Optimizing ZT requires simultaneously enhancing the power factor ( PF=S^{2}\sigma ) while minimizing \kappa_{\text{tot}} , which presents a fundamental challenge due to the strong coupling between these parameters Biswas et al. 2012 ; Snyder and Toberer 2008 ; Pei et al. 2011 . This challenge has motivated the development of materials exhibiting the “phonon glass-electron crystal” (PGEC) behavior Beekman et al. 2015 , where glass-like thermal transport coexists with crystal-like electronic properties. Recent advances have demonstrated that anisotropic crystals can achieve this PGEC behavior directionally, with specific crystallographic axes showing simultaneous phonon localization and efficient charge transport Zhan et al. 2024 ; Zhan et al. 2022 ; Su et al. 2022 ; Wang et al. 2023 . The fundamental origin of anisotropic transport decoupling lies in the distinct crystallographic dependence of electronic and vibrational properties. In PbSnS 2 , the out-of-plane transport superiority originates from: (1) interlayer Sn-5 s /S-3 p orbital hybridization enabling high electron mobility ( \mu\approx 60 cm 2 /V \cdot s) along the c-axis, and (2) twisted NaCl-type structure with strong anharmonicity suppressing \kappa_{L} (<0.5 W/m \cdot K) in the same direction Zhan et al. 2024 . Parallel mechanisms are observed in n-type SnSe Su et al. 2022 , where (1) strain-induced bond angle reduction enhances out-of-plane charge transport through improved orbital overlap, while (2) the inherent van der Waals gaps between layers establish two-dimensional phonon confinement perpendicular to the conduction pathway. These systems exemplify how directional selectivity can be engineered through either covalent interlayer coupling (PbSnS 2 ) or controlled structural distortion (SnSe), while both approaches utilize anisotropic lattice dynamics to break the traditional transport coupling. Mixed-anion chalcogenides have recently emerged as promising thermoelectric materials due to their intrinsically low thermal conductivity and tunable electronic properties Zhao et al. 2010 ; Li et al. 2015 ; Luu and Vaqueiro 2016 . The coexistence of stereochemically active lone pairs (Bi 3+ 6 s 2 ) and mixed anion coordination (S 2- /Cl - ) in compounds like CuBiSCl 2 creates a unique bonding hierarchy that strongly suppresses phonon propagation, with reported \kappa_{L} values below 1 W/m \cdot K at room temperature Shen et al. 2024 . However, the fundamental relationship between anisotropic structural motifs and direction-dependent charge transport remains underexplored, particularly regarding how specific crystallographic axes can simultaneously optimize electronic mobility and phonon localization. Moreover, the potential role of four-phonon scattering in such anisotropic systems has not been quantitatively assessed, despite its recognized importance in materials with ultralow thermal conductivity Wu et al. 2024 ; Yuan et al. 2024 . In this work, we employ first-principles calculations to systematically investigate the anisotropic thermoelectric properties of CuBiSCl 2 . Our analysis reveals that the material achieves exceptional a -axis performance through: (1) high electron mobility (138 cm 2 /V \cdot s) enabled by delocalized Bi-6 p /S-3 p orbitals at the conduction band minimum, and (2) suppressed lattice thermal conductivity ( \kappa_{L} = 0.40 W/m \cdot K at 300 K) resulting from Cu-dominated anharmonic vibrations and four-phonon scattering. The combination of these effects yields a peak ZT of 1.57 along the a -axis at 700 K, establishing CuBiSCl 2 as a promising anisotropic thermoelectric material. Our findings provide fundamental insights into how directional bonding hierarchies can be engineered to achieve decoupled charge-phonon transport in mixed-anion compounds. Results and Discussion The crystal structure of CuBiSCl 2 (space group Cmcm ) exhibits pronounced anisotropic bonding through two distinct coordination geometries (Fig. 1 ). Copper ions occupy distorted CuS 2 Cl 4 octahedra, where the axial Cu–S bonds (2.25 Å) are significantly shorter than the equatorial Cu–Cl distances (2.75 Å), resulting in a quasi-linear S–Cu–S coordination. This creates a striking contrast between the strong covalent Cu–S interactions (second-order interatomic force constants, IFC = 3.00 eV/Å 2 ) and weak ionic Cu–Cl contacts (IFC = 0.26 eV/Å 2 ). Bismuth ions reside in asymmetric BiS 2 Cl 6 polyhedra, displaying three distinct bonding regimes: two short Bi–S bonds (2.70 Å), two intermediate Bi–Cl bonds (2.75 Å), and four elongated Bi \cdots Cl interactions (3.12 Å). The connectivity of these polyhedral units reveals a dimensional hierarchy in bonding strength. Corner-sharing CuS 2 Cl 4 octahedra form [Cu 2 S 2 ] n chains along the c -axis, while edge-sharing BiS 2 Cl 6 units create [BiSCl 2 ] n ribbons along the a -axis. These strongly bonded frameworks are interconnected along the b -axis through weak Cl-mediated linkages (Cu–Cl = 2.75 Å, Bi \cdots Cl = 3.12 Å), resulting in a “stiff chain/soft interchain” architecture. This anisotropic bonding configuration, featuring rigid covalent frameworks separated by weakly bonded chlorine layers, establishes a structural motif that profoundly influences the material’s thermal transport characteristics. The directional mechanical response was characterized through harmonic analysis of strain-energy relationships (Fig. 1 (c)). Quadratic fitting of the normalized energy variation ( \Delta E/E_{0} ) versus strain ( \varepsilon ) yields dimensionless coefficients \alpha_{a} = 1.2 \times 10^{-4} (along a ), \alpha_{b} = 8.2 \times 10^{-5} (along b ) and \alpha_{c} = 3.0 \times 10^{-4} (along c ), revealing a clear

Read the complete text