Read The Influence of V-Defects, Leakage, and Random Alloy Fluctuations on the Carrier Transport in Red InGaN MQW LEDs by Huai-Chin Huang 1, Shih-Min Chen 1, Claude Weisbuch 3, James S. Speck 2, Yuh-Renn Wu 1* (2025) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2501-19020.txt.

Introduction

Red light chips lag their blue and green kin, and the gap is a physics puzzle. The authors, a five-name team writing in 2025, simulate how charge moves through the red chip's stacked wells. Three quirks share the blame in their model: pits in the crystal face, uneven alloy mix, and leak paths along flaw lines. In blue and green chips the pits help by giving charge a side door in.

In red chips that door barely cuts the start voltage, and the math still calls for more volts than labs see. Leak paths fill the gap: stray charge slips in early, pools in the wells, and screens the inner walls that block flow. The same leaks waste some charge as heat near the flaws. The team map the trade and point to build tweaks that keep the gain.

Catalog record

CREATORHuai-Chin Huang 1, Shih-Min Chen 1, Claude Weisbuch 3, James S. Speck 2, Yuh-Renn Wu 1*
YEAR2025
COLLECTIONPAPERS
FORMATTXT
FILE SIZE49 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2501-19020

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

The Influence of V-Defects, Leakage, and Random Alloy Fluctuations on the Carrier Transport in Red InGaN MQW LEDs Huai-Chin Huang 1, Shih-Min Chen 1, Claude Weisbuch 3, James S. Speck 2, Yuh-Renn Wu 1* Abstract Red InGaN-based light-emitting diodes (LEDs) exhibit lower internal quantum efficiencies (IQEs) than violet, blue, and green InGaN LEDs due to a reduction in radiative recombination rates relative to non-radiative recombination rates as the Indium composition increases. Additionally, the larger polarization and band offset barriers between high indium content InGaN quantum wells and GaN quantum barriers increase the forward voltage. In blue and green LEDs, random alloy fluctuations and V-defects play a key role in reducing the forward voltage. When V-defects are present, either naturally or intentionally introduced, they create an alternative path for carrier injection into the MQWs through the V-defect sidewalls. This injection mechanism explains the turn-on voltages of green LEDs. However, in InGaN red LEDs, these two phenomena do not reduce the forward voltage as effectively as in blue and green LEDs, and consequently, the computed forward voltage remains significantly higher than the measured one. Furthermore, currents are observed at low voltages before the turn-on voltage ( V < ℏ ​ ω / e = 2.0 ​ V V<\hbar\omega/e=2.0\,\text{V} ) of red LEDs. To address this, we introduce dislocation-induced tail states in the modeling, suggesting that leakage current through these states may play a significant role both below and at turn-on voltages. The simulation also indicates that leakage carriers below turn-on accumulate, partially diffuse in the QWs, screen the polarization-induced barrier in the low injection regime, and further reduce the forward voltage. Despite these beneficial effects, a drawback of dislocation-induced tail states is the enhanced nonradiative recombination in the dislocation line region. This study provides a detailed analysis of device injection physics in InGaN QW red LEDs and outlines potential optimization strategies. Preprint: AIP/123-QED I Introduction In recent years, the study of indium gallium nitride (InGaN) materials has gained significant attention for their applications in micro light-emitting diodes ( \mu -LEDs). The superior efficiency, thermal stability, and emission characteristics of InGaN-based red-green-blue (RGB) micro-LEDs have made them increasingly desirable, especially as display technologies trend toward smaller chip and pixel sizes [ 1 , 2 , 3 , 4 ] . Regarding efficiency, blue InGaN LEDs achieve peak internal quantum efficiency (IQE) exceeding 90% at a current density of 1-10 A/cm 2 [ 4 , 5 , 6 ] . However, improving the IQE of red InGaN LEDs has proven particularly challenging, primarily due to the “green gap” with the factors contributing to the green gap being even more pronounced in the red spectral region [ 7 , 8 ] . A key reason for the lower efficiency of high-indium-content InGaN QWs is the longer radiative lifetime caused by the large polarization-induced electric field in the QWs, which results in reduced electron-hole overlap [ 9 ] relative to other non-radiative recombination mechanisms. Another challenge is the lower crystal quality of the QWs due to the relatively low growth temperature required for high-indium-content InGaN QWs. Additionally, the wall-plug efficiency (WPE) is affected by the operating voltage, which is primarily increased due to vertical carrier injection being significantly hindered by the large polarization-induced energy barriers at the quantum well/quantum barrier interfaces and the large band offsets [ 9 , 10 , 11 , 12 ] . However, experimental results show that the turn-on voltage of red LEDs is close to its theoretical value, indicating the presence of alternative carrier injection mechanisms beyond vertical injection. Figure 1: (a) Bandgap distribution map of the simulated 9QW Red LED structure with random alloy fluctuations and V-defects. (b) Cross-section of a V-defect and threading dislocation line at the of the V-defect. The TD dislocation line is modeled as a 30 nm diameter cylinder with a high density of fast nonradiative traps, and a short nonradiative lifetime value in this region. (c) Conduction band potential plotted in log scale. The strong polarization-related and band offset barriers for the c-plane QWs result in carriers flowing through semipolar planes with much-reduced energy variations. (d) Computed band extrema across the vertical LED structure away from the V-defect, taking alloy fluctuations into account (green and violet) or not (blue and red) curves, respectively. In the case of alloy fluctuations, band potential is spatially-averaged over the QW in-plane area. Random fluctuations aid carrier flow by decreasing the effective potential of quantum barriers [ 13 ] . Two mechanisms that reduce the turn-on voltage in blue and green LEDs have been previously identified and simulated. The natural alloy fluctuation of the InGaN QW material provides local reductions in the barriers for vertical transport in GaN-based blue LEDs (QBs) (Figs. 1 (c) and 1 (d)) [ 14 , 15 ] , enabling percolative paths for currents at lower applied voltages than those required in uniform materials. However, natural alloy disorder alone is insufficient to significantly reduce the barriers for vertical transport in green or red LEDs, leading to their higher forward voltage. One approach to mitigating this issue is carrier injection through V-defects, which are three-dimensional features that form under kinetically limited epitaxial growth conditions (Figs. 1 (a) and 1 (b)) [ 14 , 16 , 17 , 18 , 19 , 20 , 21 , 22 , 23 , 24 , 25 , 26 ] . Simulations of carrier injection through the shallower and semipolar MQWs of the V-defect sidewalls show that substantial lateral hole injection into the quantum wells occurs at lower forward voltages than for vertical injection, complementing the vertical injection path. Thus, V-defects enhance the LED WPE by reducing the forward voltage [ 10 , 27 , 28 ] . However, their presence may also reduce the IQE due to the non-radiative dislocation region of the V-defect [ 28 ] . In green LEDs, V-defects ultimately improve WPE, as the voltage reduction outweighs the potential decrease in IQE. With sidewall injection from V-defects in green LEDs, current flow becomes lateral in the quantum well, where limited lateral carrier diffusion leads to local current crowding near V-defects and minimal or no improvement in current efficiency droop. However, in InGaN red LEDs, simulations show that these two phenomena do not reduce the forward voltage to the same extent as in blue and green LEDs. Consequently, the computed forward voltage remains significantly higher than the measured one. Additionally, large leakage currents are observed at low voltages before the turn-on voltage ( V<\hbar\omega/e=2.0\,\text{V} ) of red LEDs [ 29 , 30 ] . To address this, we introduce dislocation-induced tail states in the modeling, as leakage current through such states may play a significant role both below and at turn-on voltages. The simulation further reveals that leakage carriers below turn-on accumulate in the QWs, screen the piezoelectric field-induced barrier in the low injection regime, and further lower the forward voltage. While this effect is beneficial, a drawback of these dislocation-induced tail states is the enhanced nonradiative recombination in the dislocation line region. Our model incorporates tail states in a two-dimensional drift-diffusion charge control (2D-DDCC) simulation, where we successively analyze the effects of: (1) random alloy fluctuations, (2) V-defects, and (3) tail states [ 31 ] on device performance.

Read the complete text