Quench switching of Mn 2 As

Kamil Olejník, Zdeněk Kašpar, Jan Zubáč, Sjoerd Telkamp, Andrej Farkaš, Dominik Kriegner, Karel Výborný, Jakub Železný, Zbyněk Šobáň, Peng Zeng, Tomáš Jungwirth, Vít Novák, Filip Krizek · 2024

Read Quench switching of Mn 2 As by Kamil Olejník, Zdeněk Kašpar, Jan Zubáč, Sjoerd Telkamp, Andrej Farkaš, Dominik Kriegner, Karel Výborný, Jakub Železný, Zbyněk Šobáň, Peng Zeng, Tomáš Jungwirth, Vít Novák, Filip Krizek (2024) in the Tower of Babel, a free online library of public-domain works preserved in clean, searchable text. No sign-up. The full text is served as a plain-text file at a predictable URL, where text is present: https://antarctic-labs.com/tower-of-babel/arxiv-2411-01930.txt.

Description

A 2024 arXiv research paper by Kamil Olejník, Zdeněk Kašpar, Jan Zubáč, Sjoerd Telkamp, Andrej Farkaš, Dominik Kriegner, Karel Výborný, Jakub Železný, Zbyněk Šobáň, Peng Zeng, Tomáš Jungwirth, Vít Novák, Filip Krizek. We demonstrate that epitaxial thin film antiferromagnet Mn 2 As exhibits the quench-switching effect, which was previously reported only in crystallographically similar antiferromagnetic CuMnAs thin films.

Catalog record

CREATORKamil Olejník, Zdeněk Kašpar, Jan Zubáč, Sjoerd Telkamp, Andrej Farkaš, Dominik Kriegner, Karel Výborný, Jakub Železný, Zbyněk Šobáň, Peng Zeng, Tomáš Jungwirth, Vít Novák, Filip Krizek
YEAR2024
COLLECTIONPAPERS
FORMATTXT
FILE SIZE23 KB
VERSION1.0
LICENSEhttp://creativecommons.org/licenses/by/4.0/
RIGHTSCC BY
SOURCEarXiv

Source: https://arxiv.org/abs/2411-01930

Browse the full library · About the Tower of Babel

Full text

The opening of the work, from the library's hosted text:

Quench switching of Mn 2 As Kamil Olejník, Zdeněk Kašpar, Jan Zubáč, Sjoerd Telkamp, Andrej Farkaš, Dominik Kriegner, Karel Výborný, Jakub Železný, Zbyněk Šobáň, Peng Zeng, Tomáš Jungwirth, Vít Novák, Filip Krizek Abstract We demonstrate that epitaxial thin film antiferromagnet Mn 2 As exhibits the quench-switching effect, which was previously reported only in crystallographically similar antiferromagnetic CuMnAs thin films. Quench switching in Mn 2 As shows stronger increase in resistivity, reaching hundreds of percent at 5K, and significantly longer retention time of the metastable high-resistive state before relaxation towards the low-resistive uniform magnetic state. Qualitatively, Mn 2 As and CuMnAs show analogous parametric dependence of the magnitude and relaxation of the quench-switching signal. Quantitatively, relaxation dynamics in both materials show direct proportionality to the Néel temperature. This confirms that the quench switching has magnetic origin in both materials. The presented results suggest that the antiferromagnets crystalizing in the Cu 2 Sb structure are well suited for exploring and exploiting the intriguing physics of highly non-uniform magnetic states associated with the quench switching. I Introduction In the past decade, the unique properties of antiferromagnetism inspired new research directions in condensed matter, especially with focus on manipulation of their Néel vector Jungwirth et al. 2016 ; Baltz et al. 2018 ; Xiong et al. 2022 ; Chen et al. 2024 . Its orientation can be detected electrically, e.g., via anisotropic magnetoresistance Marti et al. 2014 ; Wadley et al. 2016 , spin-Hall magnetoresistance Han et al. 2016 , or second-harmonic magnetoresistance Godinho et al. 2018 . However, because of the relativistic nature of these phenomena the corresponding signals are weak, typically below one percent. We have previously demonstrated a strong and reproducible non-relativistic mechanism of manipulation of magnetic order in CuMnAs — the quench switching Kašpar et al. 2021 ; Zubáč et al. 2021 ; Surynek et al. 2024 . This effect is induced by electrical or optical pulses of length ranging from ms to fs, which temporarily heat the material above its Néel temperature (475 K in CuMnAs Wadley et al. 2015 ) and allow it to rapidly cool down. As a result the antiferromagnet remains frozen (quenched) in a metastable state, associated with a strong fragmentation of the antiferromagnetic order by a formation of nano-scale magnetic textures [5,6,7,9], which only slowly relaxes back towards the uniform equilibrium state of the antiferromagnet. The metastable state features a significant increase of resistivity, which can be measured in a straightforward two-point or four-point in-plane resistor geometry. The quench-switching effect in CuMnAs has several intriguing aspects: (i) the high-resistive metastable states are multi-level, controllable by magnitude, length, delay or order of switching pulses; (ii) switching times can match characteristic \mu s/ns scales [5] of microcontrollers/microprocessors, as well as ps-scales [5,7] of THz or optical technologies; (iii) the change in resistivity at room temperature can reach ten percent (100% at low temperature) with very low energy cost of \approx aJ/nm 3 required for switching Wadley et al. 2016 ; (iv) the (sub)ps attempt rates and activation barriers E/k_{B}\approx 30\times 300 K result in temperature-dependent relaxation times spanning many orders of magnitude (from seconds at 300 K to hours at 230 K Kašpar et al. 2021 ); (v) combination of the above features conforms to the requirements of analog time-dependent logic-in-memory (spiking neuromorphic) circuits Surynek et al. 2024 . However, up to now the observation of the above phenomenology of the quench switching remained constrained to a single antiferromagnetic material — the epitaxial thin film of tetragonal CuMnAs. In this paper we report on epitaxial thin film Mn 2 As grown on GaAs substrate, which exhibits a qualitatively analogous phenomenology of the quench-switching effect as in CuMnAs. Quantitatively, the magnitude and retention time of the switching signal is larger, in proportion to the hundred degrees higher Néel temperature in Mn 2 As. Figure 1: (a) Unit cell model of Mn 2 As (Mn - red, As grey), where the arrows highlight the expected local moment orientation. (b) [110] projection model of a portion of Mn 2 As where the antifferomagnetic compensation between magnetic sub-cells A and B is highlighted within the yellow and green rectangle. (c) XRD radial scan, demonstrating high quality of a 20 nm thick Mn 2 As (red) film grown on GaAs together with comparison with CuMnAs grown on GaAs (grey) and GaP (blue) substrates. The green dashed lines highlight positions corresponding to the 00L Bragg peaks of Mn 2 As and grey dashed lines the 002 and 004 Bragg peaks of the substrate. (d) HAADF-STEM projection along [100] direction of a 20 nm film of Mn 2 As grown on a GaAs substrate. (e) HAADF-STEM zoom-in on a portion of the Mn 2 As, with an overlay indicating the Mn (red) and As (grey) atoms. Mn 2 As was selected from an in this context virtually unexplored material family of tetragonal 3d metal pnictides Motizuki et al. 2010 , which belong to the Cu 2 Sb-like P4/ nmm space group and stabilize in a wide range of accessible magnetic orders Zhang et al. 2013 . The previously synthesized bulk form of Mn 2 As is known to be isomorphic to tetragonal CuMnAs, with Cu 2 Sb-type P4/nmm crystal structure and lattice parameters a=3.78\, Å and c=6.28\, Å Austin et al. 1962 , very close to a=3.85\, Å and c=6.28\, Å of CuMnAs. The antiferromagnetic magnetic structure of Mn 2 As belongs to P a nma magnetic space group, which has doubled unit-cell along the [100] direction, as illustrated in Fig. 1 a. Beside the structural similarity between CuMnAs and Mn 2 As and the fact that both are compensated collinear in-plane antiferromagnets, there are also important differences which are highly relevant for the comparison of the quench switching process in the two materials: (i) Mn 2 As has higher Néel temperature of 570 K - 573 K Yuzuri and Yamada 1960 ; Austin et al. 1962 , approximately by 100 K higher than CuMnAs; (ii) both materials have a different magnetic symmetry: CuMnAs is PT symmetric, while Mn 2 As is P symmetric with broken PT symmetry; (iii) in Mn 2 As, Mn/Cu anti-site defects do not exist, which in CuMnAs represent the most likely low-energy point defects Máca et al. 2019 . II Material Growth and Properties The Mn 2 As samples were grown on GaAs (001) substrates by molecular beam epitaxy (MBE). After desorption of the native oxide the GaAs wafer was cooled to 570 ∘ C and a 100 nm thick GaAs buffer layer was grown. To suppress a possible current leakage to the GaAs substrate in electrical measurements, a 500 nm thick Al 0.4 Ga 0.6 As was grown as a second buffer layer in selected samples. After growth of the buffer, the sample was cooled down to 220 ∘ C (measured by band edge spectroscopy Novák et al. 2007 ) and 20, 50 or 78 nm thick Mn 2 As films were grown at 0.024Å/s. Finally, the Mn 2 As film was capped with a 3 nm thick layer of Al (at substrate temperature below 10 ∘ C) which, after oxidation at ambient conditions, forms a protective AlO x layer. Maintaining the 2:1 ratio of the Mn

Read the complete text