The investigation on tensile failure of active waveguide structure by acoustic emission measurements Authors: Zhihui Wu, Yongxin Yu, Cong Zhao, Lingjun Zhang, Yunlong Sun Published: 2026 ABSTRACT Based on the principle of active waveguide monitoring for rock slope, the physical test was designed, and the acoustic emission (AE) characteristics of the active waveguide structure were studied. The results show that the signal distribution range in the parameter correlation diagram expands from the low-amplitude to the high-amplitude region with tensile load increase. The AE amplitude rises from 35 to 55 dB to 60–85 dB, accompanied by a continuous increase in AE energy. Subsequently, continuous signals appear in the frequency bands of 50–150 kHz, accounting for 15% of the total AE events. When the tensile stress is near the peak stage, the AE signal increases sharply, the signal amplitude is distributed in the range of 40-90dB, and a large number of high-frequency signals appear in the range of 300–400 kHz, accounting for 32% of the total effective AE events. The energy amplitude level of the high-frequency band is in the range of 30%-35%. Through a series of tensile load (0.1-1.0kN/s) tests, it is found that the statistical AE counts are sensitive to the loading rate, which can effectively distinguish the tensile stage and cracking evolution trend of the active waveguide structure. The active waveguide structure can monitor the internal deformation and failure characteristics of the rock slope, so as to provide some reference for the early warning. Introduction The slope geological disasters are increasing in recent years, which seriously threaten the property safety of the people. Therefore, the early warning of slope instability is particularly important. The early warning requires effective monitoring of slope instability1–3, and then provides a reliable reference for slope disaster prevention. Therefore, the research on slope monitoring technology has considerable economic and social benefits. In the process of slope deformation and failure, the rock mass cracks and releases energy, and the signal wave propagates in the rock slope. The characteristics of AE signals have important reference indexes for slope monitoring and early warning. Existing research has verified that multiple acoustic emission parameters can effectively reflect the internal damage evolution of rock masses. For instance, hit count and cumulative energy are adopted to identify crack initiation and propagation in rock slopes4. Amplitude and frequency characteristics are analyzed to distinguish different fracture modes5. Meanwhile, signal duration and peak frequency are applied to evaluate the stability and early-warning threshold of geotechnical engineering6,7. Therefore, these AE parameters provide important reference indices for slope monitoring and early warning. Because the AE signals are easy to attenuate in rock slopes and are greatly affected by environmental factors, it is not conducive to the slope stability analysis. Some scholars have proposed using waveguide technology to monitor slope stability and reflect slope deformation characteristics by the evolution law of AE signals. Subsequently, active waveguide technology has gradually received extensive attention in the process of slope monitoring. This technology can monitor the deformation characteristics of rock and soil mass inside the slope. By the AE signal generated by the active waveguide, the deformation state and stress evolution characteristics of the slope can be effectively identified8–10. Some scholars have carried out some research on slope stability based on waveguide monitoring technology, from a single sensor monitoring to a multi-sensor monitoring system. Dixon applies acoustic emission to quantify the deformation behavior and systematically analyses the relationship between AE signals and landslide movement characteristics, providing an effective method for landslide activity assessment11. Japanese researchers have proposed the use of waveguide rods buried in the slope to achieve the purpose of continuous monitoring of slope deformation12. In the 1990 s, some researchers adopted steel rods as a waveguide structure to monitor the deformation of slopes13–16. In addition, some scholars buried the waveguide rod in the soil slope and installed AE sensors on the top of the waveguide rod to monitor the slope stability17. With the application of the waveguide rod, some scholars have improved the waveguide monitoring device, using the active waveguide monitoring device in the field monitoring test18. Dae-Sung Cheon and Yo-Seph Byun19,20 studied the evolution of AE parameters during slope deformation based on an improved acoustic emission monitoring device. There is almost no obvious deformation before the instability failure of the rock slope, and macroscopic deformation and instability failure often occur in a very short time, resulting in slope disasters often showing significant suddenness, concealment and catastrophic consequences. In fact, in the early stage of rock slope failure, there will be many microcracks in the rock mass. The instability process of the rock slope is the cumulative process of internal rock mass rupture11,21,22. The AE monitoring method can identify the micro-deformation and fracture evolution process inside the rock mass, and detect the acoustic emission phenomenon accompanying the fracture process of the rock mass. It is the basis of the early warning research. Some researchers investigate the acoustic signals generated by the rock fracture process18,23, which is a theoretical foundation for the development of monitoring and early warning technology. There are a few studies on the application of active waveguide technology in rock slope monitoring. Rock slopes generally exhibit no obvious deformation before instability and failure. Macroscopic deformation and collapse usually occur within a very short time. During the instability of unstable rock masses, the mortar part of the waveguide structure is also subjected to tensile stress from the surrounding rock mass, resulting in corresponding cracking, deformation and failure, which in turn generates high-intensity acoustic emission signals. The acoustic emission characteristics are closely related to the evolution of microcracking damage inside the mortar of the waveguide structure, enabling the AE behavior of the waveguide structure to be linked with the unstable state of the unstable rock mass. It is necessary to further study the AE characteristics of active waveguide structures in the deformation process of rock slopes, and provide a reference for early warning13,24–26. Recent advances in acoustic emission monitoring have greatly improved the accuracy and reliability of damage detection in engineering materials and structures. Advanced signal processing and machine learning methods have been successfully applied in AE monitoring to enhance the extraction of damage features and realize intelligent fault diagnosis in complex structural systems27. Meanwhile, significant progress has also been made in the quantitative characterization of dynamic damage evolution using AE technology, with new models proposed to describe the relationship between AE signals and the mechanical responses of materials under external loading28. These studies demonstrate the strong capability of AE techniques in capturing subtle damage information and provide important methodological support for the research conducted in this work29,30. Based on the monitoring principle of the active waveguide structure of the rock slope, this paper uses mortar as the filling material of the active waveguide structure, and carries out the acoustic emission monitoring test of tensile loading failure. The evolution law of AE characteristic parameters, parameter correlation and time-frequency characteristics in the fracture process of active waveguide structure is studied. The precursor law of acoustic emission is studied, and the correlation between statistical AE parameters and load rate is further explored. Monitoring principle of active waveguide structure for rock slope In the process of instability evolution of dangerous rock mass, the crack propagation will occur in the rock mass under tensile stress. With the continuous cracking of the rock mass, a dangerous rock mass is produced. In the monitoring process of dangerous rock mass by active waveguide structure, it is appropriate to use the mortar to couple the waveguide rod with the surrounding rock mass to monitor the deformation and failure process of the slope. The monitoring method is shown in Fig. 1. This study realizes real-time and high-sensitivity monitoring of tensile damage in active waveguide structures by means of acoustic emission technology. It establishes quantitative AE thresholds for different failure stages and reveals the correlation between AE characteristics and structural instability. The proposed method has strong engineering applicability and provides a reliable technical approach for early warning of rock slope instability. Furthermore, this monitoring technique can be integrated with wireless communication technologies to form a local monitoring network, demonstrating strong practical applicability. Fig. 1Schematic diagram of the monitoring method. Schematic diagram of the monitoring method. In the process of rock mass instability, the active waveguide structure is subjected to the tensile stress of the surrounding rock mass, resulting in the corresponding cracking, deformation and failure, as shown in Fig. 2. The AE characteristics are related to the evolution process of micro-fracture damage inside the mortar body. Through the instability mechanism of the unstable rock mass, the AE characteristics of the active waveguide structure during the tensile cracking process can be studied, which can effectively reflect the instability evolution process of the unstable rock mass. Fig. 2Mechanical characteristics of the active waveguide structure with mortar materials. Mechanical characteristics of the active waveguide structure with mortar materials. Physical experiment design The tensile loading tests were carried out to monitor the AE signals during the fracture process of the active waveguide structure. The test system was mainly composed of a loading system and an AE monitoring system, as shown in Fig. 3. Fig. 3Test system. Test system. Loading system The WDAJ-600 testing machine is used. The testing machine adopts intelligent control technology, which can realize loading tests under different conditions, and can measure the mechanical parameters such as tensile and compressive strength. The test system is mainly composed of a control computer, a hydraulic system, multi-channel static strain system. AE monitoring system The acoustic emission system is a PCI-28-channel device, which can collect the AE count, energy, amplitude, frequency domain, and other information during the fracture process of the active waveguide structure, and can collect the AE signal waveform. The system uses a PCI board for noise reduction, which can minimize the impact of noise in the signal acquisition process. The system can display and monitor the characteristics of AE parameters in real time, and has the characteristics of multi-channel calculation optimization. The sampling frequency of acoustic emission in the test process is 1 MHz, and the threshold value is set to 40dB. The acoustic emission signals were collected using a Nano-30 high-sensitivity piezoelectric sensor. This sensor has a frequency range of 50–750 kHz with a peak sensitivity of approximately. It is widely used in rock and material fracture tests due to its high sensitivity to high-frequency microcracking signals, making it suitable for monitoring the tensile damage process of the waveguide structure. The sensor is installed at the end of the waveguide rod to accurately collect the AE signal during the loading process. In order to better receive the AE signal, the contact surface between the sensor and the waveguide rod is coated with a coupling agent. Active waveguide structure The active waveguide structures are used to carry out experimental research. The cement mortar with a cement-sand ratio of 1:1 is used. The size of the cylindrical mortar specimen is 260 mm in length and 80 mm in diameter. The geometric dimensions of the specimen were determined based on the actual length and diameter of field anchor bolts used in rock slope engineering, ensuring the test model is consistent with real-world engineering conditions and can truly reflect the mechanical response and acoustic emission characteristics of the active waveguide structure in practical applications. The waveguide rod is made of rebar with a diameter of 18 mm and a length of 400 mm. It is installed in the longitudinal center of the mortar specimen. The completed specimen is shown in Fig. 4. Fig. 4The prepared test specimens. The prepared test specimens. In the instability evolution of unstable rock mass, the rock mass near the main fracture surface is mainly subjected to tensile stress, which causes the mortar body of the active waveguide structure to be in a state of tensile stress for a long time, until the fracture surface is completely cracked. The loading scheme of the tensile failure of the active waveguide structure is shown in Fig. 5. The above loading method is used to study the AE characteristics of the active waveguide structure under the tensile stress state, which can meet the experimental research requirements. Fig. 5Loading test for tensile failure. Loading test for tensile failure. The test process adopted a force control method, and 5 levels of loading rate were used. Three groups of parallel tests are carried out under each loading condition. The loading test scheme is shown in Table 1. The test process adopted a force control method, and five different loading rates were set for the tensile tests. To improve the credibility of experimental results, three identical parallel specimens were prepared and tested under each loading condition, and a total of 15 valid specimens were used in the whole testing program. Through comprehensive analysis, the typical sample data was selected to carry out experimental research. Table 1Testing groups of the tensile failure.loading methodLoading rate (kN/s)Parallel groupsTension cracking loading0.10A11A12A130.25A21A22A230.50A31A32A330.751.00A41A51A42A51A43A51 Table 1Testing groups of the tensile failure.loading methodLoading rate (kN/s)Parallel groupsTension cracking loading0.10A11A12A130.25A21A22A230.50A31A32A330.751.00A41A51A42A51A43A51 Testing groups of the tensile failure. 0.75 1.00 A41 A51 A42 A51 A43 A51 Results and analysis Analysis of failure characteristics of active waveguide structure The AE characteristics of active waveguide structure under tensile load are studied through experiments, which can provide a reference for analyzing the instability evolution state of slope rock mass. The loading rates of the test were set to 0.10 kN/s, 0.25 kN/s, 0.50 kN/s, 0.75 kN/s and 1.00 kN/s, respectively, to simulate the different expansion states of the slope rock mass. Under the tensile loading, the final failure mode of the active waveguide structure is shown in Fig. 6. Fig. 6Failure mode of the active waveguide structure (a) initial loading stage (b) stable development stage (c) near the fracture stage. Failure mode of the active waveguide structure (a) initial loading stage (b) stable development stage (c) near the fracture stage. Figure 6 shows tensile failure modes of the active waveguide structure at different deformation stages: (a) In the initial loading stage, a small amount of cracks began to form inside the specimen, resulting in a small amount of AE signals; (b) In the stable development stage, the internal cracks continue to expand, the AE signal is gradually active, and the cumulative AE energy begins to show an obvious upward trend; (c) Near the fracture stage, the cracks are in the unstable expansion stage, and more and more internal micro-fractures are gradually formed, forming macroscopic cracks. Finally, the AE counts reach their peak. AE characteristics during the tensile failure test Based on the tensile failure test of the active waveguide structure, the AE parameters, parameter correlation and time-frequency evolution characteristic are studied, and the correlation between AE statistical counts and tensile load rate is explored. Quantitative thresholds and statistical characterization are adopted to improve the reliability of stage identification. Analysis of AE parameters Fig. 7AE parameters characteristics (a) Distribution of AE count; (b) Distribution of energy (mv×ms); (c) Distribution of amplitude (dB); (d) Distribution of frequency domain (kHz). AE parameters characteristics (a) Distribution of AE count; (b) Distribution of energy (mv×ms); (c) Distribution of amplitude (dB); (d) Distribution of frequency domain (kHz). As shown in Fig. 7, the tensile fracture process of the specimen can be divided into three stages: the initial loading stage, the stable development stage and the fracture stage. From the diagram, it can be seen that in the initial loading stage, a small number of micro-cracks are initiated inside the specimen, the AE count is small, the cumulative energy curve rises slowly, the signal amplitude is distributed in 40 ~ 70 dB, and the frequency domain is distributed in a band near 50 kHz and 150 kHz. With the gradual increase of tensile stress, it enters a stable development stage. The crack propagation begins to intensify inside the specimen, the AE count increases, and the cumulative energy curve begins to show a clear upward trend. The amplitude distribution is in the range of 40 ~ 85 dB. It is concentrated in the range of 40–60 dB. At this stage, a small number of high-frequency signals begin to appear. Prior to testing, the acoustic emission system was properly calibrated with standard parameters suitable for cement-sand mortar and steel rod composite waveguide structures. The AE threshold was set to 40 dB to suppress background noise interference. The peak definition time (PDT) was determined as 200 µs, the hit definition time (HDT) as 800 µs, and the hit locking time (HLT) as 1000 µs. These timing parameters were optimized to accurately identify AE signals generated from matrix cracking and interfacial debonding, avoid false or repeated hits, and ensure stable and consistent data collection during the entire loading process. As the specimen approaches the fracture stage, a large number of AE signals are generated, and the cumulative energy curve rises sharply. The amplitude is distributed in 40–90 dB, and a large number of high-frequency signals appear, mainly concentrated in the range of 300–400 kHz. With the continuous expansion of the internal cracks in the specimen, the specimen breaks instantaneously, and the stress level almost drops vertically. Subsequently, the specimen was subjected to tensile failure, forming obvious tensile cracks, and the AE count decreased significantly. The above results show that the AE characteristics of the active waveguide structure are related to the structure fracture stage. The AE monitoring can provide a reference for judging the fracture evolution stage of the active waveguide structure. Correlation analysis of AE parameters Fig. 8Evolution process of AE amplitude-energy. Evolution process of AE amplitude-energy. Figure 8 is the amplitude-energy correlation diagram of the AE signal under the tensile failure mode. In the initial loading stage, the signal amplitude and energy are at a low level, and the signal points are concentrated on a relatively small scale. With the tensile stress increase, the amplitude and energy increase slowly, and the expansion degree of signal discrete points in the correlation diagram is relatively small. Near the fracture stage, the internal cracks of the mortar mass are rapidly generated when the tensile stress is close to the peak value. The amplitude-energy correlation diagram begins to expand sharply. There are more high-amplitude and high-energy AE signals. Finally, the signal points are distributed in a wide range. Fig. 9Evolution process of AE duration-count. Evolution process of AE duration-count. Figure 9 is the correlation diagram of AE signal duration-count. In the initial loading stage, the acoustic emission activity is not active, the AE signal duration and count are at a relatively low level, and the signal distribution is concentrated on a small scale. With the continuous increase of tensile stress, the AE signal duration in the stable development stage has increased, and the number of AE counts has also begun to increase, but the distribution range of signal discrete points has not expanded significantly. Near the fracture stage, a large number of new cracks are generated with a large number of AE signals. It is worth noting that the signal points are basically distributed in strips, and the AE signal duration is positively correlated with the count in a large range. Fig. 10Evolution process of AE signal count-frequency. Evolution process of AE signal count-frequency. As shown in Fig. 10, in the initial loading stage, the AE signal count is at a low level, and the frequency domain is mainly concentrated near the range of 50 kHz and 150 kHz. The signals are mainly concentrated near the 50 kHz and 150 kHz frequency bands, accounting for 15% of the total effective AE events. With the further increase of tensile stress, the count density of the AE signal increases, the frequency band range becomes wider, and a small part of the high-frequency signal appears in the range of 300 ~ 400 kHz. The signals are mainly concentrated near the 300 kHz and 400 kHz frequency bands, accounting for 32% of the total effective AE events. Then, near the fracture stage, a large number of microcracks generate inside the mortar mass. The AE signal is extremely active, and the number of high-frequency AE signals also increases significantly. Fig. 11Evolution process of AE energy-frequency. Evolution process of AE energy-frequency. Figure 11 is the correlation diagram of AE signal energy and frequency. In the initial loading stage, the energy value of the AE signal is maintained at a low level, and the frequency domain is mainly distributed near 50 kHz and 150 kHz. The signals are mainly concentrated near the 50 kHz and 150 kHz frequency bands, accounting for 15% of the total effective AE events. With the tensile stress increase, the energy value and frequency domain range increase, and some high-frequency AE signals begin to appear, which are concentrated in the range of 300 ~ 400 kHz. The signals are mainly concentrated near the 300 kHz and 400 kHz frequency bands, accounting for 32% of the total effective AE events. The loading is close to the tensile failure stage, and the AE signals energy in each frequency band increases significantly. Correlation analysis of statistical AE counts and loading rate Based on a series of tensile loading rates, the variation characteristics of statistical AE counts during the test process are analyzed. Fig. 12Characteristics of statistical AE counts under series tensile loading rates. Characteristics of statistical AE counts under series tensile loading rates. As shown in Fig. 12, in the initial loading stage and the stable development stage, the fluctuation range of statistical AE counts is small, and remains at the same level basically. Near the peak state, the microcracks begin to expand, and the AE events are extremely active. The statistical AE counts begin to increase significantly and show a sharp rise. Under the condition of 0.10 kN/s low loading rate, the peak value of AE statistical count is about 110,000, the peak time is about 730 s, and the duration time of the test process is the longest, indicating that the material damage evolves slowly under low loading rate. When the loading rate is increased to 0.25 kN/s, the peak value of AE statistical count is about 200,000, the peak time is advanced to 170 s, the signal intensity and release rate are significantly improved, and the damage development process is accelerated. When the loading rate further increases to 0.50 kN/s, the peak value of AE statistical count rises to 300,000, and the rising section of the curve is steeper, indicating that the crack propagation is more rapid at a high loading rate. When the loading rate continues to increase to 1.0 kN/s, the peak value of AE statistical count is about 350 000, and the peak time is further shortened to 50 s. The faster loading rate leads to brittle fracture of the sample. The regression fitting of the AE count-time series is carried out, and the fitting degree of each working condition is greater than 0.90. The measured data under different loading rates are in good agreement with the fitting curves, which indicates that the fitting method can better describe the evolution characteristics of AE statistical count under different loading rates, and provides a reliable basis for quantitative analysis of the influence of loading rate on failure characteristics. Fig. 13The correlation between statistical AE counts and loading rates. (a) The relationship between statistical AE counts and loading rates. (b) The correlation between the statistical AE counts and the loading rates during the fracture stage. The correlation between statistical AE counts and loading rates. (a) The relationship between statistical AE counts and loading rates. (b) The correlation between the statistical AE counts and the loading rates during the fracture stage. As shown in Fig. 13a, the statistical AE counts under different loading rates remain at a low level in the early stage, and begin to increase sharply near the fracture stage, which is significantly higher than the previous statistical values. Figure 13b reflects the correlation between the AE statistical count and the loading rate during the fracture stage. It can be seen that the statistical AE counts and the loading rates have a typical positive correlation trend. The fitted linear equation indicates that the number of AE events per unit time increases linearly with the loading rate. A linear regression model is expressed as y = 309409.78x + 91939.64, with a correlation coefficient of 0.91. It indicates that there is a good correlation between the AE events and loading rate. By analyzing the evolution trend of statistical AE counts under different loading rates, it can be used to judge the possible tensile stress state of the active waveguide structure. The statistical AE counts in the fracture stage can reflect the influence of loading rate on the fracture behavior of the waveguide structure, which can be used as the characteristic parameter to predict the fracture process, and provide important support for monitoring and early warning based on acoustic emission technology. Time-frequency evolution characteristics of the AE signal Through the wavelet analysis of the AE signals, the time-frequency evolution trend during the tensile loading process is obtained, and the characteristic points of time-frequency analysis are as shown in Fig. 14. Fig. 14Characteristic points of time-frequency analysis. Characteristic points of time-frequency analysis. Fig. 15Time-frequency characteristics during the tensile loading process. Time-frequency characteristics during the tensile loading process. Figure 15a,b reflects the time-frequency diagram during the initial loading stage. Due to the small tensile stress, the number of micro-fractures inside the specimen is small. The time-frequency characteristic shows an obvious low-frequency distribution, near 50kHz and 150 kHz bands, and most energy of the AE signal is mainly concentrated in the low-frequency bands. Figure 15c,d shows the time-frequency diagram in the stable development stage. The frequency domain range has been expanded, and the signal energy is mainly distributed near the low frequency of 50 ~ 150 kHz. As the tensile stress gradually increases, the microcracks gradually expand with some high-frequency signals, and the energy amplitude of the high-frequency band increases. Figure 15e,f is the time-frequency diagram near the fracture stage. In this stage, a large number of microcracks appear and propagate, and the high-frequency domain is mainly distributed in the range of 300 ~ 400 kHz. The energy amplitude of the high-frequency band shows a high level, and the energy amplitude improves significantly. The results show that when the tensile stress approaches the fracture state, the frequency domain of the AE signals becomes wider, and the energy amplitude in the high-frequency domain begins to increase significantly, which can be regarded as the precursor identification of the active waveguide structure failure. Fig. 16Energy percentage characteristics of the high-frequency band. Energy percentage characteristics of the high-frequency band. Figure 16 shows the evolution trend of the energy percentage of the high-frequency band in the tensile failure mode. In the initial loading stage, the energy percentage presents a relatively minimum value, mainly concentrated in the low level range. With the increase of tensile stress, the energy percentage increases gradually. Near the fracture failure stage, the energy percentage in the high-frequency band increases significantly, remaining in the range of 30%~35% high level, until the specimen appears tensile failure. The energy percentage of the high-frequency band is closely related to the fracture process of the active waveguide structure. The energy percentage of the high-frequency band can be used as an effective index to judge the fracture state of the specimen. When the energy percentage begins to reach a large value, and remains in a high level range, it indicates that the micro-cracks inside the active waveguide structure are in a rapid development state, and then the structure will fail. The AE signal indexes can be used to effectively distinguish the instability evolution state of the active waveguide structure, including AE counts, parameter correlation, time-frequency characteristic, energy percentage, etc. The evolution characteristics of AE parameters under the tensile failure process of the active waveguide structure are shown in Table 2. Table 2Evolution characteristics of AE parameter indexes.AE parameter characteristicsInitial loading stageStable development stageNear fracture stageAE countLow level(15%)Increase gradually(35%)Increase rapidly(more than 50%)Cumulative energy curveRise slowlyRise fastDrop steeplyFrequency domainLow-frequency domainHigh-frequency signals appear(15%−20%)High-frequency signal is dense(more than 32%)Energy percentageLow levelIncrease graduallyMaintaining high level(30%~35%)AE duration-countSmall-scaleSmall-scaleSmall range concentration → large rangeAE amplitude-energySmall rangeSmall rangeSmall range concentration → large rangeStatistical AE countsHorizontal status(15%)Horizontal status(35%)Increase sharply(more than 50%) Table 2Evolution characteristics of AE parameter indexes.AE parameter characteristicsInitial loading stageStable development stageNear fracture stageAE countLow level(15%)Increase gradually(35%)Increase rapidly(more than 50%)Cumulative energy curveRise slowlyRise fastDrop steeplyFrequency domainLow-frequency domainHigh-frequency signals appear(15%−20%)High-frequency signal is dense(more than 32%)Energy percentageLow levelIncrease graduallyMaintaining high level(30%~35%)AE duration-countSmall-scaleSmall-scaleSmall range concentration → large rangeAE amplitude-energySmall rangeSmall rangeSmall range concentration → large rangeStatistical AE countsHorizontal status(15%)Horizontal status(35%)Increase sharply(more than 50%) Evolution characteristics of AE parameter indexes. Through comprehensive analysis, it can be seen that in the initial loading stage, the tensile stress is small and the activity of AE events is low. With the gradual increase of tensile stress, the AE count gradually increases, the high-frequency signals begin to increase gradually, and the signal discrete points of the parameters correlation diagram begin to expand on a large scale range. Near the fracture stage, the internal cracks of the specimen are in the unstable expansion state, the AE count rises sharply, and a large number of high-frequency signals appear mainly in the range of 300–400 kHz. The energy amplitude of the high-frequency band shows a high level, and the energy percentage of the high-frequency domain is obviously improved, fluctuating within the high-level range. Then the active waveguide structure formed obvious tensile cracks, and the specimen broke instantaneously. In addition, based on a series of tensile loading tests, it is found that the AE count is sensitive to the change of load rates. There is a good correlation between the statistical AE counts and the loading rates. Near the fracture stage, the curve of statistical AE counts begins to increase sharply. In the process of field monitoring, the characteristics of statistical AE counts can be used to analyze the instability evolution trend of the dangerous rock mass. Under the influence of multiple factors, the formation and evolution process of dangerous rock mass may be very complex. Through the analysis of acoustic emission monitoring data, the comprehensive application of the AE signal parameters is helpful to improve the identification accuracy of the instability evolution stage of the rock slope, and provide reference information for early warning of slope instability. Regarding the relevance to real operating conditions, the experimental results are highly representative. The laboratory tests simulate the tensile-dominated stress state that occurs in actual slope engineering, and the identified AE characteristics can be directly applied to field monitoring. The proposed AE feature-based damage mode recognition method provides a reliable basis for judging the structural stability of the active waveguide system in real environments, thereby enhancing the practical applicability of the monitoring technology. The findings of this study provide a reliable technical reference for slope stability monitoring, and can support the optimized design of monitoring systems in geotechnical engineering. Considering that acoustic emission parameters differ greatly among individual specimens owing to the non-uniform internal structure and random micro-defects of rock-like materials, all graphical results in this study adopt the average values of three parallel test data under the same working condition, rather than test data from a single typical sample. Such processing can weaken the influence of individual specimen variability and accidental errors, so as to accurately reflect the general evolution characteristics of AE signals. Discussion At present, there are many methods and monitoring approaches for slope stability analysis. The mechanical methods rely on a large number of geotechnical parameters, which makes it difficult to realize real-time dynamic monitoring and early warning. Displacement monitoring technologies such as GNSS, GPS, and remote sensing can monitor surface deformation, but they usually fail to identify microcrack activities before macroscopic deformation. In contrast, the active waveguide structure shows significant advantages in monitoring rock slope collapse, which can track the progressive failure process and internal damage evolution of rock slopes. When the rock slope tends to collapse, the waveguide structure is subjected to tension loading and produces continuous AE signals during the whole process of microcrack initiation, stable propagation, and unstable fracture. Compared with displacement monitoring, it can capture early precursor information before macroscopic deformation and improve the timeliness of early warning. Therefore, the active waveguide monitoring technology can make up for the deficiencies of existing monitoring methods, and provide a reliable early warning. Acoustic emission has been used as an effective monitoring technique for capturing microcracks in geotechnical materials. Typical AE parameters, including hit count, cumulative energy, amplitude and duration, have been adopted to identify fracture evolution modes9,10. Nevertheless, conventional AE monitoring for slopes has the disadvantage of severe signal attenuation and environmental interference, which restricts warning reliability and field applicability. To overcome these limitations, waveguide-based AE monitoring has been developed and gradually applied to slope monitoring. With improved device integration, active waveguide systems have been used in field monitoring. Previous research mainly concentrates on the AE signals induced by soil slope deformation, focusing on the empirical relationship between AE activity and displacement rate11,13,16,19. The slope stability analysis methods are complicated and require extensive soil parameters and field monitoring data. In recent years, machine learning methods have been increasingly adopted to establish slope stability assessment models, providing significant guidance for slope hazard monitoring26,27. However, investigations focusing on tensile failure during rock slope collapse remain quite limited. The rock slope collapse is dominated by tensile stress near the main fracture surface, and the tensile fracture mechanism and the AE characteristics of active waveguide structures are still unclear. There is relatively little research content regarding the evolution of amplitude distributions, parameter correlation patterns, and high-frequency precursor features during progressive tensile failure. The study reveals the AE evolution characteristics of the active waveguide structures under tension loading, and explores the mechanical correlation between waveguide tensile damage and rock slope instability. Furthermore, the wavelet transform is used to analyze the time-frequency characteristics of the AE signal, and the energy percentage of each frequency band component can be calculated, so as to accurately analyze the frequency band energy properties under the different loading stages. It constructs a multi-parameter comprehensive classification criterion integrating AE count, amplitude, frequency, energy, and parameter correlations, supporting reliable field identification of rock slope failure. The AE precursor indicators can provide some reference for field monitoring of active waveguide systems. When the proportion of 300–400 kHz high-frequency signals exceeds 32% of total effective AE events, and the high-frequency energy ratio reaches 30%−35%, the active waveguide structure is approaching tensile fracture, indicating a high risk of slope instability. The relationship between loading rate and statistical AE counts allows a certain estimation of rock slope collapse state, and a sharp increase in AE counts indicates accelerating crack propagation, which can be used to determine that the rock slope is in an unstable state. The abundant high-frequency AE signals generated in the tensile failure stage of cement mortar are probably governed by multiple internal microscopic damage. As a typical brittle multiphase composite material, massive microcracks continuously initiate and expand under tensile loading. In the tensile fracture stage, severe tensile stress induces widespread debonding at the interface transition zone between aggregate and cement paste. These small-scale and rapid fracture behaviors continuously generate high-frequency elastic waves, thereby concentrating the occurrence of high-frequency AE signals. With the sharp increase in microscopic fracture events, such dynamic fracture behaviors further enrich the high-frequency components of stress waves in the later failure stage. These AE indicators are suitable for long-term monitoring of the high-risk rock slopes. The study adopts idealized tensile loading tests, while real rock slopes are subjected to complex geological conditions and environmental disturbances, such as rainfall and seismic loading. Further research is required to apply this method to a field monitoring strategy for early warning. In addition, integrating AE parameters with machine learning classification will improve the intelligent recognition of rock slope failure stages and the prediction accuracy of instability probability. Conclusions Based on the acoustic emission monitoring principle of active waveguide structure for the rock slope, a series of physical experiments was carried out. The main conclusions are as follows : At the initial stage, the AE amplitude is concentrated in the range of 40 ~ 50dB. The signals are mainly concentrated near the 50 ~ 150 kHz frequency bands, accounting for 15% of the total effective AE events. And the signal energy is concentrated in the low-frequency domain. The signal points in the parameter correlation diagram are concentrated in a relatively small range in the initial stage. As the tensile stress gradually increases, the AE signal count, energy, and amplitude gradually increase, and some high-frequency signals begin to appear. Near the fracture stage, the signal points are dispersed in a larger range, and the active waveguide structure generates obvious macroscopic tensile cracks.When the tensile stress is near the fracture stage, the AE signals increase sharply. The signal amplitude is distributed in the range of 40 ~ 90 dB, and a large number of high-frequency signals appear in the range of 300 ~ 400 kHz, accounting for 32% of the total effective AE events. The energy amplitude of the high-frequency domain increases, and the energy percentage is maintained at a relatively high level of 30%~35%.Through a series of different loading rates (0.1 ~ 1.0kN/s) tests, it is found that the statistical AE counts are sensitive to the loading rate, which can effectively distinguish the fracture stage and evolution trend of the active waveguide structure. The strong correlation characteristics can be used to provide a reference for the early warning of rock slope instability. At the initial stage, the AE amplitude is concentrated in the range of 40 ~ 50dB. The signals are mainly concentrated near the 50 ~ 150 kHz frequency bands, accounting for 15% of the total effective AE events. And the signal energy is concentrated in the low-frequency domain. The signal points in the parameter correlation diagram are concentrated in a relatively small range in the initial stage. As the tensile stress gradually increases, the AE signal count, energy, and amplitude gradually increase, and some high-frequency signals begin to appear. Near the fracture stage, the signal points are dispersed in a larger range, and the active waveguide structure generates obvious macroscopic tensile cracks. At the initial stage, the AE amplitude is concentrated in the range of 40 ~ 50dB. The signals are mainly concentrated near the 50 ~ 150 kHz frequency bands, accounting for 15% of the total effective AE events. And the signal energy is concentrated in the low-frequency domain. The signal points in the parameter correlation diagram are concentrated in a relatively small range in the initial stage. As the tensile stress gradually increases, the AE signal count, energy, and amplitude gradually increase, and some high-frequency signals begin to appear. Near the fracture stage, the signal points are dispersed in a larger range, and the active waveguide structure generates obvious macroscopic tensile cracks. When the tensile stress is near the fracture stage, the AE signals increase sharply. The signal amplitude is distributed in the range of 40 ~ 90 dB, and a large number of high-frequency signals appear in the range of 300 ~ 400 kHz, accounting for 32% of the total effective AE events. The energy amplitude of the high-frequency domain increases, and the energy percentage is maintained at a relatively high level of 30%~35%. When the tensile stress is near the fracture stage, the AE signals increase sharply. The signal amplitude is distributed in the range of 40 ~ 90 dB, and a large number of high-frequency signals appear in the range of 300 ~ 400 kHz, accounting for 32% of the total effective AE events. The energy amplitude of the high-frequency domain increases, and the energy percentage is maintained at a relatively high level of 30%~35%. Through a series of different loading rates (0.1 ~ 1.0kN/s) tests, it is found that the statistical AE counts are sensitive to the loading rate, which can effectively distinguish the fracture stage and evolution trend of the active waveguide structure. The strong correlation characteristics can be used to provide a reference for the early warning of rock slope instability. Through a series of different loading rates (0.1 ~ 1.0kN/s) tests, it is found that the statistical AE counts are sensitive to the loading rate, which can effectively distinguish the fracture stage and evolution trend of the active waveguide structure. The strong correlation characteristics can be used to provide a reference for the early warning of rock slope instability.