A diffuse-interface model for predicting the evolution of metallic negative electrodes and interfacial voids in solid-state batteries with homogeneous and polycrystalline solid electrolyte separators.

Sourav Chatterjee, Michael Tonks, William Gardner, Marina Sessim · 2024

Read A diffuse-interface model for predicting the evolution of metallic negative electrodes and interfacial voids in solid-state batteries with homogeneous and polycrystalline solid electrolyte separators. by Sourav Chatterjee, Michael Tonks, William Gardner, Marina Sessim (2024) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2412-17147.txt.

Introduction

Sourav Chatterjee, Michael Tonks, William Gardner, and Marina Sessim model a failure mode in solid-state batteries, in a research paper from 2024. As a metal electrode gives up and regains ions during use, empty pockets, called voids, can grow where it meets the solid electrolyte. Those voids weaken the cell.

Their model follows the electrode surface and the voids at the same time. They test it on a sodium cell with a ceramic separator, in cases with a clean contact, one void, and many voids. Void growth rose in step with how fast sodium atoms left the void edge. Grain boundaries in the ceramic changed growth only locally.

Catalog record

CREATORSourav Chatterjee, Michael Tonks, William Gardner, Marina Sessim
YEAR2024
COLLECTIONPAPERS
FORMATTXT
FILE SIZE113 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2412-17147

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

A diffuse-interface model for predicting the evolution of metallic negative electrodes and interfacial voids in solid-state batteries with homogeneous and polycrystalline solid electrolyte separators. Sourav Chatterjee, Michael Tonks, William Gardner, Marina Sessim Abstract This paper presents a novel diffuse-interface electrochemical model that simultaneously simulates the evolution of the metallic negative electrode and interfacial voids during the stripping and plating processes in solid-state batteries. The utility and validity of this model are demonstrated for the first time on a cell with a sodium (Na) negative electrode and a Na- β ′′ \beta^{\prime\prime} -alumina ceramic solid electrolyte (SE) separator. Three examples are simulated. First, stripping and plating with a perfect electrode/electrolyte interface; second, stripping and plating with a single interfacial void at the electrode/electrolyte interface; third, stripping with multiple interfacial voids. Both homogeneous SE properties and polycrystalline SEs with either low or high conductivity grain boundaries (GBs) are considered for all three examples. Heterogeneous GB conductivity has no significant impact on the behavior with a perfect electrode/electrolyte interface. However, it does result in local changes to void growth due to interactions between the void edge and the GBs. The void growth rate is a linear function of the flux of Na atoms at the void edge, which in turn depends on the applied current density. We also show that the void coalescence rate increases with applied current density and can be marginally influenced by GB conductivity. Journal: Journal of the Electrochemical Society 1 Introduction Since the 1990s, lithium (Li)-ion batteries (LIBs) have been the prevalent form of energy-storage technology used in portable devices and electric vehicles [ 1 , 2 ] . However, conventional LIBs with a graphite negative electrode are soon expected to reach their specific energy limit ( \sim 250 Wh/kg) [ 3 , 4 , 5 ] . By replacing graphite with Li metal as the negative electrode, cells with higher specific energy ( > 500 Wh/Kg) and voltage could be potentially realized because Li has \sim 10 times higher specific capacity ( 3861 mAh/g) than graphite ( 372 mAh/g); and has one of the lowest standard reduction potentials ( -3.04 V vs standard hydrogen electrode) [ 5 , 6 , 7 ] . However, the global reserves of Li are limited, and the future cost of Li is expected to increase given the rising energy-storage demands [ 8 , 9 ] . Batteries with metallic sodium (Na) negative electrodes are an attractive alternative to Li metal batteries because Na is more abundant and has a lower cost than Li and has a higher specific capacity ( 1166 mAh/g) than graphite. Batteries with metallic negative electrodes and ionically-conducting liquid electrolytes fail due to dendrite-induced cell shortcircuiting [ 10 , 11 , 7 , 12 ] . Another disadvantage of liquid electrolytes is that they are highly flammable [ 1 ] . Substituting liquid electrolytes with ionically-conducting ceramic-based solid electrolytes is a promising strategy to enable metallic negative electrodes and mitigate the fire risk associated with LIBs. Consequently, all-solid-state batteries (ASSBs) with metallic negative electrodes and ceramic-based solid-state electrolytes are considered a safer and promising alternative to LIBs [ 13 ] . Despite these advantages, ASSBs can fail due to void-induced dendrite formation at relatively high cycling current densities [ 14 , 15 ] , making them unsuitable for fast-charging applications. Several researchers have reported Na or Li dendrite penetration through the ceramic-based solid electrolyte separators at cycling current densities that are well below the desired current densities required for fast-charging applications [ 16 , 17 , 18 , 19 , 20 , 21 ] [ 22 ] [ 11 ] , [ 23 ] . Recently, Kasemchainan et al. [ 19 ] pointed out two critical current densities that are relevant in understanding dendrite formation during the cycling of ASSBs. First is the critical current density for plating (CCP), above which cell failure invariably occurs due to dendrite formation. Second is the critical current density for stripping (CCS), above which cell failure occurs due to void-induced dendrite formation. Cycling above CCS inevitably leads to void formation at the electrode/solid electrolyte separator interface. These voids increase the interfacial resistance [ 24 ] and cause the current to get concentrated near the void edges. During subsequent charging cycle, these current density hotspots induce dendrite formation as the local current density may well exceed CCP [ 19 ] , [ 21 ] [ 25 , 26 , 27 ] . Consequently, the CCS determines the maximum cycling current density below which ASSBs can be safely cycled without dendrite formation [ 28 ] . Thus, understanding factors that mitigate void formation and increase CCS can help design practical and fast-charging ASSBs. Several experimental groups [ 29 , 14 , 30 , 31 , 28 , 15 ] , including Kasemchainan et al. [ 19 ] , have suggested factors that enhance CCS in ASSBs with metallic electrodes. One is applying an increased stack pressure on the metallic negative electrode as it suppresses void growth due to creep deformation. Another factor that helps reduce void formation is using alkali metal electrodes with lower creep resistance, such as Na or potassium [ 32 ] . This explains why Na-metal ASSBs typically exhibit higher CCS than Li-metal ASSBs for a given applied stack pressure and temperature [ 15 ] . For instance, Jolly et al. [ 28 ] reported CCS to be around 1.5-2.5 mA/cm 2 at room temperature in an ASSB with a Na negative electrode and a Na- {\beta^{\prime\prime}} -alumina ceramic solid electrolyte separator when cycled under a stack pressure of 4-9 MPa. Although these factors are useful indicators in mitigating void growth, a quantitative understanding of the impact of metallic electrodes and solid electrolyte properties on void evolution is still lacking. Moreover, atomistic [ 33 , 34 ] and continuum scale [ 35 , 36 , 37 ] models have been proposed in the literature to understand void formation and growth in ASSBs. However, these works have been applied only to Li metal batteries. For instance, Yang et al. studied the impact of adhesion energy and pressure on void formation in a Li-metal/Li 7 La 3 Zr 2 O 12 (LLZO) cell using large-scale molecular dynamics simulations. Their results suggest strong interface adhesion and high pressure mitigate void formation during stripping [ 33 ] . At the continuum scale, Zhao et al. [ 36 ] used the phase-field method to simulate the evolution of micron-sized single and multiple interfacial voids in a Li/LLZO cell. Consistent with experimental observation [ 19 ] , they showed that an interfacial void grows during stripping and shrinks during plating preferentially along the electrode/solid electrolyte interface. Agier et al. [ 35 ] used a sharp-interface approach to show that sufficient Li flux concentration is required for void growth to occur during stripping in a Li/LLZO cell. Barai et al. [ 37 ] showed the impact of both bulk and surface diffusion of Li on void growth in a Li/LLZO cell. One limitation of these works is that they all assume a homogenous solid electrolyte separator. Typical solid electrolyte separators in ASSBs are polycrystalline, consisting of grain boundaries (GBs) with an ionic conductivity higher or lower than the grain

Read the complete text