Extremely high excitonic g g -factors in 2D crystals by alloy-induced admixing of band states

Katarzyna Olkowska-Pucko, Tomasz Woźniak, Elena Blundo, Natalia Zawadzka, Łucja Kipczak, Paulo E. Faria Junior, Jan Szpakowski, Grzegorz Krasucki, Salvatore Cianci, Diana Vaclavkova, Dipankar Jana, Piotr Kapuściński, Amit Pawbake, Shalini Badola, Magdalena Grzeszczyk, Daniele Cecchetti, Giorgio Pett · 2025

Read Extremely high excitonic g g -factors in 2D crystals by alloy-induced admixing of band states by Katarzyna Olkowska-Pucko, Tomasz Woźniak, Elena Blundo, Natalia Zawadzka, Łucja Kipczak, Paulo E. Faria Junior, Jan Szpakowski, Grzegorz Krasucki, Salvatore Cianci, Diana Vaclavkova, Dipankar Jana, Piotr Kapuściński, Amit Pawbake, Shalini Badola, Magdalena Grzeszczyk, Daniele Cecchetti, Giorgio Pett (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2503-23071.txt.

Introduction

Katarzyna Olkowska-Pucko and a large team of co-authors studied atom thin crystals that glow brightly, in work published in 2025. These layered crystals have rich behavior tied to spin and to valleys in their energy bands, and their response to a magnet is modest in pure form.

By mixing two metals in the crystal in varied shares, the team raised that magnetic response sharply, up to about two and a half times the usual value at one mix. Light based measures in a magnet confirmed the trend. Computer models matched the data and traced the effect to a reshaping of the energy bands by mixing. The alloys also react more to strain, a trait suited to custom light devices.

Catalog record

CREATORKatarzyna Olkowska-Pucko, Tomasz Woźniak, Elena Blundo, Natalia Zawadzka, Łucja Kipczak, Paulo E. Faria Junior, Jan Szpakowski, Grzegorz Krasucki, Salvatore Cianci, Diana Vaclavkova, Dipankar Jana, Piotr Kapuściński, Amit Pawbake, Shalini Badola, Magdalena Grzeszczyk, Daniele Cecchetti, Giorgio Pett
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE67 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2503-23071

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Extremely high excitonic g g -factors in 2D crystals by alloy-induced admixing of band states Katarzyna Olkowska-Pucko, Tomasz Woźniak, Elena Blundo, Natalia Zawadzka, Łucja Kipczak, Paulo E. Faria Junior, Jan Szpakowski, Grzegorz Krasucki, Salvatore Cianci, Diana Vaclavkova, Dipankar Jana, Piotr Kapuściński, Amit Pawbake, Shalini Badola, Magdalena Grzeszczyk, Daniele Cecchetti, Giorgio Pettinari, Igor Antoniazzi, Zdeněk Sofer, Iva Plutnarová, Kenji Watanabe, Takashi Taniguchi, Clement Faugeras, Marek Potemski, Adam Babiński, Antonio Polimeni, Maciej R. Molas Abstract Monolayers (MLs) of semiconducting transition metal dichalcogenides ( S-TMDs ) emit light very efficiently and display rich spin-valley physics, with gyromagnetic ( g g -) factors of about -4. Here, we investigate how these properties can be tailored by alloying. Magneto-optical spectroscopy is used to reveal the peculiar properties of excitonic complexes in Mo x W 1-x Se 2 MLs with different Mo and W concentrations. We show that the alloys feature extremely high g g -factors for neutral excitons, that change gradually with the composition up to reaching values of the order of -10 for x ≈ 0.2 x\approx 0.2 . First-principles calculations corroborate the experimental findings and provide evidence that alloying in S-TMDs results in a non-trivial band structure engineering, being at the origin of the high g g -factors. The theoretical framework also suggests a higher strain sensitivity of the alloys, making them promising candidates for tailor-made optoelectronic devices. Introduction— Semiconducting transition metal dichalcogenides ( S-TMDs ) monolayers (MLs), such as MoS 2 , MoSe 2 , WS 2 , WSe 2 , and MoTe 2 , exhibit several intriguing optical properties [ 1 , 2 , 3 , 4 , 5 , 6 , 7 , 8 , 9 , 10 , 11 , 12 ] . In particular, the optical response of S-TMDs is dominated by excitonic effects [ 8 , 13 , 14 , 15 , 16 ] , and, moreover, the MLs can be divided into two subgroups: bright MLs with a bright optically-active exciton ground state (MoSe 2 and MoTe 2 ), and darkish MLs whose exciton ground state is spin-forbidden and thus optically-dark (MoS 2 , WS 2 , and WSe 2 ) [ 17 , 10 , 8 , 18 , 19 , 20 , 21 , 22 , 23 , 11 , 24 , 25 , 26 , 27 , 28 , 29 ] . In S-TMD MLs, the lowest energy optically-active excitons (referred to as A excitons) have energies that span the spectral range from 1.15 eV for MoTe 2 [ 7 ] up to 2.1 eV for WS 2 [ 27 ] . Continuous energy tuning within this range can be achieved by mixing two transition metal atoms ( i.e. , Mo and W) or two chalcogen atoms ( e.g. , S and Se), which induces the creation of S-TMD alloys with adjustable stoichiometry ratio ( e.g. , Mo x W 1-x Se 2 and WS 2x Se 2-2x ) [ 30 ] . Such compositional tuning opens new possibilities for absorbing and emitting light at desired wavelengths, which is crucial for optoelectronics applications [ 31 , 32 , 33 , 34 , 35 ] . The opportunities enabled by alloying can be further exploited in fields such as valleytronics [ 36 ] , which employs local energy extrema, i.e. , the so-called valleys, to encode and process binary information, with applications for quantum computers [ 37 , 38 , 39 , 40 , 41 ] . Bright A excitons in S-TMD ML are formed by an electron-hole pair originating from the inequivalent \pm K valleys of the hexagonal Brillouin zone, and are associated selectively to \sigma^{\pm} circularly polarized light [ 42 , 8 , 43 ] . The energy degeneracy of excitons at the \pm K valleys can be lifted by applying a magnetic field perpendicular to the ML plane giving rise to the excitonic Zeeman effect described by the excitonic Landé g -factor ( g ) [ 44 , 45 ] . In an external field ( B ), the g -factor value is related to the energy splitting between excitons from the \pm K points with \sigma^{\pm} polarizations, i.e. , \Delta E(B)=E_{\sigma^{+}}(B)-E_{\sigma^{-}}(B)=g\,\mu_{B}B, ( \mu_{B} is the Bohr magneton). Theoretically, the magnetic field couples to both the spin and orbital parts of the Bloch states, and thus the excitonic g -factor reflects the energy difference between the conduction (CB) and valence (VB) bands in both the \pm K valleys [ 46 , 44 , 45 ] . For S-TMD MLs, the g -factors are approximately equal to -4 [ 19 , 13 , 47 , 44 , 48 , 23 , 21 , 25 , 49 , 50 , 27 ] for the A excitons. Moreover, while a significant variation in the ML dielectric environment affects such physical quantities as the exciton binding energies and therefore the diamagnetic shift of excitons [ 51 , 52 , 53 , 54 , 55 ] , the g -factor value stays insensitive [ 55 , 56 ] . For the WSSe ML with almost 50/50 S/Se ratio, the excitonic g -factor is close to -4 [ 57 ] , similarly to the WS 2 and WSe 2 MLs. On the other hand, investigating the g -factors of MLs of Mo-W alloys could be of particular interest, since these alloys combine bright and darkish MLs. Figure 1: (a) Low-temperature ( T =10 K) example PL spectra of MoSe 2 , WSe 2 , and Mo x W 1-x Se 2 MLs encapsulated in hBN flakes. (b) Extracted energy of neutral exciton (X) as a function of molybdenum (Mo) concentration. The dashed lines are guided to the eye. In this Letter, we investigate the magneto-optical properties of excitonic complexes in Mo x W 1-x Se 2 MLs encapsulated in hexagonal BN (hBN) with different ratios of Mo and W atoms and compare the results with those achieved for WSe 2 and MoSe 2 MLs. Using low-temperature ( T =10 K) photoluminescence (PL) experiments carried out in external out-of-plane magnetic fields up to 30 T, we extract the g -factors of the neutral (X) and charged (T) excitons. While the measured T g -factors for Mo x W 1-x Se 2 MLs vary from around -3.5 to almost -5 and are thus comparable to those of MoSe 2 and WSe 2 MLs, the g -factors for the X transitions change gradually from about -4 for MoSe 2 , to about -4.5 when the Mo concentration is \sim 85\% then -6 when the Mo concentration is \sim 70\% , to about -7 when it reaches \sim 50\% , and even up to about -10 for Mo concentrations of \sim 20\% , to then go back to -4 in WSe 2 . This striking tunability of the g -factor is verified by first principles calculations of the band structures and angular momenta of MoSe 2 and WSe 2 MLs and their alloys. The calculated values of the g -factors show a trend similar to the experimental ones and also reveal an additional increase and decrease under the application of compressive or tensile biaxial strains, respectively. Our studies indicate that the alloying of S-TMD MLs is an efficient mechanism to enhance

Read the complete text