Annealing behaviour of charge collection of neutron irradiated diodes from 8-inch p-type silicon wafers
Matteo M. Defranchis · 2025
Read Annealing behaviour of charge collection of neutron irradiated diodes from 8-inch p-type silicon wafers by Matteo M. Defranchis (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2503-01520.txt.
Introduction
A team of detector researchers tested how silicon sensors heal after radiation damage, in work published in 2025. The sensors are being built for a new calorimeter in the CMS detector at the Large Hadron Collider. That machine will shine far more brightly than before, so its parts must survive strong neutron doses. Small test diodes on the new eight-inch wafers served as the test pieces.
The team exposed diodes to neutrons at a reactor in Slovenia, at thirteen dose levels. They then measured how much charge each diode could still collect while it was held warm, a step called annealing. The tests used an electric pulse method to read charge flow. Results helped the group judge whether thicker sensors can work in the harshest zones, and how much healing to expect during planned shutdowns.
Catalog record
| CREATOR | Matteo M. Defranchis |
|---|---|
| YEAR | 2025 |
| COLLECTION | PAPERS |
| FORMAT | TXT |
| FILE SIZE | 39 KB |
| VERSION | 1.0 |
| LICENSE | http://creativecommons.org/licenses/by/4.0/ |
| RIGHTS | CC BY |
| SOURCE | arXiv |
Source: https://arxiv.org/abs/2503-01520
Browse the full library · About the Tower of Babel
Full text
The opening of the work, from the library's hosted text:
Annealing behaviour of charge collection of neutron irradiated diodes from 8-inch p-type silicon wafers Matteo M. Defranchis Abstract To face the higher levels of radiation due to the 10-fold increase in integrated luminosity during the High-Luminosity LHC, the CMS detector will replace the current Calorimeter Endcap (CE) using the High-Granularity Calorimeter (HGCAL) concept. The electromagnetic section as well as the high-radiation regions of the hadronic section of the CE will be equipped with silicon pad sensors, covering a total area of 620 m 2 \rm m^{2} . Fluences up to 1.0 ⋅ 10 16 n eq / cm 2 \rm 1.0\cdot 10^{16}~n_{eq}/cm^{2} and doses up to 2 MGy are expected considering an integrated luminosity of 3 ab − 1 \rm ab^{-1} . The whole CE will normally operate at -35°C in order to mitigate the effects of radiation damage. The silicon sensors are processed on 8-inch p-type wafers with an active thickness of 300 µm, 200 µm and 120 µm and cut into hexagonal shapes for optimal use of the wafer area and tiling. With each main sensor several small sized test structures (e.g pad diodes) are hosted on the wafers, used for quality assurance and radiation hardness tests. In order to investigate the radiation-induced bulk damage, 28 diodes have been irradiated with reactor neutrons at the TRIGA reactor in JSI (Jožef Stefan Institute, Ljubljana) to 13 fluences between 6.5 ⋅ 10 14 n eq / cm 2 \rm 6.5\cdot 10^{14}~n_{eq}/cm^{2} and 1.5 ⋅ 10 16 n eq / cm 2 \rm 1.5\cdot 10^{16}~n_{eq}/cm^{2} . The charge collection of the irradiated silicon diodes was determined through transient current technique (TCT) measurements. The study focuses on the isothermal annealing behaviour of the bulk material at 60°C. The results have been used to extend the usage of thicker silicon sensors in regions expecting higher fluences and are being used to estimate the expected annealing effects of the silicon sensors during year-end technical stops and long HL-LHC shutdowns currently foreseen with a temperature around 0°C. 1 Introduction The High-Luminosity Large Hadron Collider (HL-LHC) upgrade aims at enhancing the performance of the LHC, the most powerful particle accelerator in the world, to boost the potential for scientific discoveries starting from 2030. The project includes increasing the luminosity (and thus the collision rate) by a factor of five beyond the original LHC design specifications. The integrated luminosity will be increased by a factor of ten. This poses significant challenges in terms of radiation tolerance and event pileup for the detectors [ 1 , 2 ] . As part of the HL-LHC upgrade within the CMS Experiment [ 3 ] , the current Calorimeter Endcap (CE) will be replaced, using the novel High Granularity Calorimeter (HGCAL) concept. It will consist of 47 sampling layers interleaved with Cu, CuW, Pb and stainless steel absorber plates and will include nearly six million readout channels. Silicon sensors were selected as active material for the majority of the CE upgrade due to their compactness, rapid signal formation, and adequate radiation hardness. At the HL-LHC, these silicon sensors will be subjected to hadron fluences ranging from approximately \rm 2.0\cdot 10^{14} 1-MeV neutron-equivalents per square centimeter \rm(n_{eq}/cm^{2}) to \rm 1.0\cdot 10^{16}n_{eq}/cm^{2} after an integrated luminosity of 3000 \rm fb^{-1} . Around 620 \rm m^{2} of silicon sensors will cover the entire electromagnetic (CE-E) section and the high-radiation region of the hadronic (CE-H) section of the calorimeter. The silicon sensors are fabricated on 8-inch wafers and diced to form a hexagonal shape for efficient use of the wafer area and tiling [ 4 , 2 ] . In this paper, we report about three measurement campaigns investigating isothermal annealing behaviour of the charge collection capability of the silicon bulk material using dedicated test structure 5x5 \rm mm^{2} diodes from the edge region of the wafer, irradiated with reactor neutrons up to \rm 1.5\cdot 10^{16}n_{eq}/cm^{2} . As the CMS detector region to be occupied by CE will be irradiated predominantly by neutrons [ 2 ] , these particles were the main focus of the irradiation. The campaigns were performed in 2021 and 2023 in two different measurement setups. Section 2 gives an overview and detailed information about the samples used in each campaign. The measurement setups and techniques are described in section 3 . An insight into the data analysis procedure is presented in section 4 . The discussion on the systematic uncertainties is provided in section 5 . The results and interpretation of the obtained data can be found in section 6 . Finally, the summary and conclusions are given in section 7 . 2 Samples The silicon sensors to be used in the CMS Calorimeter Endcap upgrade consist of DC-coupled, planar, high resistivity (>3 kΩcm), p-type hexagonal silicon sensors with a crystal orientation of <100> produced on 8-inch circular wafers by Hamamatsu Photonics K.K 1 1 1 https://www.hamamatsu.com/eu/en.html (shown in figure 1 ) [ 2 ] . Sensors are produced in three different active thicknesses and two material types. 300 µm and 200 µm sensors are produced in the float zone (FZ) process, whereas 120 µm sensors are produced in the epitaxial (EPI) process on top of a handling wafer of \sim 180 µm thickness. The remaining space left around the hexagonal main sensor (called "halfmoons") is used for the fabrication of small-sized test structures, which have an identical production process as the main sensor. The test structures include, among others, single diodes which can be used to investigate the bulk radiation hardness of the sensors. For the measurements presented here, square diodes with a side length of 5 mm are chosen. The (main) n+ pad implant is surrounded by a guard ring. Figure 1 : CE full sensor on 8-inch circular wafer including test structures. The silicon crystal orientation is presented as black dashed lines. The example halfmoon section containing the diode used in this publication is marked in red frame (the diode used has cross-sectional area 5x5 \rm mm^{2} ). Reproduced from [ 5 ] . In the following, results from three independent charge collection measurement campaigns are presented, performed in two different setups referred to as "TCT+ setup" and "Particulars setup" 2 2 2 https://particulars.si/index.php . The setups are described in detail in section 3 . In the TCT+ setup, two measurement campaigns were performed - one in 2021 with CE version-1 prototype samples, irradiated to intermediate fluences ( \rm 6.5\cdot 10^{14}n_{eq}/cm^{2} to \rm 1.0\cdot 10^{16}n_{eq}/cm^{2} ) and one in early 2023 with CE version-2 prototype samples (and with additional version-1 prototype 120 µm samples), irradiated to higher fluences ( \rm 1.5\cdot 10^{15}n_{eq}/cm^{2} to \rm 1.4\cdot 10^{16}n_{eq}/cm^{2} ). The third campaign was performed in the Particulars setup in 2023, where CE pre-series samples, irradiated to higher fluences ( \rm 2.0\cdot 10^{15}n_{eq}/cm^{2} to \rm 1.5\cdot 10^{16}n_{eq}/cm^{2} ), were measured. Version-1, version-2 prototypes and pre-series sensors represent different iterations of sensors produced for CE. The iterations differ in terms of parameters regarding the oxidation process. Typical variations in the bulk production process are known to be independent of the manufacturer’s oxidation process. The bulk properties of the silicon material are defined in the procurement documents and are expected to remain consistent across production iterations. All wafers are certified