The effect of grain boundary misorientation on hydrogen flux using a phase-field based diffusion and trapping model Published in: Advanced Engineering Materials 26(22)(2024): 2401561

Abdelrahman Hussein, Byungki Kim, Kim Verbeken, Tom Depover · 2024

Read The effect of grain boundary misorientation on hydrogen flux using a phase-field based diffusion and trapping model Published in: Advanced Engineering Materials 26(22)(2024): 2401561 by Abdelrahman Hussein, Byungki Kim, Kim Verbeken, Tom Depover (2024) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2412-19129.txt.

Introduction

Abdelrahman Hussein and co-authors model how grain boundaries steer hydrogen through metals in a 2024 paper. Trapped hydrogen can embrittle steel and alloys. Boundaries between crystal grains both trap and channel it. Their phase-field model splits boundaries into high-angle and low-angle types.

Uptake runs showed smaller grains soak up more hydrogen. Boundaries acted as high-flux paths overall. High-angle boundaries, binding hydrogen more strongly, carried the most flux. Yet the pattern twists with local trapping balance. The model helps engineers predict where hydrogen damage will strike first in pipelines, pressure tanks, and other steel parts.

Catalog record

CREATORAbdelrahman Hussein, Byungki Kim, Kim Verbeken, Tom Depover
YEAR2024
COLLECTIONPAPERS
FORMATTXT
FILE SIZE30 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2412-19129

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

The effect of grain boundary misorientation on hydrogen flux using a phase-field based diffusion and trapping model Published in: Advanced Engineering Materials 26(22)(2024): 2401561 Abdelrahman Hussein, Byungki Kim, Kim Verbeken, Tom Depover Abstract Understanding hydrogen-grain boundary (GB) interactions is critical to the analysis of hydrogen embrittlement in metals. This work presents a mesoscale fully kinetic model to investigate the effect of GB misorientation on hydrogen diffusion and trapping using phase-field based representative volume elements (RVEs). The flux equation consists of three terms: a diffusive term and two terms for high and low angle grain boundary (H/LAGB) trapping. Uptake simulations showed that decreasing the grain size resulted in higher hydrogen content due to increasing the GB density. Permeation simulations showed that GBs are high flux paths due to their higher enrichment with hydrogen. Since HAGBs have higher enrichment than LAGBs, due to their higher trap-binding energy, they generally have the highest hydrogen flux. Nevertheless, the flux shows a convoluted behavior as it depends on the local concentration, alignment of GB with external concentration gradient as well as the GB network connectivity. Finally, decreasing the grain size resulted in a larger break-through time and a larger steady-state exit flux. 1 Introduction One of the challenges for realizing the full potential of hydrogen as a reliable clean energy carrier is hydrogen embrittlement (HE). This is a broad family of damage micromechanisms, which are activated by the accumulation (trapping) of hydrogen at different microstructure features, predominantly at grain boundaries (GBs) and interfaces [ 1 , 2 , 3 ] . Yet, GBs and interfaces are complex and multifaceted features that can be categorized based on the type of the phases comprising the interface, their orientations, topology etc. These interfaces are critical hydrogen assisted crack initiation sites in several alloys. Triple junctions (TJs) were reported as crack initiation sites [ 4 ] in austenitic steels. Interaction of strain localization and interface decohesion were reported in dual-phase [ 5 ] , ferritic [ 6 ] and pearlitic steels [ 7 ] . High angle grain boundaries (HAGBs) were found to be more susceptible to hydrogen assisted crack initiation and propagation compared to low angle grain boundaries (LAGBs) in Ni alloy 725 [ 8 ] . Increasing the fraction of special low-energy grain boundaries improved the resistance to intergranular cracking in pure Ni [ 9 ] . Hence, grain boundary engineering (GBE) is one of the primary strategies to alleviate the severity of HE [ 10 , 11 ] . From this brief overview, a comprehensive GBE strategy requires a solid understanding of the two-way hydrogen GB interactions, i.e. how GBs retain hydrogen and how hydrogen initiates damage at the GBs. The former will be the topic of this article. Traditionally, the kinetics of hydrogen diffusion and trapping are investigated using permeation experiments [ 12 ] . More novel techniques like atom probe tomography, scanning kelvin probe force microscopy and silver decoration could provide more spatial and temporal resolution of hydrogen-microstructure interactions [ 13 , 14 ] . To understand the effect of GB misorientation on hydrogen flux, Koyama et al [ 15 ] used permeation experiments together with in-situ silver decoration to spatially and kinetically resolve hydrogen mapping at the exit side of pure Fe. They found that GBs, especially HAGBs, are high flux paths compared to the lattice. This flux depends on the local diffusivity and concentration gradient. Since a constant diffusivity was assumed in pure Fe [ 16 ] , the increased GB hydrogen enrichment due to trapping resulted in such high flux. In order to have more quantitative understanding of such complex interactions, a fully kinetic mesoscale hydrogen diffusion and trapping model, which can resolve features like GBs and their type is required. The most widely used models in the analysis of hydrogen transport are based on the macroscopic models of McNabb and Foster [ 17 ] , Oriani [ 18 ] , which is coupled with mechanical effects by Sofronis and McMeeking [ 19 ] and further modified by Krom et al. [ 20 ] . Mesoscale models based on representative volume elements (RVEs) [ 21 , 22 , 23 ] can provide more quantitative understanding of such complex interactions. To this end, a phase-field 1 1 1 It should be noted that in this work, the phase-field method is used to develop RVEs and represent microstructure features like grains and GBs, which is different than the phase-field fracture used in [ 24 ] . based fully kinetic hydrogen diffusion and trapping model that can resolve the effect of HAGBs/LAGBs on hydrogen flux is presented in this work. First, starting from a total free energy functional in section 2 , a fully kinetic hydrogen diffusion and trapping equation is derived. The computational setup together with the RVE generation and assigning orientations to account for GB misorientation is described in section 3 . Three RVEs were generated to study the effect of grain size. Additionally, two types of simulations were performed: uptake and permeation. The results of these simulations are discussed in section 4 and were in good qualitative agreement with the experiments in [ 15 ] . The methodology described in this work lays the foundation for in-silico framework for grain boundary engineered hydrogen resistant microstructures. 2 Modelling framework 2.1 Equilibrium and transport equations The phase-field method represents the grains by a vector of order parameters \phi_{i} , which take the values 0\leq\phi\leq 1 . The principle of the phase-field based hydrogen diffusion and trapping model is to use functions of the phase-field order parameters as potentials, where their functional gradient induces a trapping flux. A fully kinetic equation for hydrogen diffusion and trapping at HAGB/LAGB can be then derived from the total free energy functional F=\int_{V}\Big[f^{\mathrm{ch}}+f^{\mathrm{HAGB}}+f^{\mathrm{LAGB}}\Big]dV (1) Where f^{\mathrm{ch}} is the chemical free energy. The solvent atoms are considered fixed in their lattice position, and thus, do not contribute to the entnropy of mixing part of f^{\mathrm{ch}} . Using the compound energy formalism for a two-sublattice model, where the solvent atoms are assumed fixed in their lattice position, and considering only the ideal chemical free-energy f^{\mathrm{ch}}=(1-\theta)G_{X:Va}+\theta G_{X:H}+\frac{NRT}{V_{\mathrm{m}}}\left[(1-\theta)\ln(1-\theta)+\theta\ln\theta\right] (2) Where the solvent atom is X , \theta is the hydrogen occupancy, hydrogen atoms (H) and vacancies (Va) occupy the interstitial sites, N is the number of interstitial sites per lattice unit cell per solvent atom. For the case of the BCC lattice with tetrahedral interstitial sites N=6 , while for FCC lattice with octahedral sites N=4 [ 25 ] . R is the universal gas constant, T is the temperature and V_{\mathrm{m}} is the molar volume of the host lattice. A double-obstacle potential can be used with the misorientation angle \Delta\psi_{\alpha\beta} between two grains \alpha and \beta for calculating the HAGBs function g(\phi)_{\mathrm{HAGB}} and LAGBs function g(\phi)_{\mathrm{LAGB}} according to Algorithm 1 . f^{\mathrm{HAGB}} is the HAGB trapping energy density, which is constructed to decrease with increasing hydrogen occupancy f^{\mathrm{HAGB}}=g(\phi)_{\mathrm{HAGB}}(1-\kappa_{\mathrm{HAGB}}\theta) (3) Where \phi is the vector of phase-field variables representing each grain, which takes the values 0\leq\phi\leq 1 . g(\phi)_{\mathrm{HAGB}} is the double-obstacle potential representing the HAGB. \kappa_{\mathrm{HAGB}} is a parameter related to the HAGB trap-binding energy that will be evaluated from equilibrium as described later. Similarly, f^{\mathrm{LAGB}} is the LAGB trapping energy

Read the complete text