The link between Microstructural Heterogeneity, Diffusivity, and Hydrogen Embrittlement

Daniel J. Long ∗, Edmund Tarleton, Alan C.F. Cocks, Felix Hofmann † · 2025

Read The link between Microstructural Heterogeneity, Diffusivity, and Hydrogen Embrittlement by Daniel J. Long ∗, Edmund Tarleton, Alan C.F. Cocks, Felix Hofmann † (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2502-13793.txt.

Introduction

Daniel Long, Edmund Tarleton, Alan Cocks, and Felix Hofmann linked crystal-scale structure in two thousand twenty-five to hydrogen damage in metals. Green hydrogen may power future aircraft, but hydrogen can make fuel system metals brittle. How the metal's inner grain pattern steers hydrogen build-up was not well captured at part scale.

Their model joins micro-scale mechanics with hydrogen transport in a random, multi-scale frame that still runs at millimetre scale. Grain pattern strongly shaped where hydrogen gathered, with loading speed in play. For stainless steel and nickel, model results matched measured embrittlement, tying loading-rate effects to grain-scale hydrogen motion. Designers should build grain traits into hydrogen-proof metals.

Catalog record

CREATORDaniel J. Long ∗, Edmund Tarleton, Alan C.F. Cocks, Felix Hofmann †
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE73 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2502-13793

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

The link between Microstructural Heterogeneity, Diffusivity, and Hydrogen Embrittlement Daniel J. Long ∗, Edmund Tarleton, Alan C.F. Cocks, Felix Hofmann † Abstract Correspondence: ∗ [email protected] , † [email protected] Abstract Green hydrogen is likely to play a major role in decarbonising the aviation industry. It is crucial to understand the effects of microstructure on hydrogen redistribution, which may be implicated in the embrittlement of candidate fuel system metals. We have developed a stochastic multiscale finite element modelling framework that integrates micromechanical and hydrogen transport models, such that the dominant microstructural effects can be efficiently accounted for at millimetre length scales. Our results show that microstructure has a significant effect on hydrogen localisation in elastically anisotropic materials, which exhibit an interesting interplay between microstructure and millimetre-scale hydrogen redistribution at various loading rates. Considering 316L stainless steel and nickel, a direct comparison of model predictions against experimental hydrogen embrittlement data reveals that the reported sensitivity to loading rate is strongly linked with rate-dependent grain scale diffusion. These findings highlight the need to incorporate microstructural characteristics in the design of hydrogen resistant materials. 1 Introduction As the UK government strives to achieve Net Zero by 2050, many of the largest industries are exploring pathways to integrate renewable and environmentally friendly energy sources. For the aerospace sector, hydrogen may become a viable alternative propulsion fuel. The challenges of this, however, are the known damaging effects of hydrogen in metallic materials [ 1 ] . This is not to mention the unprecedented complexity of a hydrogen fuel system which would encompass vast temperature and pressure ranges (from high pressure cryogenic storage to high temperature combustion [ 2 ] ). Whilst many models [ 3 , 4 ] have been developed to capture hydrogen embrittlement (HE) in structural metallic materials, little has been achieved towards explaining the large degree of variation reported between different alloys [ 5 ] . Understanding this will be vital for effective material selection and design. Using a multiscale modelling methodology, this paper investigates the connection between varying degrees of HE and relevant microstructural properties. Across the theoretical and experimental literature, the most widely reported mechanisms for HE (in non-hydride forming materials) are hydrogen enhanced localised plasticity (HELP) [ 6 , 7 ] and hydrogen enhanced decohesion (HEDE) [ 8 , 9 ] . The mechanistic basis for HELP is that dislocations sequester and trap mobile hydrogen, which enhances dislocation mobility, resulting in the accelerated accumulation of dislocations, i.e., localised plasticity and damage [ 10 ] . Existing experimental evidence [ 11 ] , which is supported by discrete dislocation analyses [ 12 ] , suggests that hydrogen reduces the interaction energies between dislocations, leading to diminished hardening rates and the early onset of plasticity. The HEDE mechanism suggests that the interfacial cohesive strengths of grain boundaries (GBs) and other microstructural hydrogen trapping sites are diminished by the presence of hydrogen, resulting in brittle interfacial fracture (as opposed to ductile void growth and coalescence), for which there is ample experimental evidence [ 13 , 14 , 15 ] . Atomistic modelling by Katzarov et al. [ 8 ] showed that during decohesion of (111) planes in stressed and hydrogenated \alpha -Fe, plane separation promotes hydrogen ingress and trapping (due to expansion of interstitial sites), which reduces the interface binding energy and hence the interfacial cohesive strength by up to a third, even for very low bulk hydrogen concentrations. While HELP and HEDE mechanisms are often attributed to the embrittlement of materials independently of one another, it is conceivable that they act reciprocally, viz., HELP promotes HEDE. Robertson et al. [ 16 ] reported that HELP accelerates the rate at which glissile dislocations pile up at GBs, while also reducing pile-up dislocation spacing (due to hydrogen-affected dislocation interaction energies). The consequences of increased dislocation mobility and density are that (i) there is an increased probability of slip along GBs, which can weaken the cohesive strength, (ii) transport of hydrogen to the GBs is increased via high density dislocations networks, and (iii) GB disorder will increase due to the increased likelihood for slip transfer between grains where the local stress field is enhanced by dense dislocation pile-ups [ 16 , 17 ] . The main consequence of (iii) is that the capacity for hydrogen at GBs will be increased. These HE mechanisms are strongly influenced by the local hydrogen content, and hence, factors which affect the redistribution of hydrogen at microstructure length scales need to be carefully considered. Hassan et al. [ 4 ] used a micromechanical crystal plasticity finite element (CPFE) modelling framework to study the transient redistribution of hydrogen in pre-hydrogenated non-textured polycrystals under external and plasticity-driven residual internal stresses after deformation. The diffusion model accounted for the evolution of hydrogen traps (dislocations) driven by plastic strain evolution, which were shown to substantially reduce the overall apparent diffusivity through polycrystalline 316L stainless steel. Moreover, the application of 20% biaxial strain to the equiaxed polycrystal was predicted to drive H concentrations up by up to a factor of two (relative to the initial value), while residual stresses due to plasticity in the unloaded state yielded similar results. Tondro et al. [ 18 ] adopted a similar framework to study the hydrostatic stress-driven redistribution of hydrogen in zirconium polycrystals; results showed that the distribution of loads between hard and soft grains significantly influences how hydrogen is distributed. Specifically, load shedding [ 19 ] means that higher hydrostatic stresses are generated in hard grains, driving an increased hydrogen-influx, whilst soft grains exhibit more plasticity and greater dislocation content which increase trapped hydrogen. In general, GB stress concentration features accumulated high levels of hydrogen, and triple junctions were found to promote particularly high concentrations, likely to foster HEDE. In modelling the direct mechanical effects of hydrogen, numerous approaches from atomistic to millimetre length scales have been utilised. Ab initio models [ 6 , 8 ] were previously discussed in the context of HE; these methods have generated important mechanistic insights into HELP and HEDE, which are crucial for deterministic model development at larger length scales. Similarly, dislocation-level models have been developed to study these respective embrittlement mechanisms. Using a discrete dislocation plasticity (DDP) framework, Irani et al. [ 20 ] showed that the tensile hydrostatic stress field generated by an individual dislocation (trap) attracts hydrogen; Yu et al. [ 12 ] later demonstrated via DDP modelling that hydrogen can accelerate dislocation generation and slip planarity. While both of these findings provide helpful reinforcing evidence of HELP, due to the pragmatic limitations of high-fidelity modelling, DDP cannot yet predict material behaviour at component length scales. At the grain scale, CPFE modelling has been most widely used to study microstructure-driven hydrogen redistribution and embrittlement [ 4 , 21 , 22 , 23 ] . Ilin et al. [ 21 ] were among the first to illustrate the effects of microstructure heterogeneity on the localisation of hydrogen in a case study of 316L stainless steel under uniaxial tensile loads; strain-rate was shown to impact the magnitude of redistribution significantly due to the time dependent nature of hydrogen diffusion. Hussein et al. [ 23 ] later presented a thorough comparative study of the micromechanical redistribution of hydrogen in high and low-strength

Read the complete text